A coating is formed on a substrate by depositing a solution comprising a resin containing at least 2 Si-H groups and a solvent in a manner in which at least 5 volume % of the solvent remains in the coating after deposition followed by exposing the coating to an environment…
Spaulding Michael John
Low dielectric constant films with improved elastic modulus. The method of making such coatings involves providing a porous network coating produced from a resin containing at least 2 Si-H groups where the coating has been thermally cured and has a dielectric constant in the…
A coating is formed on a substrate by depositing a solution comprising a resin containing at least 2 Si-H groups and a solvent in a manner in which at least 5 volume % of the solvent remains in the coating after deposition followed by exposing the coating to an environment…
Low dielectric constant films with improved elastic modulus. The method of making such coatings involves providing a porous network coating produced from a resin containing at least 2 Si-H groups. The coating can be thermally cured and has a dielectric constant in the range of…
This invention pertains to a method for producing thermally stable multi-layer coatings and the coatings produced therefrom. The multi-layer coating is comprised of a first coating produced from hydrogen silsesquioxane having a thickness of 1.25 to 2.25 mum and a second coating…
This invention pertains to a method for producing crack-free, insoluble, greater than 1.25 mu m thick coatings from hydrogen silsesquioxane resin compositions. The method for producing the coating comprises applying a fillerless hydrogen silsesquioxane resin composition onto a…
This invention pertains to a method for producing crack-free, insoluble, greater than 1.25 mu m thick coatings from hydrogen silsesquioxane resin compositions. The method for producing the coating comprises applying a fillerless hydrogen silsesquioxane resin composition onto a…
Trenches in a semiconductor substrate are filled by (i) dispensing a film forming material on the semiconductor substrate and into the trenches; (ii) curing the dispensed film forming material in the presence of an oxidant at a first low temperature for a first predetermined…
Low dielectric constant films with improved elastic modulus. An SiO2-containing plasma treated coating is provided, the coating being formed by providing a porous network coating produced from a resin molecule containing at least 2 Si-H groups, curing the porous network coating…
PROBLEM TO BE SOLVED: To obtain a method for forming a coating with low dielectric constant. SOLUTION: A solution containing at least two resins containing an Si-H group and a solvent is deposited on a substrate, so that at least 5 vol.% solvent remains in coating after being…
This invention pertains to a method for producing thermally stable multi-layer coatings and the coatings produced therefrom. The multi-layer coating is comprised of a first coating produced from hydrogen silsesquioxane having a thickness of 1.25 to 2.25 µm and a second coating…
Low dielectric constant films with improved elastic modulus. The method of making such coatings involves providing a porous network coating produced from a resin containing at least 2 Si-H groups. The coating can be thermally cured and has a dielectric constant in the range of…
Trenches in a semiconductor substrate are filled by (i) dispensing a film forming material on the semiconductor substrate and into the trenches; (ii) curing the dispensed film forming material in the presence of an oxidant at a first low temperature for a first predetermined…
PROBLEM TO BE SOLVED: To provide a method for manufacturing a multi-layer film having heat stability and a film manufactured by the method. SOLUTION: This film is a multi-layer film comprising a first film made of a hydrogen silsesquioxane resin (H resin) and having a thickness…
Low dielectric constant films with improved elastic modulus. An SiO 2 -containing plasma treated coating is provided, the coating being formed by providing a porous network coating produced from a resin molecule containing at least 2 Si—H groups, curing the porous network…
Trenches in a semiconductor substrate are filled by (i) dispensing a film forming material on the semiconductor substrate and into the trenches; (ii) curing the dispensed film forming material in the presence of an oxidant at a first low temperature for a first predetermined…
Low dielectric constant films with improved elastic modulus. An SiO2-containing plasma cured coating having a first dielectric constant and having a first elastic modulus is provided, the coating being formed by providing a porous network coating produced from a resin molecule…
This invention pertains to a method for producing crack-free, insoluble and greater than 1.25 µm thick coatings from hydrogen silsesquioxane resin compositions. This method comprises applying a fillerless hydrogen silsesquioxane resin composition onto a substrate and thereafter…
This invention pertains to a method for producing thermally stable multi-layer coatings and the coatings produced therefrom. The multi-layer coating is comprised of a first coating produced from hydrogen silsesquioxane having a thickness of 1.25 to 2.25 µm and a second coating…
This invention pertains to a method for producing thermally stable multi-layer coatings and the coatings produced therefrom. The multi-layer coating is comprised of a first coating produced from hydrogen silsesquioxane having a thickness of 1.25 to 2.25 µm and a second coating…
This invention pertains to a method for producing crack-free, insoluble and greater than 1.25 µm thick coatings from hydrogen silsesquioxane resin compositions. This method comprises applying a fillerless hydrogen silsesquioxane resin composition onto a substrate and thereafter…
This invention pertains to a method for producing crack-free, insoluble and greater than 1.25 µm thick coatings from hydrogen silsesquioxane resin compositions. This method comprises applying a fillerless hydrogen silsesquioxane resin composition onto a substrate and thereafter…
A coating is formed on a substrate by depositing a solution comprising a resin containing at least 2 Si-H groups and a solvent in a manner in which at least 5 volume % of the solvent remains in the coating after deposition followed by exposing the coating to an environment…
Low dielectric constant films with improved elastic modulus. The method of making such coatings involves providing a porous network coating produced from a resin containing at least 2 Si-H groups. The coating can be thermally cured and has a dielectric constant in the range of…
Low dielectric constant films with improved elastic modulus. An SiO2-containing plasma cured coating having a first dielectric constant and having a first elastic modulus is provided, the coating being formed by providing a porous network coating produced from a resin molecule…