This invention relates to a nitrogen-alloyed steel with a high wear resistance, which is manufactured via spray compacting and has the following composition (in mass-%): C: 0.8-2.5%, N: 0.03-0.75%, Si: 0.15-1.8%, Mn: ≦1.0%, P: ≦0.03%, S: ≦0.05%, Cr: 4.0-11.5%, Mo: 0.5-6.0%, V:…
Schruff Ingolf
The invention relates to a steel with a high resistance to wear and tear and corrosion which is produced by spray deposition and is composed of the following (in percent by weight): C: 0.5 - 2.5 %, Si: </= 1.0 %, Mn: </= 1.0 %, P: </= 0.03 %, S: </= 0.03 %, Cr: 12.0…
The invention concerns a nitrogen alloyed steel with higher wear resistance, which is produced by means of spray compacting and has the following composition (in mass/percentage): C: 0.8 2.5 %; N: 0.03 0.75 %; Si: 0.15 1.8 %; Mn: </= 1.0 %; P: </= 0.03 %; S: </= 0.05 %;…
The invention relates to a steel with a high resistance to wear and tear and corrosion which is produced by spray deposition and is composed of the following (in percent by weight): C: 0.5 - 2.5 %, Si: ≤ 1.0 %, Mn: ≤ 1.0 %, P: ≤ 0.03 %, S: ≤ 0.03 %, Cr: 12.0 - 20.0 %, Mo: 0.1 -…
Nitrogen alloyed steel produced by spray compacting contains (in wt.%): 0.8-2.5 C, 0.03-0.75 N, 0.15-1.8 Mn, not more than 1.0 P, not more than 0.03 S, not more than 0.05 S, 5.0-11.5 Cr, 0.5-6.0 Mo, not more than 4.0 V, not more than 4.0 Nb, not more than 3.5 W, not more than…
The invention relates to a steel with a high resistance to wear and tear and corrosion which is produced by spray deposition and is composed of the following (in percent by weight): C: 0.5 - 2.5 %, Si: ≤ 1.0 %, Mn: ≤ 1.0 %, P: ≤ 0.03 %, S: ≤ 0.03 %, Cr: 12.0 - 20.0 %, Mo: 0.1 -…
Nitrogen alloyed steel produced by spray compacting contains (in wt.%): 0.8-2.5 C, 0.03-0.75 N, 0.15-1.8 Mn, not more than 1.0 P, not more than 0.03 S, not more than 0.05 S, 5.0-11.5 Cr, 0.5-6.0 Mo, not more than 4.0 V, not more than 4.0 Nb, not more than 3.5 W, not more than…
Nitrogen alloyed steel produced by spray compacting contains (in wt.%): 0.8-2.5 C, 0.03-0.75 N, 0.15-1.8 Mn, not more than 1.0 P, not more than 0.03 S, not more than 0.05 S, 5.0-11.5 Cr, 0.5-6.0 Mo, not more than 4.0 V, not more than 4.0 Nb, not more than 3.5 W, not more than…
The invention concerns a nitrogen alloyed steel with higher wear resistance, which is produced by means of spray compacting and has the following composition (in mass/percentage): C: 0.8 2.5 %; N: 0.03 0.75 %; Si: 0.15 1.8 %; Mn: ≤ 1.0 %; P: ≤ 0.03 %; S: ≤ 0.05 %; Cr: 4.0 11.5…
Nitrogen alloyed steel produced by spray compacting contains (in wt.%): 0.8-2.5 C, 0.03-0.75 N, 0.15-1.8 Mn, not more than 1.0 P, not more than 0.03 S, not more than 0.05 S, 5.0-11.5 Cr, 0.5-6.0 Mo, not more than 4.0 V, not more than 4.0 Nb, not more than 3.5 W, not more than…
Procedimiento para la fabricación de un acero de aleación con nitrógeno con una resistencia al desgaste elevada con la siguiente composición (en masa - %): C: 0, 8-2, 5% N: 0, 03-0, 75% Si: 0, 15-1, 8% Mn: :51, 0% P: < 0, 03% S <- 0, 05% Cr: 5, 0-11, 5% Mo: 0, 5¿6, 0% V:…