Methods are provided for reducing or minimizing the temperature dependence of a pitch feed or fraction for use in carbon fiber production, such as a mesophase pitch feed or fraction or an isotropic pitch feed or fraction. A pitch sample can be characterized to determine a…
Smith Stuart E
Pitch compositions suitable for spinning may comprise: a pitch having a softening point (SP) below 400° C. and is capable of achieving a radial Hencky strain prior to break of about 0.7 to about 10, at spinning temperature (Ts) ranging from about SP−30° C. to about SP+80° C.…
Nucleation enhancement and/or growth rate improvement of mesophase in pitch compositions derived from hydrocarbon feedstocks can be achieved by: reacting in a reaction zone a blend comprising an isotropic feed and a seeding agent, to produce a reacted pitch having a mesophase…
Pitch compositions may be obtained by subjecting one or more crude oils to steam cracking. Processes for producing pitch compositions suitable for spinning into fibers from steam cracking of crude oils may comprise: steam cracking of one or more crude oils in a steam cracking…
Sulfur-crosslinked olefins, particularly sulfur-crosslinked heavy hydrocarbon products having one or more sulfur-crosslinked olefin moieties, may undergo pyrolysis to form sulfur-doped porous carbon having high BET surface area values. Pyrolysis to form the sulfur-doped porous…
Pitch compositions may be obtained by subjecting one or more crude oils to steam cracking. Processes for producing pitch compositions suitable for spinning into fibers from steam cracking of crude oils may comprise: steam cracking of one or more crude oils in a steam cracking…
A disclosed method comprises providing a heavy hydrocarbon feedstock comprising paraffinic froth treated bitumen and/or solvent de-asphalted bitumen; thermally cracking the heavy hydrocarbon feedstock to produce a cracked stream and a gas; distilling the cracked stream to…
A method of making one or more 2,5-dimethylhexenes is described. The method includes reacting isobutene with isobutanol in the presence of a platinum group metal catalyst to form one or more 2,5-dimethylhexenes. A method of making p-xylene using one or more 2,5-dimethylhexenes…
A pitch composition suitable for spinning may comprise: a pitch having a softening point temperature (T sp ) of 400° C. or less, and an oxidation onset temperature (OOT) at least 10° C. below the T sp at a ramp rate of 10° C./min. A carbon fiber may comprise: a carbon fiber…
Pitch compositions suitable for spinning may comprise: a pitch having a softening point (SP) below 400 °C and is capable of achieving a radial Hencky strain prior to break of about 0.7 to about 10, at spinning temperature (T s ) ranging from about SP-30 °C to about SP+80 °C.…
Nucleation enhancement and/or growth rate improvement of mesophase in pitch compositions derived from hydrocarbon feedstocks can be achieved by: reacting in a reaction zone a blend comprising an isotropic feed and a seeding agent, to produce a reacted pitch having a mesophase…
Pitch compositions suitable for spinning may comprise: a pitch having a softening point (SP) below 400 °C and is capable of achieving a radial Hencky strain prior to break of about 0.7 to about 10, at spinning temperature (T
Pitch compositions suitable for spinning may comprise: a pitch having a softening point (SP) below 400 °C and is capable of achieving a radial Hencky strain prior to break of about 0.7 to about 10, at spinning temperature (T
Pitch compositions may be obtained by subjecting one or more crude oils to steam cracking. Processes for producing pitch compositions suitable for spinning into fibers from steam cracking of crude oils may comprise: steam cracking of one or more crude oils in a steam cracking…
Pitch compositions may be obtained by subjecting one or more crude oils to steam cracking. Processes for producing pitch compositions suitable for spinning into fibers from steam cracking of crude oils may comprise: steam cracking of one or more crude oils in a steam cracking…
A pitch composition suitable for spinning may comprise: a pitch having a softening point temperature (T
A pitch composition suitable for spinning may comprise: a pitch having a softening point temperature (T
Nucleation enhancement and/or growth rate improvement of mesophase in pitch compositions derived from hydrocarbon feedstocks can be achieved by: reacting in a reaction zone a blend comprising an isotropic feed and a seeding agent, to produce a reacted pitch having a mesophase…
A disclosed method comprises providing a heavy hydrocarbon feedstock comprising paraffinic froth treated bitumen and/or solvent de-asphalted bitumen; thermally cracking the heavy hydrocarbon feedstock to produce a cracked stream and a gas; distilling the cracked stream to…
Pitch compositions suitable for spinning may comprise: a pitch having a softening point (SP) below 400 °C and is capable of achieving a radial Hencky strain prior to break of about 0.7 to about 10, at spinning temperature (Ts) ranging from about SP-30 °C to about SP+80 °C.…
Nucleation enhancement and/or growth rate improvement of mesophase in pitch compositions derived from hydrocarbon feedstocks can be achieved by: reacting in a reaction zone a blend comprising an isotropic feed and a seeding agent, to produce a reacted pitch having a mesophase…
A pitch composition suitable for spinning may comprise: a pitch having a softening point temperature (Tsp) of 400°C or less, and an oxidation onset temperature (OOT) at least 10°C below the Tsp at a ramp rate of 10°C/min. A carbon fiber may comprise: a carbon fiber produced from…
Pitch compositions may be obtained by subjecting one or more crude oils to steam cracking. Processes for producing pitch compositions suitable for spinning into fibers from steam cracking of crude oils may comprise: steam cracking of one or more crude oils in a steam cracking…
Asphalt compositions suitable for spinning may comprise: asphalt having a Softening Point (SP) of less than 400 ℃ and a spinning temperature (T) in the range of about SP-30 ℃ to about SP+80 DEG C s ) The radial Hencky strain before fracture of about 0.7 to about 10 can be…
The increased nucleation and/or improved growth rate of mesophases in bitumen compositions derived from hydrocarbon feedstocks may be achieved by: reacting a blend comprising an isotropic feed and a seeding agent in a reaction zone to produce reacted bitumen, having a mesophase…