A wear-resistant material which comprises certain concentrations of carbon, nitrogen, oxygen, niobium/tantalum as well as other metallic elements. The material comprises a metal matrix and hard phases embedded therein. The hard phases comprise one or more of carbides, nitrides,…
Schweiger Herbert
The invention concerns a cold-worked steel of high compressive strength for tools and parts simultaneously subjected to several stresses. The steel of the invention evinces a composition in % by weight of C: 0.6 to 1.5 Si: 0.2 to 1.6 Mn: 0.2 to 1.2 Cr: 5.0 to 10.0 Mo: up to 3.0…
A hot-working steel article, e.g., tool, comprising a material which comprises, in % by weight, 0.451 to 0.598 C, 0.11 to 0.29 Si, 0.11 to 0.39 Mn, 4.2 to 4.98 Cr, 2.81 to 3.29 Mo, 0.41 to 0.69 V, with the balance iron, contaminants and accompanying elements, as well as an alloy…
A chromium-molybdenum-vanadium steel has specified impurity content and accompanying elements for producing tools with isotropic properties. A ferrous metal alloy, of composition (by wt.) 0.25-0.79% C, 1.10-7.95% Cr, 0.56-3.49% Mo, 0.26-1.48% V and balance Fe, contains impurity…
A hot-working steel article, e.g., tool, comprising a material which comprises, in % by weight, 0.451 to 0.598 C, 0.11 to 0.29 Si, 0.11 to 0.39 Mn, 4.2 to 4.98 Cr, 2.81 to 3.29 Mo, 0.41 to 0.69 V, with the balance iron, contaminants and accompanying elements, as well as an alloy…
Heat-deviating steel object is made from a composition containing (in wt.%): 0.451-0.598 carbon, 0.11-0.29 silicon, 0.11-0.39 manganese, 4.21-4.98 chromium, 2.81-3.29 molybdenum, 0.41-0.69 vanadium and a balance of iron and impurities. The object has a hardness of at least 58…
Die Erfindung betrifft einen Kaltarbeitsstahl mit hoher Druckfestigkeit für Bauteile und Werkzeuge, die gleichzeitig mehreren Beanspruchungsarten unterworfen sind. Erfindungsgemäß weist der Stahl eine Zusammensetzung von in Gew-% C Ø,6 bis 1,5 Si Ø,2 bis 1,6 Mn Ø,2 bis 1,2 Cr…
The ferrous alloy contains (wt.%) 0.3-0.5 C; 0.4-1.6 Si; 0.3-0.8 Mn; 3.2-6.5 Cr; 0-2 Mo; 0-3 W; 0.95-2 (Mo + W/2); 0.25-1.2 V; 0.75-1.6 Al; 1.2-2.6 (Al + Si); 0-0.2 Nb; 0-0.15 Ti; max 0.35 Ni; max 0.015N; and balance Fe.
A hot-forming steel alloy comprising, in addition to iron and impurity elements, carbon, silicon, manganese, chromium, molybdenum, vanadium and nitrogen within the concentration ranges set forth in the claims. This abstract is neither intended to define the invention disclosed…
The hot working steel alloy consists of alloy elements having carbon (0.37-0.40 wt.%), silicon (0.18-0.26 wt.%), manganese (0.50-0.58 wt.%), chromium (4.90-5.10 wt.%), molybdenum (1.65-1.80 wt.%), vanadium (0.52-0.60 wt.%), nitrogen (0.012-0.015 wt.%), phosphorus (0.005 wt.%),…
Gun barrel for firearms made from a deformed material and method for producing the gun barrel material. The material has a chemical composition in % by weight of: Content C Si Mn P S Cr Mo Min 0.28 0.08 0.15 3.6 1.2 Max 0.36 0.26 0.35 0.005 0.002 4.4 1.8 Content Ni V W Ti As +…
A wear-resistant material which comprises certain concentrations of carbon, nitrogen, oxygen, niobium/tantalum as well as other metallic elements. The material comprises a metal matrix and hard phases embedded therein. The hard phases comprise one or more of carbides, nitrides,…
Carbide-forming metallic melt solidification kinetics and matrix composition control comprises alloying with aluminum in amo dependant on the carbon and group V element contents. An alloying process, for controlling the solidification kinetics and matrix composition of…
Gun barrel of firearms, preferably lightweight small guns formed from a deformed material with a chemical composition comprising carbon (0.28-0.36 wt.%), silicon (0.08-0.26 wt.%), manganese (0.15-0.35 wt.%), phosphorus (0.005 wt.%), sulfur (0.002 wt.%), chromium (3.6-4.4 wt.%),…
PROBLEM TO BE SOLVED: To provide a hot-working steel article in which high degrees of material hardness and toughness value on a remarkably increased level in the rigidity properties are assured, and which provides improved wear resistance in combination with satisfactory heat…
A machine component or part for alternating mechanical stresses up to a temperature of at most 160° C. The component or part comprises a thermally quenched and tempered steel alloy which comprises carbon, silicon, manganese, chromium, molybdenum and vanadium in certain…
The hot working steel alloy consists of alloy elements having carbon (0.37-0.40 wt.%), silicon (0.18-0.26 wt.%), manganese (0.50-0.58 wt.%), chromium (4.90-5.10 wt.%), molybdenum (1.65-1.80 wt.%), vanadium (0.52-0.60 wt.%), nitrogen (0.012-0.015 wt.%), phosphorus (0.005 wt.%),…
A wear-resistant material comprises (in weight%) carbon (0.3-3.5), nitrogen (0.05-4), oxygen (0.002-0.25), niobium/tantalum (3-18), and remainder of metallic elements and impurities. A microstructure of the material comprises a metal matrix and hard phases embedded in the…
The ferrous alloy contains (wt.%) 0.3-0.5 C; 0.4-1.6 Si; 0.3-0.8 Mn; 3.2-6.5 Cr; 0-2 Mo; 0-3 W; 0.95-2 (Mo + W/2); 0.25-1.2 V; 0.75-1.6 Al; 1.2-2.6 (Al + Si); 0-0.2 Nb; 0-0.15 Ti; max 0.35 Ni; max 0.015N; and balance Fe.
A chromium-molybdenum-vanadium steel has specified impurity content and accompanying elements for producing tools with isotropic properties. A ferrous metal alloy, of composition (by wt.) 0.25-0.79% C, 1.10-7.95% Cr, 0.56-3.49% Mo, 0.26-1.48% V and balance Fe, contains impurity…
Heat-deviating steel object is made from a composition containing (in wt.%): 0.451-0.598 carbon, 0.11-0.29 silicon, 0.11-0.39 manganese, 4.21-4.98 chromium, 2.81-3.29 molybdenum, 0.41-0.69 vanadium and a balance of iron and impurities. The object has a hardness of at least 58…
The ferrous alloy contains (wt.%) 0.3-0.5 C; 0.4-1.6 Si; 0.3-0.8 Mn; 3.2-6.5 Cr; 0-2 Mo; 0-3 W; 0.95-2 (Mo + W/2); 0.25-1.2 V; 0.75-1.6 Al; 1.2-2.6 (Al + Si); 0-0.2 Nb; 0-0.15 Ti; max 0.35 Ni; max 0.015N; and balance Fe.