KR 810,001,942 B1#62363730 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredKR · Utility
Furnace for the melting and refining of copper
Inventors: Schummer A, Berndt G, Kapell G, Hansen JAssignee: Norddeutsche RaffinerieFiled 1978-08-07 · Granted 1981-11-28

Apparatus for the melting and refining of Cu comprises a shaft furnace (1) which discharges molten Cu onto one end of a hearth furnace having a discharge outlet (13) at the opposite end. A downwardly extending partition serving to divide the hearth into two zones and means are…

SE 7,907,586 L#111127279 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredSE · Utility
Forfarande for upparbetning av hyttmellanprodukter, sulfidmalmer och/eller malmkoncentrat
Inventors: Schummer A, Hansen U-j, Kopke MAssignee: Norddeutsche AffinerieFiled 1979-09-12

In the processing of sulfur-containing metallurgical intermediates, sulfide ores or ore concentrates at a flame temperature of at least 1500 DEG C. in which sulfur dioxide and a melt are formed, acid sludge from the acid treatment of petroleum and mineral oils is substituted for…

SE 8,100,496 L#109464374 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredSE · Utility
Sett att tillverka valsat stal med god svetsbarhet, hog elasticitetsgrens och slagseghet vid mycket laga temperaturer
Inventors: Schummer A, De La Hamette J, Lessel G, Beck J-p, Frantz AAssignee: ArbedFiled 1981-01-27

To produce a rolled steel product such as rolled steel bars for reinforcing concrete, steel containing carbon, manganese, silicon, aluminium and niobium is rolled in at least three passes. The total reduction during the three passes or the last three passes as the case may be is…

SE 8,105,317 L#84269539 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredSE · Utility
Sett att tillverka valsat stal med god svetsbarhet, hog elasticitetsgrens och slagseghet vid mycket laga temperaturer
Inventors: Schummer A, De La Hamette J, Lessel G, Beck J P, Frantz AAssignee: ArbedFiled 1981-09-08

A rolled steel product (concrete- reinforcing rod) containing at most 0.16% C, at most 2.0% Mn, and at least 0.03% Al, and optionally containing up to 0.55% Si, up to 0.05% Nb, up to 0.1 V, and up to 10% Ni, is reheated to austenitization temperature, held at this temperature…