The chips are maintained for at least 10 mins. at a temp. of at least 50 deg. C after presteaming, preimpregnation with H2O and/or sulphite soln., washing and drying, but before final impregnation, preheating and finishing. Pref. (i) the wood chips are preimpregnated with a…
Inventor / Author Profile
Swan B E
0Total Forward Citations
4Indexed Patents
0Patent H-Index
Frequent Co-Inventors: Dillner B M S Otto C T C
11 The present invention relates to the treatment of wood-chips for the manufacture of chemi-thermomechanical pulp, known as CTMP. After pre-steaming and pre-impregnation, washing and drying, but before final impregnation, pre-heating and refining, the wood-chips are kept at an…
The chips are maintained for at least 10 mins. at a temp. of at least 50 deg. C after presteaming, preimpregnation with H2O and/or sulphite soln., washing and drying, but before final impregnation, preheating and finishing. Pref. (i) the wood chips are preimpregnated with a…