Patents
Inventor / Author Profile

Schultz Jerold M

156Total Forward Citations
9Indexed Patents
5Patent H-Index
US 5,674,555 A#402834 Most Cited · 77 citations2.7/yr · PR 17.53ExpiredUS · Utility
Process for preparing group Ib-IIIa-VIa semiconducting films
Inventors: Birkmire Robert W, Schultz Jerold M, Marudachalam Matheswaran, Hichri HabibAssignee: Univ DelawareFiled 1995-11-30 · Granted 1997-10-07

Methods are provided for the production of supported monophasic group I-III-VI semiconductor films. In the subject methods, a substrate is coated with group I and III elements and then contacted with a reactive group VI element containing atmosphere under conditions sufficient…

US 4,574,108 A#2009735 Most Cited · 32 citations0.8/yr · PR 7.45ExpiredUS · Utility
Fiber reinforced composite
Inventors: Fakirov Stoyko C, Schultz Jerold MAssignee: Univ DelawareFiled 1985-05-02 · Granted 1986-03-04

Fibers and plastic materials reinforced with these fibers which have a diameter that varies along the fiber axis are provided. The fibers increase the strength of the material by reducing fiber pull out from the plastic matrix. The variation in diameter results in an undulating…

US 4,575,470 A#6290130 Most Cited · 15 citations0.4/yr · PR 2.79ExpiredUS · Utility
Chemically bonded polyolefin laminates
Inventors: Fakirov Stoyko C, Lee I-hwa, Schultz Jerold MAssignee: Univ DelawareFiled 1983-11-18 · Granted 1986-03-11

The present invention relates to laminates of polyolefin laminae and strips chemically bonded in the solid state by reactions initiated by cross-linking catalysts interspersed at the interface of contacting laminae. Catalysts to initiate crosslinking reactions at temperatures…

US 4,915,885 A#7040445 Most Cited · 14 citations0.4/yr · PR 2.17ExpiredUS · Utility
Process of making a blend of PET and PBT
Inventors: Avramova Nadka V, Avramov Isak A, Fakirov Stoyko C, Schultz Jerold MAssignee: Univ DelawareFiled 1988-06-23 · Granted 1990-04-10

A process of preparing a homogeneous amorphous polymeric blend of polyethyleneterephthalate (PET) and polybutyleneterephthalate (PBT) which includes intimately mixing the PET and PBT at a weight ratio of about 10:90-90:10, melting the mixture at 290°-330° C., cooling the mixture…

US 4,715,919 A#8866209 Most Cited · 11 citations0.3/yr · PR 3.68ExpiredUS · Utility
Interfacial bonding of polymeric laminae in the solid state
Inventors: Fakirov Stoyko C, Schultz Jerold MAssignee: Univ DelawareFiled 1985-09-20 · Granted 1987-12-29

The invention relates to chemically bonded laminated structures and their production from oriented polymeric laminae. The bonds between the contacting lamina are formed by chemical reaction across their interface involving constituent molecular chains of each laminae. Three…

US 4,980,237 A#28579781 Most Cited · 3 citations0.1/yr · PR 1.47ExpiredUS · Utility
Welded or laminated polyamides
Inventors: Avramova Nadka V, Fakirov Stoyko C, Schultz Jerold MAssignee: Univ DelawareFiled 1989-12-07 · Granted 1990-12-25

Polyamide bodies, e.g., foils or sheets, are welding together or laminated by forming methylene bridges between nitrogen atoms in the separate bodies by pressing them together in the presence of a alkaline paraformaldehyde/methanol solution containing a catalytic amount of…

US 4,895,612 A#48264060 Most Cited · 1 citations0.0/yr · PR 0.92ExpiredUS · Utility
Method for welding and laminating polyamides
Inventors: Avramova Nadka V, Fakirov Stoyko C, Schultz Jerold MAssignee: Univ DelawareFiled 1988-06-23 · Granted 1990-01-23

Polyamide bodies, e.g., foils or sheets, are welding together or laminated by forming methylene bridges between nitrogen atoms in the separate bodies by pressing them together in the presence of a alkaline paraformaldehyde/methanol solution containing a catalytic amount of…

US 4,842,789 A#77177357 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredUS · Utility
Preparation of high-modulus, high-strength linear polycondensates
Inventors: Evstatiev Michail G, Fakirov Stoyko C, Schultz Jerold MAssignee: Univ DelawareFiled 1988-06-23 · Granted 1989-06-27

Described and claimed is a process for obtaining high-modulus, high-strength linear polycondensates, e.g., polyamides, comprising the sequential steps drawing at room temperature, isothermal annealing at 180 DEG -270 DEG C., a second drawing at room temperature, and a second…