Patents
US 5,178,686 A#4767161 Most Cited · 18 citations0.6/yr · PR 4.90ExpiredUS · Utility
Lightweight cast material
Inventors: Schmid Eberhard E, Ruehle ManfredAssignee: Metallgesellschaft AgFiled 1991-03-28 · Granted 1993-01-12

Shaped bodies which are improved in high-temperature strength, resistance to thermal shock and fatigue limit can be made of a lightweight cast material which consists mainly of aluminum and in addition contains 5 to 15% by weight magnesium silicide.

US 5,097,887 A#8499011 Most Cited · 12 citations0.3/yr · PR 2.15ExpiredUS · Utility
Process of making a pressure-diecast, fiber-reinforced part
Inventors: Schmid Eberhard E, Neite GunterAssignee: Metallgesellschaft AgFiled 1990-09-05 · Granted 1992-03-24

A preshaped body of ceramic fibers is placed into a mold and molten aluminum-silicon alloy material is charged into the mold. The pressure is increased in a controlled manner so that the shaped fibrous body is penetrated by the molten material and the final pressure is…

US 5,141,703 A#8850085 Most Cited · 11 citations0.3/yr · PR 3.85ExpiredUS · Utility
Process of producing Mg2 Si-containing alloys
Inventors: Schmid Eberhard E, Oldenburg Kersten V, Frommeyer GeorgAssignee: Metallgesellschaft AgFiled 1991-05-07 · Granted 1992-08-25

In a fusion-metallurgical process of producing fine-grained hereogeneous, ductile alloys which contain Mg 2 Si, the grain size of the Mg 2 Si crystallites formed by primary solidification is kept below 30 μm by doping the molten alloy with 0.05 to 2% by weight of phosphorus.

EP 0,478,025 A1#25187409 Most Cited · 4 citations0.1/yr · PR 1.33PendingEP · Application
Components for engines and vehicles

To improve the technological mechanical properties in cast magnesium or magnesium-alloy components for engines and vehicles, finely laminate and solid silicide is embedded in the matrix. <IMAGE>

EP 0,457,380 A1#47567892 Most Cited · 1 citations0.0/yr · PR 0.96PendingEP · Application
Process for manufacturing of alloys containing magnesium disilicide

In a process for the melt-metallurgical manufacture of fine-grained heterogeneous ductile alloys containing Mg2Si, the alloy melt is doped with 0.05 to 2.00% by weight of phosphorus to achieve a grain size of < 30 mu m of the Mg2Si crystallites which solidify first.

CA 2,041,233 A1#116752987 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Process of producing mg2si-containing alloys

ABSTRACT In a fusion-metallurgical process of producing fine-grained hereogeneous, ductile alloys which contain Mg2Si, the grain size of the Ng2Si crystallites formed by primary solidification is kept below 30 µm in that the molten alloy is doped with 0.05 to 2.00% by weight…

EP 0,417,826 A1#94045721 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Process for making a pressure cast reinforced fibre component
Inventors: Schmid Eberhard E Dr, Neite Guenter DrAssignee: Metallgesellschaft AgFiled 1990-08-21

In a process for the production of a fibre-reinforced component of an aluminium/silicon alloy having at least one preshaped body cast therein and comprising ceramic fibres, after insertion of the shaped fibre body and introduction of the melt into the mould the shaped fibre body…