The granular sponge iron is supplied to a roller press at temperatures of 600 to 850° C. for molding the hot briquets. There is produced a strip structure of sponge iron containing formed hot briquets, which are arranged at a distance from each other. By smashing the strip…
Schimo Siegfried
The direct reduced iron (DRI) which for at least 80 wt-% has a grain size of not more than 3 mm is melted in an electric arc furnace. The furnace contains a bath of liquid iron. During the operation of the furnace a foamy slag layer is formed on the bath and the DRI falls by…
During operation of the furnace (1), directly reduced iron is fed from above into the foam slag layer (9) through at least one movable lance (6).
According to the invention, direct reduced iron of at least 80 wt. % and having a maximum grain size of 3 mm is smelted in an electric arc furnace. The furnace contains a bath comprised of liquid iron. During operation of the furnace, a foamed slag layer forms on the bath. The…
The granular sponge iron is fed into a roller press at temperatures of 600-850 DEG C to form hot briquets. A strip structure is thereby formed from sponge iron with ausformed hot briquets separated from one another by gaps. The strip structure is smashed to isolate the hot…
Verfahren zum Schmelzen von feinkörnigem, direkt reduziertem Eisen (DRI), das zu mindestens 80 Gew.-% eine Körnung von höchstens 3 mm aufweist, in einem Elektrolichtbogenofen, der ein Bad aus flüssigem Eisen und auf dem flüssigen Eisen eine Schaumschlakkeschicht enthält, wobei…
The present invention relates to a kind of methods for the tray carriage loading the mobile grate for loose unpacked material heat treatment.In the first step, it is applied to first layer as initial bed on the stoker surface of tray carriage.In at least one second step,…
According to the invention, direct reduced iron of at least 80 wt. % and having a maximum grain size of 3 mm is smelted in an electric arc furnace. The furnace contains a bath comprised of liquid iron. During operation of the furnace, a foamed slag layer forms on the bath. The…
A method for cleaning of a roller screen transporting and screening particles by means of at least three rotating rollers. The rollers are installed in succession at given clearances and arranged transversally in relation to the transport direction of the particles to screen a…
A method of for cleaning roll screen, which is conveyed and is screened particle by least three rotating rollers.The roller is installed with given Connexin, and the lateral arrangement relative to the conveying direction of particle, to screen the particle size of desired…
1. Process for hot briqueting granular sponge iron according to which said granular sponge iron is fed into a roller press at temperatures of 600-850 degree C to form hot briquets a strip structure is thereby formed from sponge iron with ausformed hot briquets separated from one…
Procedimiento para la fusión de hierro de grano fino, reducido directamente (DRI), que presenta al menos el 80% en peso de un granulado como máximo de 3 mm, en un horno eléctrico de arco voltaico, que contiene un baño de hierro líquido y sobre éste una capa de escoria espumosa,…
Procedimiento para la fusión de hierro de grano fino, reducido directamente (DRI), que presenta al menos el 80% en peso de un granulado como máximo de 3 mm, en un horno eléctrico de arco voltaico, que contiene un baño de hierro líquido y sobre éste una capa de escoria espumosa,…
A method for charging pallet cars of a traveling grate for the thermal treatment of bulk material includes in a first step a first layer is applied as a hearth layer on a grate surface of the pallet car. In at least one second step a second layer at the same time or successively…
um processo para limpeza de uma peneira de rolo transportando e peneirando as partículas por meio de pelo menos três rolos giratórios. os rolos são instalados em sucessão em dadas folgas e dispostos transversalmente em relação à direção de transporte das partículas para…
Patente de Invenção: <B>"PROCESSO DE FUSãO DE FERRO REDUZIDO DIRETO, GRANULADO FINO EM UM FORNO DE ARCO ELéTRICO"<D>. O ferro reduzido direto (FRD) que por pelo menos 80% em peso tem um tamanho do grão de não mais do que 3 mm é fundido em um forno de arco…
The granular sponge iron is fed into a roller press at temperatures of 600-850 °C to form hat briquets. A strip structure is thereby formed from sponge iron with ausformed hot briquets separated from one another by gaps. The strip structure is smashed to isolate the hot…
The granular sponge iron is fed into a roller press at temperatures of 600-850 .degree.C to form hat briquets. A strip structure is thereby formed from sponge iron with ausformed hot briquets separated from one another by gaps. The strip structure is smashed to isolate the hot…
The starting material is lateritic ore which contains nickel oxide and/or cobalt oxide. From water and comminuted ore, of which at least 80 wt-% have grain sizes of not more than 0.5 mm, a pumpable suspension is formed. The ore-containing sus-pension is passed through an…