Patents
Inventor / Author Profile

Simons John C M

65Total Forward Citations
9Indexed Patents
3Patent H-Index
Frequent Co-Inventors: Drongelen Jan Van Van Drongelen Jan
EP 0,802,251 A1#1736491 Most Cited · 35 citations1.2/yr · PR 7.49PendingEP · Application
Styrenic block copolymer based hot-melt adhesives
Inventors: Van Drongelen Jan, Simons John C MAssignee: Hercules IncFiled 1996-04-15

Disclosed are hot-melt adhesive compositions suitable for the manufacture of soft goods. They have a melt viscosity of 60,000 mPa.s or less at a temperature of 120°C and include: (a) 50 to 150 parts by weight of a styrenic block copolymer or mixtures and/or modified and/or…

CN 1,172,839 A#6666204 Most Cited · 14 citations0.5/yr · PR 3.79ExpiredCN · Utility
Styrenic block copolymer based hot-melt adhesives, their use for disposable soft goods, and tackifying resins contained therein
Inventors: Drongelen Jan Van, Simons John C MAssignee: Hercules IncFiled 1997-04-15

Disclosed are hot-melt adhesive compositions suitable for the manufacture of soft goods. They have a melt viscosity of 60,000 mPa.s or less at a temperature of 120 DEG C and include: (a) 50 to 150 parts by weight of a styrenic block copolymer or mixtures and/or modified and/or…

JP H1046128 A#9924987 Most Cited · 10 citations0.4/yr · PR 3.17ExpiredJP · Utility
Hot melt adhesive based on styrene block copolymer, use of the same for disposable nondurables and tackifying resin contained in the same
Inventors: Van Drongelen Jan, Simons John C MAssignee: Hercules IncFiled 1997-04-14

PROBLEM TO BE SOLVED: To provide a hot melt adhesive composition suitable for the production of flexible articles and to provide a partially hydrogenated hydrocarbon resin useful as a tackifying resin. SOLUTION: This composition comprises 50-150 pts.wt. styrene block copolymer…

EP 1,035,188 A1#28476990 Most Cited · 3 citations0.1/yr · PR 1.50PendingEP · Application
Viscosity modifier for hot-melt adhesives
Inventors: Van Drongelen Jan, Simons John C MAssignee: Hercules IncFiled 1996-04-15

Disclosed is the use of an aromatic hydrocarbon resin having the following properties:an R&B softening point of 50°C to 150°C;an MMAP cloudpoint of 20°C or lessa DACP cloudpoint of 0°C or less, andan Mz value of 15,000 Dalton or less as a viscosity modifier in a hot-melt…

CA 2,202,192 A1#80341225 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Styrenic block copolymer based hot-melt adhesives, their use for disposable soft goods, and tackifying resins contained therein
Inventors: Simons John C M, Van Drongelen JanAssignee: Hercules IncFiled 1997-04-09

Disclosed are hot-melt adhesive compositions suitable for the manufacture of soft goods. They have a melt viscosity of 60,000 mPa.s or less at a temperature of 120°C and include (a) 50 to 150 parts by weight of a styrenic block copolymer or mixtures and/or modified and/or…

MX 9,702,709 A#144532322 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredMX · Utility
Styrenic block copolymer based hot-melt adhesives.
Inventors: Drongelen Jan Van, Simons John C MAssignee: Hercules IncFiled 1997-04-14

Disclosed are hot-melt adhesive compositions suitable for the manufacture of soft goods. They have a melt viscosity of 60,000 mPa.s or less at a temperature of 120 degree C and include: (a) 50 to 150 parts by weight of a styrenic block copolymer or mixtures and/or modified…

TW 438,873 B#93311490 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredTW · Utility
Styrenic block copolymer based hot-melt adhesives, their use for disposable soft goods, and tackifying resing contained therein
Inventors: Van Drongelen Jan, Simons John C MAssignee: Hercules IncFiled 1997-04-25 · Granted 2001-06-07

Disclosed are hot-melt adhesive compositions suitable for the manufacture of soft goods. They have a melt viscosity of 60,000 mPa.s or less at a temperature of 120 DEG C and include: (a) 50 to 150 parts by weight of a styrenic block copolymer or mixtures and/or modified and/or…