Adhesive blend of wood rosin and a thermoplastic graft copolymer prepared by heating for about 15 seconds to 60 minutes, with mixing, a trunk copolymer of at least two monomers, at least one of said monomers providing amine-reactive sites taken from the group consisting of the…
Sinclair Harold K
Polyvinyl alcohol coatings used to improve the bouyant life of elastomeric balloons include polyvinyl alcohol and a water soluble carbohydrate extender such as dextrose, at levels up to four times the weight of the polyvinyl alcohol. The improved coatings of the present…
The oxidation resistance of elastomeric balloons made from natural rubber is greatly improved by coating the exterior of the balloon with a film of uncured elastomer, preferably neoprene. The uncured elastomer coating maintains the clarity of the inflated balloons. These…
Abstract of the Disclosure 6-Nylons and 12-nylons having primary amino end-groups and an average degree of polymerization of about 5-60 are grafted onto elastomeric trunk polymers having anhydride groups, vicinal carboxylic groups, or carboxylic groups adjacent to alkoxycarbonyl…
ABSTRACT OF THE DISCLOSURE Process for the preparation of thermoplastic graft copolymers which comprises heating for about 15 seconds to 60 minutes, with mizing, a trunk copolymer of at least two monomers, at least one of said monomers pro-viding amine-reactive sites taken from…
The floating life of toy elastomeric balloons inflated with helium is greatly increased through modifying polyvinyl alcohol coatings from the prior art by removing the glycerine plasticizer from the coating and adding an extender comprised of a saccha-ride, such as dextrose, at…
The floating life of toy elastomeric balloons inflated with helium is greatly increased through modifying polyvinyl alcohol coatings from the prior art by removing the glycerine plasticizer from the coating and adding an extender comprised of a saccha-ride, such as dextrose, at…