WO 2011/035748 A1#8381869 Most Cited · 12 citations0.8/yr · PR 2.37PendingWO · Application
Method and device for etching back a semiconductor layer

The invention relates to a method for at least partially etching back a semiconductor layer (1) of a substrate (3), wherein the substrate (3) is arranged at least partially in an etching solution (5) and wherein areas of the semiconductor layer (3) located outside the etching…

WO 2011/160814 A2#21004451 Most Cited · 5 citations0.3/yr · PR 1.46PendingWO · Application
Method for creating a passivated boron-doped region, especially during production of a solar cell, and solar cell with passivated boron-diffused region

The invention relates to a method for fabrication of a passivated boron-doped region, especially in a solar cell, comprising the steps of a) providing a semiconductor substrate, b) forming a boron-doped region (202,302,402,502) in said semiconductor substrate (201, 201, 301,…

EP 1,890,338 A1#23209957 Most Cited · 4 citations0.2/yr · PR 1.79PendingEP · Application
Method of texturing silicon wafer for fabricating solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Univ KonstanzFiled 2006-08-19

The method involves placing a silicon wafer (3) in a texturing solution (7), which exhibits temperature of eighty degrees Celsius and consists of water, which is displaced with one weight percentage up to six weight percentage potassium hydroxide or two weight percentage up to…

WO 2008/022671 A1#22770752 Most Cited · 4 citations0.2/yr · PR 2.34PendingWO · Application
Method for texturing silicon wafers for producing solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Univ Konstanz, Fath PeterFiled 2007-07-12

In a method for texturing silicon wafers for producing solar cells, the step of introducing a silicon wafer makes use of a texturing solution which is at a temperature of at least 80 degrees Celsius and which comprises water admixed with 1 percent by weight to 6 percent by…

US 2009246969 A1#32921689 Most Cited · 3 citations0.2/yr · PR 1.07PendingUS · Application
Method for texturing silicon wafers for producing solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Uni KonstanzFiled 2007-07-12

In a method for texturing silicon wafers for producing solar cells, the step of introducing a silicon wafer involves the use of a texturing solution which is at a temperature of at least 80 degrees Celsius and which comprises water admixed with 1 percent by weight to 6 percent…

DE 102010024834 A1#40050092 Most Cited · 2 citations0.1/yr · PR 1.01PendingDE · Application
Verfahren zur Herstellung eines passivierten, Bor-dotierten Bereichs, insbesondere während der Herstellung einer Solarzelle, und Solarzelle mit einem passivierten, Bor-dotierten Bereich

Die Erfindung betrifft ein Verfahren zur Herstellung eines passivierten, Bor-dotierten Bereichs, insbesondere in einer Solarzelle, welches die Schritte a) Bereitstellen eines Halbleitersubstrats, b) Ausbilden eines Bor-dotierten Bereichs (202; 302; 402; 502) in genanntem…

TW 201,207,928 A#35771470 Most Cited · 2 citations0.1/yr · PR 1.25ActiveTW · Utility
Process and apparatus for texturizing a flat semiconductor substrate
Inventors: Wefringhaus Eckard, Queisser Steffen, Nagel DeniseAssignee: Rena GmbhFiled 2010-08-19

Process for texturizing a flat semiconductor substrate (1), comprising arranging the semiconductor substrate (1) in such a way that an underside (2) to be texturized is being orientated facing down and contacted from below by a texturization solution (5) during a texturization…

CN 101,507,000 B#102813236 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Method of texturing silicon wafer for fabricating solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Univ KonstanzFiled 2007-07-12 · Granted 2014-02-26

The present invention discloses a method for producing solar battery for texturing the silicon wafer. In the method, a step of introducing silicon wafer relates to adopting a texturing processing solution. The temperature of texturing processing solution is at least 80 DEG C.…

DE 102010024834 B4#154379218 Most Cited · 0 citations0.0/yr · PR 0.56ActiveDE · Utility
Verfahren zur Herstellung eines passivierten, Bor-dotierten Bereichs

Verfahren zur Herstellung eines passivierten Bor-dotierten Bereichs, umfassend die Schrittea) Bereitstellen eines Siliziumsubstrats (201; 301; 401; 501),b) Ausbilden eines Bor-dotierten Bereichs (202; 302; 402; 502) im genannten Siliziumsubstrat (201; 301; 401), wobei die…

DE 102010024836 A1#108692610 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Method for manufacturing solar cell utilized for converting electromagnetic radiation into electrical power, involves electrically connecting two sets of metal contacts with p-doped region and n-doped region, respectively

The method involves forming a p-doped region (302) i.e. boron-doped region, and an n-doped region (303) i.e. phosphorus-doped region, in a semiconductor substrate (301), where a part of a surface area of the substrate belongs to the n-doped region. Dielectric sheets (304, 305)…

DE 102010044271 A1#134310965 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Verfahren zur Herstellung einer Solarzelle

Die Erfindung betrifft ein Verfahren zur Herstellung einer Solarzelle mit den Schritten Bereitstellen eines p- oder n-dotierten Halbleitersubstrats (201), das mindestens eine Oberfläche mit einer Textur mit Minima (203) und Maxima (202) aufweist, Eindiffundieren von…

EP 1,890,338 B1#68405530 Most Cited · 0 citations0.0/yr · PR 0.56ActiveEP · Utility
Method of texturing silicon wafer for fabricating solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Univ KonstanzFiled 2006-08-19 · Granted 2011-06-22

The method involves placing a silicon wafer (3) in a texturing solution (7), which exhibits temperature of eighty degrees Celsius and consists of water, which is displaced with one weight percentage up to six weight percentage potassium hydroxide or two weight percentage up to…

EP 2,426,723 A2#101156758 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method for manufacturing a solar cell

The method involves providing a p or n-doped semiconductor substrate (201). A texture with minima (203) and maxima (202) is formed by diffusion of n-dopant atoms when using p-doped semiconductor substrate or p-dopant atoms when using n-doped semiconductor substrate in the…

EP 2,481,080 A1#109298709 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method and device for etching back a semiconductor layer

The invention relates to a method for at least partially etching back a semiconductor layer (1) of a substrate (3), wherein the substrate (3) is arranged at least partially in an etching solution (5) and wherein areas of the semiconductor layer (3) located outside the etching…

KR 20120080577 A#86252445 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
Method for etching back semiconductor layer and device thereof

본 발명에 의하면, 에칭액(5) 바깥에서 적어도 부분적으로 기판(3)이 정렬되며, 에칭액(5)의 바깥에 놓여 있는 반도체층(1)의 영역은 에칭액(5)으로부터 나오는 반응 증기(11)에 의하여 적어도 부분적으로 제거되며, 반응 증기(11)에 의한 에칭백 속도(etching back rate)의 조절을 위하여 비활성가스 및/또는 적어도 반응가스가 에칭액(5)의 바깥에 놓여 있는 에칭백될 도핑된 반도체층(1)의 영역으로 주입되는 방법 및 장치가 제공된다.

TW 200,816,507 A#69088664 Most Cited · 0 citations0.0/yr · PR 0.56ActiveTW · Utility
Method for texturing silicon wafers for producing solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Univ KonstanzFiled 2007-08-09

In a method for texturing silicon wafers for producing solar cells, the step of introducing a silicon wafer makes use of a texturing solution which is at a temperature of at least 80 degrees Celsius and which comprises water admixed with 1 percent by weight to 6 percent by…

US 8,182,706 B2#139306918 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for texturing silicon wafers for producing solar cells
Inventors: Fath Peter, Melnyk Ihor, Wefringhaus EckardAssignee: Fath Peter, Melnyk IhorFiled 2007-07-12 · Granted 2012-05-22

In a method for texturing silicon wafers for producing solar cells, the step of introducing a silicon wafer involves the use of a texturing solution which is at a temperature of at least 80 degrees Celsius and which comprises water admixed with 1 percent by weight to 6 percent…

WO 2011/160814 A3#116158899 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Method for creating a passivated boron-doped region, especially during production of a solar cell, and solar cell with passivated boron-diffused region

The invention relates to a method for fabrication of a passivated boron -doped region, especially in a solar cell, comprising the steps of a) providing a semiconductor substrate, b) forming a boron-doped region (202, 302, 402, 502) in said semiconductor substrate (201, 201, 301,…