A mass of diamond crystals contacting a mass of elemental silicon are confined within a pressure-transmitting medium. The resulting charge assembly is subjected to a pressure of at least 25 kilobars causing application of isostatic pressure to the contacting masses which…
Tuft Roy E
A polycrystalline diamond body infiltrated by a silicon atom-containing metal (e.g., silicon alloy) is bonded to a substrate comprising cemented carbide with a barrier of refractory material extending between the diamonds cemented together with silicon atom-containing binder and…
Improvements are provided in reaction vessel construction used in the growth of diamond by the process disclosed in U.S. Pat. No. 3,297,407 -- Wentorf, Jr. In assembly of the reaction vessel of this invention, the plug of catalyst-solvent material is disposed between the source…
An adherently bonded polycrystalline diamond body is produced by forming a charge composed of a mass of diamond crystals in contact with a mass of eutectiferous silicon-rich alloy wherein the alloy is in contact or in association with hexagonal boron nitride, confining such…
Type Ib or mixed type Ib-Ia natural diamond crystal is annealed at an annealing temperature ranging from about 1500° C to about 2200° C under a pressure which prevents significant graphitization of the diamond during the annealing to convert at least 20% of the total amount of…
Type Ib synthetic diamond crystal is annealed at an annealing temperature ranging from about 1500° C. to about 2200° C. under a pressure which prevents significant graphitization of the diamond during the annealing to convert at least about 20% of the total amount of type Ib…
A smooth surface of a diamond or cubic boron nitride crystal is bombarded with ions sufficiently to penetrate the surface and impart an ion implanted region in the crystal in a predetermined pattern, the resulting crystal is charged electrostatically, and a powder is applied to…
Improvements are provided in reaction vessel construction used in the growth of diamond by the process disclosed in U.S. Pat. No. 3,297,407 -- Wentorf, Jr. In assembly of the reaction vessel of this invention, the plug of catalyst-solvent material is disposed between the source…
A diamond or cubic boron nitride crystal containing growth discontinuities resulting from changes in the environment of the growing crystal and having at least one smooth outside surface which intersects the growth discontinuities is charged electrostatically, a fine powder is…
ABSTRACT OF THE DISCLOSURE Type Ib diamond crystal is annealed at an annealing temperature ranging from about 1500°C to about 2200°C under a pressure which prevents significant graphitization of the diamond during the annealing to convert at least about 20% of the total amount…
ABSTRACT OF THE DISCLOSURE A mass of diamond crystals contacting a mass of elemental silicon is confined within a pressure-transmitting medium. The resulting charge assembly is subjected to a pressure of at least 25 kilobars, causing application of isostatic pressure to the…
Abstract of the Disclosure An adherently bonded polycrystalline diamond body is produced by forming a charge composed of a mass of diamond crystals in contact with a mass of eutectiferous silicon-rich alloy wherein the alloy is in contact or in association with hexagonal boron…