Patents
Inventor / Author Profile

Terrien Pascal

93Total Forward Citations
93Indexed Patents
5Patent H-Index
US 5,427,635 A#4105474 Most Cited · 20 citations0.7/yr · PR 5.67ExpiredUS · Utility
Martenstitic stainless steel with improved machinability
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-06-13 · Granted 1995-06-27

The subject of the invention is a martensitic stainless steel with improved machinability, characterized in that its weight composition is the following: carbon lower than 1.2% silicon lower than or equal to 2% manganese lower than or equal to 2% chromium: 10.5</=Cr</=19%…

RU 2,080,410 C1#5680002 Most Cited · 16 citations0.6/yr · PR 3.43ExpiredRU · Utility
Martensite stainless steel exhibiting the improved workability
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-06-10 · Granted 1997-05-27

FIELD: metallurgy. SUBSTANCE: steel has the following composition, wt. -%: carbon - less 1.2; silicon - not above 2; manganese - not above 2; chrome 10.5-19; sulfur - not above 0.55; calcium - not less 32 x $$$; oxygen - not less 70 x $$$, and iron - the rest. Ratio of calcium :…

US 5,496,515 A#6775084 Most Cited · 14 citations0.5/yr · PR 3.07ExpiredUS · Utility
Ferritic stainless steel with improved machinability
Inventors: Pedarre Pierre, Terrien PascalAssignee: Ugine Savoie SaFiled 1995-04-12 · Granted 1996-03-05

Ferritic stainless steel with improved machinability, which can be used especially in the field of screw machining, characterized by the following composition: C<0.17% Si<2.0% Mn<2.0% Cr[11-20] % Ni<1.0% S≦0.55% Ca>30×10 -4 % O>70×10 -4 % the Ca/O ratio,…

EP 0,629,714 A1#9062193 Most Cited · 11 citations0.3/yr · PR 2.73PendingEP · Application
Martensitic stainless steel with improved machinability
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-06-06

Martensitic stainless steel with improved machinability, characterised in that its composition by weight is the following: - carbon lower than 1.2 % - silicon lower than or equal to 2 % - manganese lower than or equal to 2 % - chromium: 10.5 < Cr < 19 % - sulphur lower…

US 5,795,411 A#15097721 Most Cited · 7 citations0.2/yr · PR 1.83ExpiredUS · Utility
Ferritic stainless steel wire and steel wool
Inventors: Terrien Pascal, Pedarre Pierre, Sicoli Bernadette, Bioteau ClaudeAssignee: Ugine Savoie SaFiled 1996-11-04 · Granted 1998-08-18

Ferritic stainless steel which can be used for the production of steel wool, whose composition by weight is the following: carbon≦0.2%, silicon≦2%, manganese≦2%, 11%≦chromium≦30%, nickel≦1%, sulfur≦0.030, calcium≧×10 -4 %, oxygen≧40 ×10 -4 %, the calcium and oxygen contents…

EP 0,736,610 A1#31226382 Most Cited · 3 citations0.1/yr · PR 1.17PendingEP · Application
Resulfurized austenitic stainless steel with improved machinability, suitable for use in the field of high-speed cutting and on the automatic lathe
Inventors: Terrien Pascal, Cholin Xavier, Pedarre PierreAssignee: Ugine Savoie SaFiled 1996-03-15

Austenitic stainless steel contains in wt.%- less than 0.1C; less than 2Si; less than 2Mn; 7-12Ni; 15-25Cr; 0.01-0.55 S; 1-5Cu; less than 0.0035Ca; less than 0.007 O with the ratio of Ca to O being 0.2-0.6.

EP 0,773,306 A1#33202922 Most Cited · 3 citations0.1/yr · PR 1.05PendingEP · Application
Stainless ferritic steel, suitable for producing steel wool

Ferritic stainless steel for making wire wool comprises 11-30 wt.% chromium, up to the following levels of other elements - 0.2% carbon, 2% silicon, 2% manganese, 1% nickel and 0.030% sulphur and also at least 0.0015% calcium and at least 0.0040% oxygen, the ratio of Ca to O…

FR 2,720,410 A1#33202923 Most Cited · 3 citations0.1/yr · PR 1.05PendingFR · Application
Acier inoxydable ferritique à usinabilité améliorée.
Inventors: Pedarre Pierre, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-05-31

Acier inoxydable ferritique à usinabilité améliorée utilisable notamment dans le domaine du décolletage, caractérisé en la composition suivante: (CF DESSIN DANS BOPI) le rapport entre la teneur en calcium et en oxygène Ca/O étant 0,2 <= Ca/O <= 0,6, ledit acier étant…

JP H07150308 A#30577450 Most Cited · 3 citations0.1/yr · PR 1.21ExpiredJP · Utility
Martensite stainless steel with improved cuttability
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-06-14

PURPOSE: To improve machinability without changing forging characteristics and mechanical characteristics at hot and cold by specifying a content of S and a value of Ca/O in the compsn. of a martensitic stainless steel. CONSTITUTION: Component adjustment is executed in such a…

DE 69,423,930 T2#36872606 Most Cited · 2 citations0.1/yr · PR 1.14ExpiredDE · Utility
Martensitisches rostfreies Stahl mit verbesserter Bearbeitbarkeit
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie Imphy UgineFiled 1994-06-06 · Granted 2000-08-17

Martensitic stainless steel with improved machinability, characterised in that its composition by weight is the following: - carbon lower than 1.2 % - silicon lower than or equal to 2 % - manganese lower than or equal to 2 % - chromium: 10.5 < Cr < 19 % - sulphur lower…

EP 0,629,714 B1#45016021 Most Cited · 2 citations0.1/yr · PR 0.88ExpiredEP · Utility
Martensitic stainless steel with improved machinability
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie ImphyFiled 1994-06-06 · Granted 2000-04-12

Martensitic stainless steel with improved machinability, characterised in that its composition by weight is the following: - carbon lower than 1.2 % - silicon lower than or equal to 2 % - manganese lower than or equal to 2 % - chromium: 10.5 < Cr < 19 % - sulphur lower…

EP 0,773,306 B1#39919664 Most Cited · 2 citations0.1/yr · PR 1.01ExpiredEP · Utility
Stainless ferritic steel, suitable for producing steel wool
Inventors: Terrien Pascal, Bioteau Claude, Pedarre Pierre, Sicoli BernadetteAssignee: Ugine Savoie ImphyFiled 1996-10-01 · Granted 2000-12-20

Ferritic stainless steel for making wire wool comprises 11-30 wt.% chromium, up to the following levels of other elements - 0.2% carbon, 2% silicon, 2% manganese, 1% nickel and 0.030% sulphur and also at least 0.0015% calcium and at least 0.0040% oxygen, the ratio of Ca to O…

US 5,656,237 A#36741579 Most Cited · 2 citations0.1/yr · PR 1.14ExpiredUS · Utility
Resulfurized austenitic stainless steel with improved machinability
Inventors: Terrien Pascal, Cholin Xavier, Pedarre PierreAssignee: Ugine Savoie SaFiled 1996-04-08 · Granted 1997-08-12

The present invention relates to a resulfurized austenitic stainless steel with improved machinability, and which is especially useful in the field of machining at high cutting speed and in the field of bar turning.

UA 26,151 C2#50751697 Most Cited · 1 citations0.0/yr · PR 0.85ExpiredUA · Utility
Мартеhситhа hержавіюча сталь покращеhої оброблюваhості
Inventors: Bletton OlІvier, Bayol Jacquues, Terrien PascalAssignee: UgІne SavoieFiled 1994-06-14

Martensitic stainless steel of improved workability contains carbon, silicon, manganese, chromium, sulfur, calcium, oxygen, iron. Steel contains components at following ratio, wt. %: Carbon Below 1.2 Silicon Not more 2 Manganese Not more 2 Chromium 10.5 – 19 Sulfur Not more 0.55…

CA 2,125,732 A1#154183654 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Machinability martensitic stainless steel
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-06-13

L'invention a pour objet un acier inoxydable martensitique à usinabilité améliorée, caractérisé en ce que sa composition pondérale est la suivante : - carbone inférieur à 1,2% - silicium inférieur ou égal à 2% - manganèse inférieur ou égal à 2% - chrome : 10,5<Cr<19% -…

CA 2,125,732 C#91875360 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Machinability martensitic stainless steel
Inventors: Bletton Olivier, Bayol Jacques, Terrien PascalAssignee: Ugine Savoie SaFiled 1994-06-13 · Granted 2000-08-01

L'invention a pour objet un acier inoxydable martensitique à usinabilité améliorée, caractérisé en ce que sa composition pondérale est la suivante : - carbone inférieur à 1,2% - silicium inférieur ou égal à 2% - manganèse inférieur ou égal à 2% - chrome : 10,5<Cr<19% -…

CA 2,150,445 A1#137287592 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Ferritic stainless steel with improved machinability
Inventors: Pedarre Pierre, Terrien PascalAssignee: Ugine Savoie SaFiled 1995-05-29

Acier inoxydable ferritique à usinabilité améliorée utilisable notamment dans le domaine du décolletage, caractérisé en la composition suivante: C < 0,17 % Si < 2,0 % Mn < 2,0 % Cr [11 - 20] % Ni 1,0 % S > 0,55 % Ca > 30 10-4 % O > 70 10-4 % le rapport entre la…

CA 2,150,445 C#110649718 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Ferritic stainless steel with improved machinability
Inventors: Pedarre Pierre, Terrien PascalAssignee: Pierre Pedarre, Pascal TerrienFiled 1995-05-29 · Granted 2001-04-10

Acier inoxydable ferritique à usinabilité améliorée utilisable notamment dans le domaine du décolletage, caractérisé en la composition suivante: C < 0,17 % Si < 2,0 % Mn < 2,0 % Cr [11 - 20] % Ni 1,0 % S > 0,55 % Ca > 30 10-4 % O > 70 10-4 % le rapport entre la…

CA 2,173,573 A1#62814278 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Improved Machinability Resuflurized Austemitic Stainless Steel, Specially for Very High Cutting Speed Machining and for Bar Turning
Inventors: Terrien Pascal, Cholin Xavier, Pedarre PierreAssignee: Ugine Savoie SaFiled 1996-04-04

Austenitic stainless steel contains in wt.%- less than 0.1C; less than 2Si; less than 2Mn; 7-12Ni; 15-25Cr; 0.01-0.55 S; 1-5Cu; less than 0.0035Ca; less than 0.007 O with the ratio of Ca to O being 0.2-0.6.

CA 2,173,573 C#70770703 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Improved machinability resuflurized austemitic stainless steel, specially for very high cutting speed machining and for bar turning
Inventors: Terrien Pascal, Pedarre Pierre, Cholin XavierAssignee: Pascal Terrien, Xavier CholinFiled 1996-04-04 · Granted 1999-12-28

Austenitic stainless steel contains in wt.%- less than 0.1C; less than 2Si; less than 2Mn; 7-12Ni; 15-25Cr; 0.01-0.55 S; 1-5Cu; less than 0.0035Ca; less than 0.007 O with the ratio of Ca to O being 0.2-0.6.

CA 2,188,505 A1#102181221 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Ferritic stainless steel usable for steel wool production

Ferritic stainless steel for making wire wool comprises 11-30 wt.% chromium, up to the following levels of other elements - 0.2% carbon, 2% silicon, 2% manganese, 1% nickel and 0.030% sulphur and also at least 0.0015% calcium and at least 0.0040% oxygen, the ratio of Ca to O…

CA 2,188,505 C#65050033 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Ferritic stainless steel usable for steel wool production
Inventors: Terrien Pascal, Pedarre Pierre, Sicoli Bernadette, Bioteau ClaudeAssignee: Ugine Savoie SaFiled 1996-10-22 · Granted 2003-12-09

Ferritic stainless steel for making wire wool comprises 11-30 wt.% chromium, up to the following levels of other elements - 0.2% carbon, 2% silicon, 2% manganese, 1% nickel and 0.030% sulphur and also at least 0.0015% calcium and at least 0.0040% oxygen, the ratio of Ca to O…

CZ 100,096 A3#83167216 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCZ · Utility
Re-sulfided austenitic stainless steel with improved machinability
Inventors: Terrien Pascal, Cholin Xavier, Pedarre PierreAssignee: Ugine Savoie SaFiled 1996-04-04

Austenitic stainless steel contains in wt.%- less than 0.1C; less than 2Si; less than 2Mn; 7-12Ni; 15-25Cr; 0.01-0.55 S; 1-5Cu; less than 0.0035Ca; less than 0.007 O with the ratio of Ca to O being 0.2-0.6.