Patents
US 2013048150 A1#5022267 Most Cited · 18 citations1.4/yr · PR 2.33PendingUS · Application
Method for producing workpieces from lightweight steel having material properties that are adjustable across the wall thickness

A method for producing a workpiece having properties which are adjustable across a wall thickness or strip thickness of the workpiece, includes the steps of subjecting the workpiece to a decarburizing annealing treatment under an oxidizing atmosphere and to an accelerated…

WO 2014/180456 A1#5915136 Most Cited · 16 citations1.3/yr · PR 2.18PendingWO · Application
Method for producing components from lightweight steel

The invention relates to a method for producing components from an austenitic lightweight steel which is metastable in its initial state, by forming of a sheet, a circuit board or a pipe in one or more steps, exhibiting a temperature-dependent TRIP and/or TWIP effect during…

US 2009196785 A1#10808706 Most Cited · 10 citations0.6/yr · PR 1.61PendingUS · Application
Transformable Lightweight Structural Steel

A transformable lightweight structural steel, which exhibits a resistance to hydrogen embrittlement, has TRIP and TWIP properties and contains the following elements (in wt.-%): C 0.05 to <=1.0; Al 0.0 to <=11.0; Si 0.0 to <=6.0; Al+Si>0.05; Mn 9.0 to =25.0; H<20…

US 2016122839 A1#10826231 Most Cited · 10 citations1.0/yr · PR 1.57PendingUS · Application
Method for producing components from lightweight steel

A method is disclosed for producing components from an austenitic lightweight steel which is metastable in its initial state, by forming of a sheet, a circuit board or a pipe in one or more steps, exhibiting a temperature-dependent TRIP and/or TWIP effect during forming. To…

US 2013240520 A1#13427074 Most Cited · 8 citations0.6/yr · PR 1.82PendingUS · Application
Energy-storing container made of lightweight steel

An energy-storing container is made of a lightweight steel having the following chemical composition (in wt %): C 0.04-2%; Mn 14-30%; Al 1.5-12%; Si 0.3-3%; Cr 0.12-6%, and additionally one or more of the following elements: Ti, V, Nb, B, Zr, Mo, Ni, Cu, W, Co, P, N, each at up…

DE 102010034161 A1#14443112 Most Cited · 7 citations0.5/yr · PR 2.42PendingDE · Application
Verfahren zur Herstellung von Werkstücken aus Leichtbaustahl mit über die Wanddicke einstellbaren Werkstoffeigenschaften

Verfahren zur Herstellung von Werkstücken aus einem austenitischen Leichtbaustahl Die Erfindung betrifft ein Verfahren zur Herstellung von Werkstücken aus einem austenitischen Leichtbaustahl mit über die Wand- oder Banddicke einstellbaren Werkstoffeigenschaften mit einer…

US 2012121452 A1#15998374 Most Cited · 7 citations0.5/yr · PR 1.42PendingUS · Application
Method for producing a hot rolled strip and hot rolled strip produced from triplex lightweight steel

The invention relates to a method for producing a hot strip from a triplex lightweight steel, wherein a melt is cast into a roughed strip and the latter is subsequently rolled into a hot strip. For this purpose, it is provided that the melt is cast in a horizontal strip casting…

CN 104,203,491 A#17771502 Most Cited · 6 citations0.5/yr · PR 1.61ActiveCN · Utility
Welding additive for electric arc welding and laser beam welding of mixed joins composed of austenitic and ferritic steel

The invention relates to a welding additive for electric arc welding and laser beam welding of mixed joins composed of austenitic and high-manganese-containing and ferritic steel, where the high-manganese-containing steel has a manganese content of at least 7-30% by weight.…

KR 20160003744 A#16983458 Most Cited · 6 citations0.6/yr · PR 1.93ActiveKR · Utility
Method for producing components from lightweight steel

본 발명은 하나 이상의 단계로 시트, 회로 기판 또는 파이프의 성형에 의해 그 초기 상태에서 준안정한, 그리고 성형 중에 온도-의존성 TRIP 및/또는 TWIP 효과를 나타내는 오스테나이트계 경량 강으로 부품을 제조하기 위한 방법에 관한 것이다. 특히 높은 인성을 갖는 부품을 얻기 위해, 성형은 TRIP/TWIP 효과를 방지하는 실온을 초과하는 온도인 40 내지 160℃에서 실행되고, 특히 높은 부품 강도를 달성하기 위해, 성형은 TRIP/TWIP 효과를 증진시키는 실온 미만의 온도인 -65…

DE 102011121679 B4#21185520 Most Cited · 5 citations0.4/yr · PR 1.43ActiveDE · Utility
Verfahren zur Herstellung von Bauteilen aus Leichtbaustahl
Inventors: Evertz Thomas Dr, Otto Manuel Dr, Springub Bianca Dr, Georgeou ZachariasAssignee: Salzgitter Flachstahl GmbhFiled 2011-12-13 · Granted 2014-01-02

Verfahren zur Herstellung von Bauteilen aus einem im Ausgangszustand austenitischen Leichtbaustahl durch Umformung eines Bleches, einer Platine oder eines Rohres in einer oder in mehreren Stufen, aufweisend einen temperaturabhängigen TRIP- und/oder TWIP-Effekt während der…

US 2012093677 A1#20871171 Most Cited · 5 citations0.4/yr · PR 1.49PendingUS · Application
Method for producing a hot rolled strip and hot rolled strip produced from ferritic steel

The invention relates to a method for producing a hot strip from transformation-free ferritic steel, wherein a melt is cast into a roughed strip and the latter is subsequently rolled into a hot strip. For this purpose, it is provided that the melt is cast in a horizontal strip…

WO 2010/102596 A1#21529076 Most Cited · 5 citations0.3/yr · PR 1.37PendingWO · Application
Method for producing a hot rolled strip and hot rolled strip produced from triplex lightweight steel

The invention relates to a method for producing a hot rolled strip from triplex lightweight steel, wherein a melt is cast into a preliminary strip and said strip is subsequently rolled into a hot rolled strip. For this purpose, it is provided that the melt is cast in a…

DE 102005062221 B3#24094524 Most Cited · 4 citations0.2/yr · PR 1.49ExpiredDE · Utility
Deformable light alloy steel with TRIP) and TWIP properties useful in production of products having decreased crack liability twinning induced plasticity (TWIP) good ductility and tensile strength without increase in hydrogen embrittlement

Deformable light alloy steel with transformation induced plasticity (TRIP) and twinning induced plasticity (TWIP) properties of composition (wt.%):C (0.05 to =1.0), Al 0.0 to =11.0), Si (0.0 to =6.0), Al+Si greater than 0.05, Mn (9.0 to =25.0, H less than 20 ppm, remainder Fe…

US 2016138146 A1#27029149 Most Cited · 4 citations0.4/yr · PR 1.12PendingUS · Application
Method for producing an energy-storing container made of lightweight steel

An energy-storing container is made of a lightweight steel having the following chemical composition (in wt %): C 0.04-2%; Mn 14-30%; Al 1.5-12%; Si 0.3-3%; Cr 0.12-6%, and additionally one or more of the following elements: Ti, V, Nb, B, Zr, Mo, Ni, Cu, W, Co, P, N, each at up…

US 9,593,392 B2#27348084 Most Cited · 4 citations0.4/yr · PR 1.03ActiveUS · Utility
Method for producing workpieces from lightweight steel having material properties that are adjustable across the wall thickness
Inventors: John Daniela, Otto Manuel, Schmidt-jÜrgensen Rune, Evertz Thomas, Georgeou ZachariasAssignee: John Daniela, Otto ManuelFiled 2011-02-10 · Granted 2017-03-14

A method for producing a workpiece having properties which are adjustable across a wall thickness or strip thickness of the workpiece, includes the steps of subjecting the workpiece to a decarburizing annealing treatment under an oxidizing atmosphere and to an accelerated…

DE 102011121705 A1#32682682 Most Cited · 3 citations0.2/yr · PR 1.09PendingDE · Application
Schweißzusatz zum Lichtbogen- und Laserstrahlschweißen von Mischverbindungen aus austenitischem und ferritischem Stahl

Die Erfindung betrifft einen Schweißzusatz zum Lichtbogen- und Laserstrahlschweißen von Mischverbindungen aus austenitischem hochmanganhaltigem und ferritischem Stahl, wobei der hochmanganhaltige Stahl einen Mangan Gehalt von mindestens 7–30 Gew.-% aufweist. Dabei besteht der…

WO 2011/113404 A1#29526740 Most Cited · 3 citations0.2/yr · PR 1.30PendingWO · Application
Method for producing workpieces from lightweight steel having material properties that can be adjusted over the wall thickness

The invention relates to a method for producing workpieces from an austenitic lightweight steel having material properties that can be adjusted over the wall thickness or strip thickness and having an alloy composition (in weight percent) comprising: C 0.2 to ≤ 1.0; Al 0.05 to…

DE 102007059006 A1#38310195 Most Cited · 2 citations0.1/yr · PR 1.07PendingDE · Application
Production of hot strip from transition-free ferritic steel comprises casting melt in horizontal strip casting unit to produce semi-finished strip of specified thickness which is then rolled with specified degree of deformation

Production of hot strip from transition-free ferritic steel comprises casting the melt in a horizontal strip casting unit without bending to produce a 6 - 20mm semi-finished strip. This is then rolled with a degree of deformation of at least 50%. An independent claim is included…

DE 102007059007 A1#38339281 Most Cited · 2 citations0.1/yr · PR 1.07PendingDE · Application
Producing hot-rolled strip from triplex structural steel for automobile industry, by casting melt in horizontal strip casting plant, free of bends and with killed-flow to form pre-strip and then rolling with deformation grade to give strip

The method for producing a hot-rolled strip from a triplex structural steel for automobile industry, comprises casting a melt in a horizontal strip casting plant, free of bends and with a killed-flow to form a pre-strip of 6-20 mm and then rolling with a deformation grade of…

DE 102011010040 B3#41164433 Most Cited · 2 citations0.1/yr · PR 0.98ActiveDE · Utility
Verfahren und Einrichtung zum Erzeugen eines gegossenen Bandes aus Stahl mit über den Bandquerschnitt und die Bandlänge einstellbaren Werkstoffeigenschaften

Verfahren und Einrichtung zum Erzeugen eines gegossenen Bandes aus Stahl mit über den Bandquerschnitt und die Bandlänge einstellbaren Werkstoffeigenschaften Die Erfindung betrifft ein Verfahren zum Erzeugen eines gegossenen Bandes aus Stahl mit über den Bandquerschnitt und die…

DE 102011117135 A1#39567595 Most Cited · 2 citations0.1/yr · PR 1.02PendingDE · Application
Energie speicherndes Behältnis aus Leichtbaustahl

Die Erfindung betrifft ein Energie speicherndes Behältnis Hergestellt aus einem Leichtbaustahl mit folgender chemischen Zusammensetzung (in Gew.-%): C 0,04–2% Mn 14–30% Al 1,5–12% Si 0,3–3% Cr 0,12–6% sowie zusätzlich eines oder mehrere der Elemente: Ti, V, Nb, B, Zr, Mo, Ni,…

DE 102011121679 A1#36234676 Most Cited · 2 citations0.1/yr · PR 1.19PendingDE · Application
Manufacturing components made of austenitic lightweight construction steel by transforming sheet metal, where steel has temperature-dependent transformation induced plasticity and/or twinning induced plasticity effect during transformation

The method of manufacturing components made of an austenitic lightweight construction steel by transforming a sheet metal, a circuit board or a tube in an initial state, is claimed, where the austenitic light metal has a temperature-dependent transformation induced plasticity…

EP 2,994,548 A1#39259553 Most Cited · 2 citations0.2/yr · PR 1.03PendingEP · Application
Method for producing components from lightweight steel

The invention relates to a method for producing components from an austenitic lightweight steel which is metastable in its initial state, by forming of a sheet, a circuit board or a pipe in one or more steps, exhibiting a temperature-dependent TRIP and/or TWIP effect during…

KR 20080081969 A#36221390 Most Cited · 2 citations0.1/yr · PR 1.19ActiveKR · Utility
Deformable lightweight structural steel

The invention relates to a deformable lightweight structural steel, which exhibits a resistance to hydrogen embrittlement, has TRIP-and TWIP properties and contains the following elements (in wt.-%): C 0.05 to 0.05; Mn 9.0 to = 25.0; H < 20 ppm, the remainder being composed…