The invention relates to an aqueous emulsion of one or more polymers that is stable in storage and is composed according to general formula (I). In said formula: R<1> represents an unbranched or branched alkyl group or alkoxy group comprising between 1 and 4 carbon atoms;…
Tamara Schmidt
a presente invenção refere-se a composições compreendendo um material de fibra e um aglutinante termoplástico específico. o aglutinante termoplástico compreende pelo menos um polímero de poliuretano termoplástico (a), em que o dito polímero de poliuretano termoplástico (a)…
To provide a matrix for fiber-reinforced product having a high glass transition temperature and good mechanical characteristics.SOLUTION: A two-component type polyurethane composition is formed of 10-80 wt.% of polyether polyol that has a viscosity of 20 mPa S-3,000 mPa S, has a…
The invention relates to compositions comprising a fiber material and a specific thermoplastic binder. The thermoplastic binder comprises at least one thermoplastic polyurethane polymer (A), wherein said thermoplastic polyurethane polymer (A) comprises a reaction product of (i)…
The invention relates to a thermoplastic polyurethane matrix resin composition, comprising (i) at least one bridged and/or fused and/or spiro polycyclic alcohol compound; (ii) at least one polyisocyanate; and (iii) at least one diol, which is different from the at least one…
The invention relates to a thermoplastic polyurethane matrix resin composition, comprising at least one C3-8 alkane diol, at least one alkoxylated aromatic diol and at least one polyisocyanate. Furthermore, the present invention relates to a fiber-reinforced composite comprising…
The invention relates to compositions comprising a fiber material and a specific thermoplastic binder. The thermoplastic binder comprises at least one thermoplastic polyurethane polymer, wherein said thermoplastic polyurethane polymer comprises a reaction product of (i) at least…
The invention relates to a two-component polyurethane composition with a viscosity of 20 mPas to 3000 mPas (EN ISO 2555, 25 °C), containing i) 10 to 80 wt.% of at least one polyol with an average molecular weight of 200 g/mol to 3000 g/mol, ii) 5 to 70 wt.% of at least one…
The invention relates to a two-component polyurethane composition containing i) 10 to 80 wt.% of at least one polyol with an average molecular weight of 200 g/mol to 3000 g/mol, ii) 5 to 60 wt.% of at least one aromatic polyisocyanate, and iii) 0 to 15 wt.% of an additive. The…