1) Composition thixotrope comprenant : - de 10 à 40 % en poids d'une bis-urée a) obtenue par réaction d'une amine aliphatique primaire al) avec un diisocyanate a2) de masse molaire inférieure à 500 g/mole, et - de 60 à 90 % en poids d'un ester b) de formule (I) :…
Verneaut Patrick
The invention relates to a thixotropic composition comprising: between 10 and 40 wt. % of a bis-urea a) obtained by reacting a primary aliphatic amine a1) with a diisocyanate a2) having a molar mass of les than 500 g/mol, and between 60 and 90 wt. % of an ester b) of formula (I)…
An adhesive sealant composition of at least one moisture-crosslinkable prepolymer and an anti-sagging agent of 5% to 30% by weight of a thixotropic composition of 10% to 40% by weight of a bisurea a) obtained by reaction of a primary aliphatic amine a1) with a diisocyanate a2)…
The invention relates to a thixotropic composition comprising: between 10 and 40 wt. % of a bis-urea a) obtained by reacting a primary aliphatic amine a1) with a diisocyanate a2) having a molar mass of les than 500 g/mol, and between 60 and 90 wt. % of an ester b) of formula (I)…
1) Composition thixotrope comprenant : - de 10 à 40 % en poids d'une bis-urée a) obtenue par réaction d'une amine aliphatique primaire al) avec un diisocyanate a2) de masse molaire inférieure à 500 g/mole, et - de 60 à 90 % en poids d'un ester b) de formule (I) :…
1) Thixotropic composition comprising: from 10% to 40% by weight of a bisurea a) obtained by reaction of a primary aliphatic amine a1) with a diisocyanate a2) having a molar mass of less than 500 g/mol, and from 60% to 90% by weight of an ester b) of formula (I): in which: R 1 ,…