In a process for producing a refractory composite material, the following components are mixed: 4-16 wt. % of silicon, 1-8 wt. % of aluminium, 5-20 wt. % of reactive alumina, 3-50 wt. % of carbon, the remainder corundum, which is partly or wholly replaced by at least one…
Inventor / Author Profile
Wegener Bernd
16Total Forward Citations
4Indexed Patents
2Patent H-Index
In a process for producing a refractory composite material, the following components are mixed: 4-16 wt. % of silicon, 1-8 wt. % of aluminium, 5-20 wt. % of reactive alumina, 3-50 wt. % of carbon, the remainder corundum, which is partly or wholly replaced by at least one…
The connection method uses a graph in which all connections (a,..k) between each network node (K1,..K7) of a first type and each network node of a second type are defined, with use of the graph for determining the optimum connection path through the network, e.g. via a Dijkstra…