Patents
Inventor / Author Profile

Sinclair Harold King

114Total Forward Citations
16Indexed Patents
2Patent H-Index
US 3,972,961 A#381271 Most Cited · 79 citations1.6/yr · PR 35.51ExpiredUS · Utility
Process for the preparation of graft copolymers
Inventors: Hammer Clarence Frederick, Sinclair Harold KingAssignee: Du PontFiled 1974-11-13 · Granted 1976-08-03

Process for the preparation of thermoplastic graft copolymers which comprises heating for about 15 seconds to 60 minutes, with mixing, a trunk copolymer of at least two monomers, at least one of said monomers providing amine-reactive sites taken from the group consisting of the…

US 4,017,557 A#1990308 Most Cited · 32 citations0.7/yr · PR 18.43ExpiredUS · Utility
Novel elastomeric graft copolymers
Inventors: Hammer Clarence Frederick, Sinclair Harold KingAssignee: Du PontFiled 1974-11-13 · Granted 1977-04-12

6-Nylons and 12-nylons having primary amino end-groups and an average degree of polymerization of about 5-60 are grafted onto elastomeric trunk polymers having anhydride groups, vicinal carboxylic groups, or carboxylic groups adjacent to alkoxycarbonyl groups by heating a…

GB 2,289,638 A#41337798 Most Cited · 2 citations0.1/yr · PR 0.98ExpiredGB · Utility
Balloons having improved resistance to oxidation
Inventors: Sinclair Harold King, Burchett Donald KAssignee: Hi Float Co IncFiled 1994-01-06

The oxidation resistance of elastomeric balloons from natural rubber is greatly improved by coating the exterior of the balloon with a film of uncured elastomer, preferably neoprene. The uncured elastomer coating maintains the clarity of the inflated balloons. These balloons are…

AU 3,812,293 A#101345885 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredAU · Utility
Gas barrier coating and coated elastomeric toy balloons
Inventors: Sinclair Harold KingAssignee: Hi Float Co IncFiled 1993-03-12

Polyvinyl alcohol coatings used to improve the bouyant life of elastomeric balloons include polyvinyl alcohol and a water soluble carbohydrate extender such as dextrose, at levels up to four times the weight of the polyvinyl alcohol. The improved coatings of the present…

CA 2,154,067 A1#131034971 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Balloons having improved resistance to oxidation
Inventors: Sinclair Harold King, Burchett Donald KAssignee: Hi Float Co IncFiled 1994-01-06

The oxidation resistance of elastomeric balloons made from natural rubber is greatly improved by coating the exterior of the balloon with a film of uncured elastomer, preferably neoprene. The uncured elastomer coating maintains the clarity of the inflated balloons. These…

EP 0,641,234 A1#136055451 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Gas barrier coating and coated elastomeric toy balloons.
Inventors: Sinclair Harold KingAssignee: Hi Float Co LtdFiled 1993-03-12

Polyvinyl alcohol coatings used to improve the bouyant life of elastomeric balloons include polyvinyl alcohol and a water soluble carbohydrate extender such as dextrose, at levels up to four times the weight of the polyvinyl alcohol. The improved coatings of the present…

EP 0,641,234 A4#109748435 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Gas barrier coating and coated elastomeric toy balloons.
Inventors: Sinclair Harold KingAssignee: Hi Float Co LtdFiled 1993-03-12

Polyvinyl alcohol coatings used to improve the bouyant life of elastomeric balloons include polyvinyl alcohol and a water soluble carbohydrate extender such as dextrose, at levels up to four times the weight of the polyvinyl alcohol. The improved coatings of the present…

WO 9,323,127 A1#71254816 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Gas barrier coating and coated elastomeric toy balloons
Inventors: Sinclair Harold KingAssignee: Hi Float Co IncFiled 1993-03-12

The floating life of toy elastomeric balloons inflated with helium is greatly increased through modifying polyvinyl alcohol coatings from the prior art by removing the glycerine plasticizer from the coating and adding an extender comprised of a saccharide, such as dextrose, at…

WO 9,416,790 A1#148869631 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Balloons having improved resistance to oxidation
Inventors: Sinclair Harold King, Burchett Donald KAssignee: Hi Float Co IncFiled 1994-01-06

The oxidation resistance of elastomeric balloons made from natural rubber is greatly improved by coating the exterior of the balloon with a film of uncured elastomer, preferably neoprene. The uncured elastomer coating maintains the clarity of the inflated balloons. These…