Patents
US 5,403,547 A#780563 Most Cited · 55 citations1.8/yr · PR 8.47ExpiredUS · Utility
Oxidation resistant low expansion superalloys
Inventors: Smith John Scott, Smith Darrell Franklin Jr, Fisher Roneldo Lee, Heck Karl AndrewAssignee: Inco Alloys IntFiled 1994-04-13 · Granted 1995-04-04

An oxidation resistant alloy containing iron, cobalt, nickel and at least 4 to 5% by weight aluminum having at least a duplex crystalline structure. One crystalline component of this structure is a gamma (fcc) phase having a gamma prime phase dispersed therein. The second…

CN 1,053,094 A#1580968 Most Cited · 37 citations1.1/yr · PR 7.77ExpiredCN · Utility
Oxidation resistant low expansion superalloys

A kind of Fe, Co, Ni and oxidation-resistant alloy of 4-5% (weight) Al at least of containing, this alloy has the two-phase crystalline structure at least.A crystal integral part of described structure is γ (face-centered cubic) phase, wherein contains γ ' phase.Compare with…

RU 2,088,684 C1#3920896 Most Cited · 21 citations0.7/yr · PR 3.70ExpiredRU · Utility
Oxidation-resistant alloy (variants)
Inventors: Smith John Scott, Smith Darrell Franklin Jr, Fisher Roneldo Lee, Heck Karl AndrewAssignee: Inco Alloys IntFiled 1991-01-14 · Granted 1997-08-27

FIELD: metallurgy, alloys nickel-cobalt-iron. SUBSTANCE: alloy has, wt. -%: nickel, 25-50; cobalt, 5-50; aluminium, 5-10; niobium, 0.5-6; manganese + silicon + copper = ,0.14-2; and iron, 20-50. Variant of alloy, wt.-%: nickel, 25-70; cobalt, 5-50; aluminium, 4-15; and iron, the…

US 5,688,471 A#6730137 Most Cited · 14 citations0.5/yr · PR 3.30ExpiredUS · Utility
High strength low thermal expansion alloy
Inventors: Smith John Scott, Hillis Ladonna Sheree, Moore Melissa AnnAssignee: Inco Alloys IntFiled 1996-08-14 · Granted 1997-11-18

The alloy of the invention provides a low coefficient of thermal expansion alloy having a CTE of about 4.9×10 -6 m/m/°C. or less at 204° C. and a relatively high strength. The alloy contains about 40.5 to about 48 nickel, about 2 to about 3.7 niobium, about 0.75 to about 2…

EP 0,588,657 A1#7280981 Most Cited · 13 citations0.4/yr · PR 3.92PendingEP · Application
Controlled thermal expansion superalloy

The invention provides a controlled coefficient of thermal expansion alloy having in weight percent about 26-50% cobalt, about 20-40% nickel, about 20-35% iron, about 4-10% aluminum, about 0.5-5% niobium plus 1/2 of tantalum weight percent and about 1.5-10% chromium.…

EP 0,147,616 A1#10986426 Most Cited · 9 citations0.2/yr · PR 4.32PendingEP · Application
Heat treatment of nickel-iron and nickel-cobalt-iron alloys
Inventors: Smith Darrell Franklin Jr, Smith John ScottAssignee: Inco Alloys IntFiled 1984-11-19

Age-hardenable, controlled low expansion nickel-iron and nickel-cobalt-iron alloys containing from 34 to 55% nickel, up to 25% cobalt, 1% to 2% titanium, 1.5% to 5.5% niobium, 0.25% to 1% silicon, up to 1.25% aluminum, up to 0.01% boron, up to 0.12% carbon, the balance, apart…

EP 0,433,072 A1#10978643 Most Cited · 9 citations0.3/yr · PR 4.49PendingEP · Application
Oxidation resistant low expansion superalloys

An oxidation resistant alloy containing iron, cobalt, nickel and at least 4 to 5% by weight aluminum having at least a duplex crystalline structure. One crystalline component of this structure is a gamma (fcc) phase having a gamma prime phase dispersed therein. The second…

EP 0,104,738 A1#16424142 Most Cited · 6 citations0.1/yr · PR 2.79PendingEP · Application
Controlled expansion alloy
Inventors: Smith Darrell Franklin Jr, Smith John ScottAssignee: Huntington AlloysFiled 1983-08-15

An age-hardenable controlled low-expansion alloy is provided which has high strength and good notch rupture strength, which contains 34 to 55% nickel, upto 25% cobalt, 1 to 2% titanium, 1.5 to 5.5% niobium, not more than 0.2% aluminium, not more than 0.11% carbon, from 0.25 to…

EP 0,856,589 A1#16934127 Most Cited · 6 citations0.2/yr · PR 1.96PendingEP · Application
Age hardenable / controlled thermal expansion alloy

The alloy of the invention provides a controlled coefficient of thermal expansion alloy that age hardens. This alloy consists essentially of, by weight percent, about 32 to 55 nickel, about 6 to 16 cobalt, about 1.2 to 7 chromium, about 0.25 to 1.5 aluminum, about 0.25 to 3…

JP H04272154 A#27651956 Most Cited · 3 citations0.1/yr · PR 2.20ExpiredJP · Utility
Oxidation resisting low expanding super-alloy

PURPOSE: To provide an alloy having a low thermal expansion coefficient by regulating the compsn. contg. specified wt.% of Ni, Co, Al, Ti, C, Cr, Mn, Si, Mo, W, Nb, Zr, B and the balance Fe. CONSTITUTION: This oxidation resistant alloy is composed of the one contg., by weight,…

EP 0,147,616 B1#37727479 Most Cited · 2 citations0.1/yr · PR 1.09ExpiredEP · Utility
Heat treatment of nickel-iron and nickel-cobalt-iron alloys
Inventors: Smith, Darrell Franklin, Jr., Smith, John ScottAssignee: Inco Alloys International, Inc.Filed 1984-11-19 · Granted 1988-04-06

Age-hardenable, controlled low expansion nickel-iron and nickel-cobalt-iron alloys containing from 34 to 55% nickel, up to 25% cobalt, 1% to 2% titanium, 1.5% to 5.5% niobium, 0.25% to 1% silicon, up to 1.25% aluminum, up to 0.01% boron, up to 0.12% carbon, the balance, apart…

EP 0,588,657 B1#41518672 Most Cited · 2 citations0.1/yr · PR 0.98ExpiredEP · Utility
Controlled thermal expansion superalloy

The invention provides a controlled coefficient of thermal expansion alloy having in weight percent about 26-50% cobalt, about 20-40% nickel, about 20-35% iron, about 4-10% aluminum, about 0.5-5% niobium plus 1/2 of tantalum weight percent and about 1.5-10% chromium.…

JP H10212544 A#36002648 Most Cited · 2 citations0.1/yr · PR 1.22ExpiredJP · Utility
Age hardening thermal expansion controlled alloy

PROBLEM TO BE SOLVED: To obtain an Ni-Fe-Co superalloy excellent in thermal expansion coefficient controllability, stress promotion boundary oxidation resistance and corrosion resistance, having good strength and improved in creep resistance so as to maintain phase stability and…

AU 547,912 B2#47776386 Most Cited · 1 citations0.0/yr · PR 0.96ExpiredAU · Utility
Nickel-cobalt-iron alloy
Inventors: Smith John Scott, Smith Darrell FranklinAssignee: Huntington AlloysFiled 1983-07-29 · Granted 1985-11-14

An age-hardenable controlled low-expansion alloy is provided which has high strength and good notch rupture strength, which contains 34 to 55% nickel, up to 25% cobalt, 1 to 2% titanium, 1.5 to 5.5% niobium, not more than 0.2% aluminium, not more than 0.11% carbon, from 0.25 to…

AU 6,805,190 A#49159161 Most Cited · 1 citations0.0/yr · PR 0.89ExpiredAU · Utility
Oxidation resistant low expansion superalloys

An oxidation resistant alloy containing iron, cobalt, nickel and at least 4 to 5% by weight aluminum having at least a duplex crystalline structure. One crystalline component of this structure is a gamma (fcc) phase having a gamma prime phase dispersed therein. The second…

AU 1,742,983 A#81519207 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Nickel-cobalt-iron alloy
Inventors: Smith John Scott, Smith Darrell FranklinAssignee: Huntington AlloysFiled 1983-07-29

An age-hardenable controlled low-expansion alloy is provided which has high strength and good notch rupture strength, which contains 34 to 55% nickel, up to 25% cobalt, 1 to 2% titanium, 1.5 to 5.5% niobium, not more than 0.2% aluminium, not more than 0.11% carbon, from 0.25 to…

AU 3,549,684 A#111707051 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Controlled expansion alloy
Inventors: Smith John Scott, Smith Darrell FranklinAssignee: Inco Alloys IntFiled 1984-11-16

Age-hardenable, controlled low expansion nickel-iron and nickel-cobalt-iron alloys containing from 34 to 55% nickel, up to 25% cobalt, 1% to 2% titanium, 1.5% to 5.5% niobium, 0.25% to 1% silicon, up to 1.25% aluminum, up to 0.01% boron, up to 0.12% carbon, the balance, apart…

AU 4,743,293 A#73537629 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Controlled thermal expansion superalloy

The invention provides a controlled coefficient of thermal expansion alloy having in weight percent about 26-50% cobalt, about 20-40% nickel, about 20-35% iron, about 4-10% aluminum, about 0.5-5% niobium plus 1/2 of tantalum weight percent and about 1.5-10% chromium.…

AU 578,634 B2#133011273 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Controlled expansion alloy
Inventors: Smith John Scott, Smith Darrell Franklin JrAssignee: Inco Alloys IntFiled 1984-11-16 · Granted 1988-11-03

Age-hardenable, controlled low expansion nickel-iron and nickel-cobalt-iron alloys containing from 34 to 55% nickel, up to 25% cobalt, 1% to 2% titanium, 1.5% to 5.5% niobium, 0.25% to 1% silicon, up to 1.25% aluminum, up to 0.01% boron, up to 0.12% carbon, the balance, apart…

AU 627,965 B2#138900965 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Oxidation resistant low expansion superalloys
Inventors: Smith John Scott, Smith Darrell Franklin Jr, Fisher Roneldo Lee, Heck Karl AndrewAssignee: Inco Alloys IntFiled 1990-12-13 · Granted 1992-09-03

An oxidation resistant alloy containing iron, cobalt, nickel and at least 4 to 5% by weight aluminum having at least a duplex crystalline structure. One crystalline component of this structure is a gamma (fcc) phase having a gamma prime phase dispersed therein. The second…

AU 667,124 B2#91227735 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Controlled thermal expansion superalloy

The invention provides a controlled coefficient of thermal expansion alloy having in weight percent about 26-50% cobalt, about 20-40% nickel, about 20-35% iron, about 4-10% aluminum, about 0.5-5% niobium plus 1/2 of tantalum weight percent and about 1.5-10% chromium.…

BR 8,304,448 A#83811588 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredBR · Utility
Liga temperavel por envelhecimento
Inventors: Smith John Scott, Smith Darrell Franklin JrAssignee: Huntington AlloysFiled 1983-08-17

An age-hardenable controlled low-expansion alloy is provided which has high strength and good notch rupture strength, which contains 34 to 55% nickel, up to 25% cobalt, 1 to 2% titanium, 1.5 to 5.5% niobium, not more than 0.2% aluminium, not more than 0.11% carbon, from 0.25 to…

BR 9,006,390 A#134747269 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredBR · Utility
Superligas de baixa expansao resistentes a oxidacao

An oxidation resistant alloy containing iron, cobalt, nickel and at least 4 to 5% by weight aluminum having at least a duplex crystalline structure. One crystalline component of this structure is a gamma (fcc) phase having a gamma prime phase dispersed therein. The second…