A method for producing austempered spheroidal graphite iron having a microstructure comprising bainite, ferrite and austenite. A nodular-iron casting containing 2-3.5% Si, 0-2% Mn, 0-5% Ni 0-0.3% Sn, 0-03% Cr, 0-3% Mo, 0-1.5% Cu, and 3.3-3.8% C and at most 0.08% P and 0-015% S…
Inventor / Author Profile
Stenfors S-e
1Total Forward Citations
2Indexed Patents
1Patent H-Index