A liner and method of forming a liner for a tungsten plug in a semiconductor device which reduces cost and improves reliability. In one aspect, it has been discovered that by depositing an initial film of titanium using any conventional process such as CVD, PVD or IMP (ion metal…
Simpson Darrell L
An interconnect structure of a semiconductor device includes a tungsten plug ( 14 ) deposited in a via or contact window ( 11 ). A barrier layer ( 15 ) separates the tungsten plug ( 14 ) from the surface of a dielectric material ( 16 ) within which the contact window or via ( 11…
A layer of doped or undoped germanosilicate glass is formed on a substrate and the layer of germanosilicate glass is thermally treated in steam to remove germanium from the germanosilicate glass, and thereby raise the reflow temperature of the germanosilicate glass so treated.…
A layer of doped or undoped germanosilicate glass is formed on a substrate and the layer of germanosilicate glass is thermally treated in steam to remove germanium from the germanosilicate glass, and thereby raise the reflow temperature of the germanosilicate glass so treated.…
A chemical mechanical polishing (CMP) process using a chemically active slurry having a polarity selected to affect the relative oxidation rates of respective crystalline planes of a polycrystalline surface being polished. The slurry polarity is controlled to equilibrate the…
A chemical mechanical polishing (CMP) process using a chemically active slurry having a polarity selected to affect the relative oxidation rates of respective crystalline planes of a polycrystalline surface being polished. The slurry polarity is controlled to equilibrate the…
An interconnect structure of a semiconductor device includes a tungsten plug ( 14 ) deposited in a via or contact window ( 11 ). A barrier layer ( 15 ) separates the tungsten plug ( 14 ) from the surface of a dielectric material ( 16 ) within which the contact window or via ( 11…
PROBLEM TO BE SOLVED: To provide a barrier layer for the interconnection structure of a semiconductor wafer and a method of depositing the barrier layer. SOLUTION: The interconnection structure of a semiconductor device contains a tungsten plug (14) deposited in a via or a…
<P>PROBLEM TO BE SOLVED: To obtain a method for forming the liner of a tungsten plug. <P>SOLUTION: This is a liner of a tungsten plug in a semiconductor device and a method for forming the liner contribute to cost reduction and enhancement of reliability. In one…
An interconnect structure of a semiconductor device includes a tungsten plug 14 deposited in a via or contact window 11. A barrier layer 15 separates the tungsten plug 14 from the surface of a dielectric material 16 within which the contact window or via 11 is formed. The…
A chemical mechanical polishing (CMP) process using a chemically active slurry having a polarity selected to affect the relative oxidation rates of respective crystalline planes of a polycrystalline surface being polished. The slurry polarity is controlled to equilibrate the…
<P>PROBLEM TO BE SOLVED: To provide a chemical mechanical polishing (CMP) process employing chemically active slurry having polarity selected to have an effect on the relative oxidation rate of respective crystal faces of a polished polycrystalline surface.…
PURPOSE: An interconnect structure and a method for depositing a barrier layer are provided to be capable of reducing the number of pasting steps in IMP(Ionized Metal Plasma) chamber and preventing generation of particles. CONSTITUTION: An interconnect structure(10) includes a…
An interconnect structure of a semiconductor device includes a tungsten plug (14) deposited in a via or contact window (11). A barrier layer (15) separates the tungsten plug (14) from the surface of a dielectric material (16) within which the contact window or via (11) is…