CN 101,472,691 A#7965357 Most Cited · 12 citations0.7/yr · PR 4.51ActiveCN · Utility
Method of continuous casting of high-aluminum steel and mold powder

A method of continuous casting, in which even in the production of a high-aluminum steel with an Al content of 0.1% or higher through continuous casting, a cast piece excelling in surface quality can be produced while preventing the occurrence of depression and cast piece…

JP 2009074119 A#23829441 Most Cited · 4 citations0.2/yr · PR 1.55ActiveJP · Utility
Method for producing molten iron

<P>PROBLEM TO BE SOLVED: To provide a method for inexpensively and stably producing molten iron containing high carbon with superior productivity while blowing an oxygen-containing gas in an iron-bath type melting furnace, which does not cause a slag-forming phenomenon in…

CN 101,743,330 A#32040194 Most Cited · 3 citations0.2/yr · PR 1.12ActiveCN · Utility
Process for producing molten iron

A process for molten-iron production which comprises: charging a solid reduced iron obtained by reducing carbon composite iron oxide briquettes with heating, a carbon material, and a fluxing agent into a melting furnace of the arc heating type while bubbling an inert gas into a…

CN 101,796,199 A#40730109 Most Cited · 2 citations0.1/yr · PR 0.99ActiveCN · Utility
Process for producing molten iron

A process for molten-iron production which comprises: charging a solid reduced iron obtained by reducing carbon composite iron oxide briquettes with heating, a carbon material, and a fluxing agent into a melting furnace of the iron bath type while bubbling an inert gas into a…

CN 102,703,636 A#35390987 Most Cited · 2 citations0.1/yr · PR 1.34ActiveCN · Utility
Continuous refining method and continuous refining facility

The number of blades (16) of an impeller (10), as well as the relations between the height (b0) of the base of the blade (16) and the height (b1) of the tip end, between the width (d) of the blade (16) and the diameter or width of a hot meal channel, between the maximum depth…

EP 2,199,414 A1#51305531 Most Cited · 1 citations0.1/yr · PR 0.85PendingEP · Application
Process for producing molten iron

A process for producing molten iron is a process in which while an inert gas is blown into a molten iron layer in an iron bath type melting furnace through bottom-blown tuyeres provided in a hearth bottom thereof to stir the molten iron layer, a carbon material, an additive…

AU 2008301652 B2#71950408 Most Cited · 0 citations0.0/yr · PR 0.56ActiveAU · Utility
Process for producing molten iron
Inventors: Fumijoto Hideaki, Tsuyoshi Mimura, Takao Harada, Masataka Tateishi, Kiminori HajikaAssignee: Kobe Steel LtdFiled 2008-09-18 · Granted 2011-06-30

A process for molten-iron production which comprises: charging a solid reduced iron obtained by reducing carbon composite iron oxide briquettes with heating, a carbon material, and a fluxing agent into a melting furnace of the iron bath type while bubbling an inert gas into a…

BR 112022009352 A2#127260075 Most Cited · 0 citations0.0/yr · PR 0.56PendingBR · Application
Método para a produção de aço fundido
Inventors: Koji Tokuda, Tsuyoshi MimuraAssignee: Kobe Steel LtdFiled 2020-11-11

MÉTODO PARA A PRODUÇÃO DE AÇO FUNDIDO. Em um método para a produção de um aço fundido de acordo com um aspecto da presente invenção, o ferro reduzido direto em estado sólido contém 3,0% em massa ou mais de SiO2 e Al2O3 no total e 1,0% em massa ou mais de carbono. Uma razão de um…

BR 112022011636 A2#145199860 Most Cited · 0 citations0.0/yr · PR 0.56PendingBR · Application
Método de produção de aço fundido
Inventors: Koji Tokuda, Tsuyoshi MimuraAssignee: Kobe Steel LtdFiled 2020-12-11

MÉTODO DE PRODUÇÃO DE AÇO FUNDIDO. É fornecido um método para produzir um aço fundido de acordo com um aspecto da presente invenção, em que: o ferro reduzido direto em estado sólido contém 3,0% em massa ou mais de SiO2 e Al2O3 no total e 1,0% em massa ou mais de carbono, uma…

CN 100,471,973 C#100952758 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Steel wire rod having excellent drawability and fatigue properties, and manufacturing method of the same
Inventors: Sei Kimura, Tsuyoshi Mimura, Tetsushi DeuraAssignee: Kobe Steel LtdFiled 2006-09-04 · Granted 2009-03-25

A steel wire rod is obtained, in which a gas flow rate during gas stirring in molten steel treatment is controlled to be 0.0005 Nm<3>/min to 0.004 Nm<3>/min per molten steel of 1 ton, thereby the rod satisfies a specified composition, and oxide base inclusions in any…

CN 101,310,028 A#112971188 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Continuous refining method and continuous refining equipment

The invention provides a continuous refining method and a continuous refining apparatus, wherein refining efficiency is improved and desiliconization or desulfurization can be stably performed without deviation by setting the number of blades (16) of an impeller (10), the…

RU 2,453,608 C2#103315128 Most Cited · 0 citations0.0/yr · PR 0.56ActiveRU · Utility
Method of manufacturing of molten cast iron
Inventors: Fumijoto Hideaki, Tsuyoshi Mimura, Takao Harada, Masataka Tateishi, Kiminori HajikaAssignee: Kobe Steel LtdFiled 2008-09-18 · Granted 2012-06-20

FIELD: metallurgy. ^ SUBSTANCE: method involves charging solid reduced iron, carbonaceous material and additional flux into a smelting tank furnace during blowing of an inert gas into a layer of molten cast iron in the melting tank furnace for melting of the cast iron through…

US 12,497,668 B2#156058526 Most Cited · 0 citations0.0/yr · PR 0.00ActiveUS · Utility
Hot metal production from DRI with electric arc heating

According to embodiments, disclosed is a method and system to maintain the soft and sparse slag characteristic favorable for an electric arc to efficiently transfer the energy to molten iron with the power input per furnace area higher than 600 KW/m2 while keeping FeO amount…

US 2026/0071288 A1#155327700 Most Cited · 0 citations0.0/yr · PR 0.00PendingUS · Application
Hot Metal Production from DRI with Electric Arc Heating
Inventors: Haruyasu Michishita, Koji Tokuda, Tsuyoshi Mimura, Katsuma FujiwaraAssignee: Filed 2025-11-12

According to embodiments, disclosed is a method and system to maintain the soft and sparse slag characteristic favorable for an electric arc to efficiently transfer the energy to molten iron with the power input per furnace area higher than 600 KW/m2 while keeping FeO amount…

WO 2009/038140 A1#111031358 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Process for producing molten iron

A process for molten-iron production which comprises: charging a solid reduced iron obtained by reducing carbon composite iron oxide briquettes with heating, a carbon material, and a fluxing agent into a melting furnace of the iron bath type while bubbling an inert gas into a…