Patents
Inventor / Author Profile

Walliser Wayne

30Total Forward Citations
10Indexed Patents
2Patent H-Index
US 6,646,094 B1#3065027 Most Cited · 25 citations1.1/yr · PR 3.28ExpiredUS · Utility
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63° C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage for…

WO 0,078,834 A1#20563822 Most Cited · 5 citations0.2/yr · PR 1.55PendingWO · Application
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63 degrees C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after…

AU 5,622,200 A#74949003 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63° C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage for…

CA 2,368,869 A1#139516011 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63 degrees C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after…

CA 2,368,869 C#98832054 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63 degrees C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after…

CA 2,634,327 A1#92425815 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using high level of catalyst at a polymerization temperature of about 63 degrees C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage…

CA 2,634,327 C#64640881 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using high level of catalyst at a polymerization temperature of about 63 degrees C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage…

EP 1,194,464 A1#83048969 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Low emission formaldehyde resin and binder for mineral fiber insulation

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63° C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage for…

EP 1,194,464 B1#74824937 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Process for preparing a low emission formaldehyde resin for mineral fibers

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63° C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage for…

ES 2,385,642 T3#139067573 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Procedimiento para preparar una resina de formaldehído de baja emisión para fibras minerales

A phenol-formaldehyde resole resin is prepared using a high level of catalyst at a polymerization temperature of about 63° C. The endpoint, measured by salt water tolerance, is selected so that the resulting resin has a water dilutability of 20:1 at neutral pH after storage for…