0.05 to 0.2% vanadium and manganese in a concentration equal to 1/4 to 2/3 of the iron concentration are added to an aluminum wrought alloy containing 0.3-1.0% Mg, 0.3-1.2% Si, 0.1-0.5% Fe and up to 0.4% Cu. This alloy is employed mainly for the manufacture of extruded products.
Schwellinger Pius
In a process for the manufacture of a shaped bar consisting of an at least partially metallic material, a preform is shaped to form the shaped bar in the partially solid/partially liquid state and the shaped bar in the partially solid/partially liquid state is guided through a…
A fastener (especially a screw or rivet), for fastening components of aluminium, magnesium and their alloys, consists of an AlZnMgCu type aluminium alloy of composition (by wt.) 6.0-8.0% Zn, 2.0-3.5% Mg, 1.0-3.0% Cu, 0.05-0.30% Zr, NOTGREATER 0.30% Cr, NOTGREATER 0.50% Mn,…
A suitable alloy of the alloy AlMgSi type employed for the manufacture of components having high capacity to absorb kinetic energy by plastic deformation contains, in wt. %, silicon 0.40 to 0.80 magnesium 0.40 to 0.70 iron max. 0.30 copper max. 0.20 manganese max. 0.15 vanadium…
Disclosed is a method for producing an aluminum-scandium master alloy. According to said method, aluminum and scandium are jointly isolated in a cathodic manner using the process parameters valid for the production of aluminum by electrolyzing aluminum oxide and scandium oxide…
Building component is made of an alloy containing (in wt.%): 0.3-1.6 Si, 0.3-1.3 Mg, max. 0.5 Fe, max. 0.9 Cu, max. 0.5 Mn, 0.05-0.3 V, max. 0.3 Co, max. 0.3 Cr, max. 0.8 Ni, max. 0.3 Zr, max. 0.05 other alloying elements, and a balance of Al.
An alloy with 6 to 10% of zinc, 2 to 4% of magnesium, 0 to 3% of copper, 0 to 0.3% of iron, 0 to 0.3% of zirconium, 0 to 0.3% of chromium, 0 to 0.3% of manganese, 0 to 0.2% of silicon and 0 to 0.2% of titanium, the remainder being aluminium of commercial purity, is homogenised…
An alloy suitable for manufacturing components out of a hollow body by high internal pressure forming contains, in wt. %, ______________________________________ Silicon 0.3 to 1.6 Magnesium 0.3 to 1.3 Iron max. 0.5 Copper max. 0.9 Manganese max. 0.5 Vanadium 0.05 to 0.3 Cobalt…
0.05 to 0.2% vanadium and manganese in a concentration equal to 1/4 to 2/3 of the iron concentration are added to an aluminum wrought alloy containing 0.3-1.0% Mg, 0.3-1.2% Si, 0.1-0.5% Fe and up to 0.4% Cu. This alloy is employed mainly for the manufacture of extruded products.
A structural component of a die cast aluminum alloy contains 0.05-0.3 wt.% vanadium. The aluminum alloy has the composition (by wt.) NOTGREATER 1.4% Si, NOTGREATER 0.8% Fe, 0.1-1.6% Mn, NOTGREATER 5.0% Mg, NOTGREATER 0.2% Ti, NOTGREATER 0.1% Zn, 0.05-0.3% V, balance Al and…
A process for forming an initial section or like component featuring a hollow interior to a final shape by means of high internal pressure in the sealed hollow interior using a medium that can flow is such that, in order to shape-form the initial section featuring at least one…
0.05 to 0.2% vanadium and manganese in a concentration equal to 1/4 to 2/3 of the iron concentration are added to an aluminum wrought alloy containing 0.3-1.0% Mg, 0.3-1.2% Si, 0.1-0.5% Fe and up to 0.4% Cu. This alloy is employed mainly for the manufacture of extruded products.
A component, produced from a hollow body by internal high pressure forming, consists of an AlMgSi type alloy having the composition (by wt.) 0.3-1.6% Si, 0.3-1.3% Mg, NOTGREATER 0.5% Fe, NOTGREATER 0.9% Cu, NOTGREATER 0.5 (preferably 0.05-0.15)% Mn, 0.05-0.3 (preferably…
Aluminum alloy contains (in wt.%) 0.3-1.2 silicon, 0.3-1.0 magnesium, 0.2-0.9 manganese, 0.05-0.3 vanadium, maximum 0.05 chromium, maximum 0.5 silver, maximum 0.4 iron, maximum 0.8 copper and maximum 0.2 zinc, with a balance of aluminum and unavoidable impurities.
A weld filler material for fusion welding of high strength aluminum alloys, especially alloys of the AlZnMgCu type, contains 4.1-6.5% of zinc, 4.0-6.0% of magnesium, 0.3-0.6% of copper, 0.3-0.5% of manganese, at most 0.1% of titanium, at most 0.3% of chromium, at most 0.3% of…
The apparatus consists of welded parts of aluminium and parts of copper bonded by laser beam welding. Also claimed is a process for welding the aluminium and copper parts together, e.g. for bonding copper pipes with aluminium foils or sheets.
The apparatus consists of welded parts of aluminium and parts of copper bonded by laser beam welding. Also claimed is a process for welding the aluminium and copper parts together, e.g. for bonding copper pipes with aluminium foils or sheets.
A process is disclosed for extruding a profiled section (40) made at least partially of a metallic material. A preform (36) is extruded in a partially solid or partially liquid state into a section (40) and the extruded section in the partially solid or partially liquid state is…
The invention relates to a method for applying a metal plating material as a plating layer (24) onto the surface of a profile (22) made of an aluminum alloy as the base material. A bolt (18) made of the base material and, in front of the bolt (18), a disk (20) comprising…
An AlMgSi alloy suitable for manufacturing components having a high capacity for absorbing kinetic energy by plastic deformation contains, in percent by weight: Silicon 0.40-0.80, Magnesium 0.40-0.70, Iron max. 0.30, Copper max. 0.20, Manganese max. 0.15, Vanadium 0.05-0.20,…
The invention relates to a method for shaping an initial profile (16a) or a similar workpiece, which comprises a profile space, into a final profile by using an internal high pressure that is generated in the sealed profile space by a flowable active medium. In order to shape…
A process for forming an initial section or like component featuring a hollow interior to a final shape by high internal pressure in the sealed hollow interior using a medium that can flow. In order to shape-form the initial section featuring at least one corner…
To shape a workpiece by an inner high pressure within a sealed profiled zone, to shape it against the profiled walls, at least one of the profile walls (22) flanking a corner zone has an inwards curvature in cross section against the direction of the pressure. The effect of the…
Bei einem Verfahren zum Umformen eines einen Profilraum aufweisenden Ausgangsprofils o. dgl. Werkstückes mittels eines in dem abgedichteten Profilraum durch ein strömbares Wirkmedium erzeugten Innenhochdruckes zu einem Endprofil werden zum Umformen des wenigstens einen…
Ein Schweisszusatzwerkstoff zum Schmelzschweissen von hochfesten Aluminiumlegierungen, insbesondere Legierungen vom Typ AlZnMgCu, enthält 4.1 - 6.5 % Zink, 4.0 - 6.0 % Magnesium, 0.3 - 0.6 % Kupfer, 0.3 - 0.5 % Mangan, max. 0.1 % Titan, max. 0.3 % Chrom, max. 0.3 % Zirkon, max.…