A crucible includes a wall made of a base material of tungsten or molybdenum or of a material based on tungsten or molybdenum. A barrier layer is disposed at least in sections on an outer side of the wall and/or in the wall. The barrier layer is made of a metallic material…
Schiftner Robert
A process for producing a glass melting component composed of refractory metal. A surface zone of the glass melting component is densified at least in sections by application of local compressive stress. As a result the surface zone has its porosity reduced compared to a volume…
The invention relates to the production of a glass-melting component (1) consisting of a refractory metal, at least some sections of a surface edge zone (2) of the glass-melting component (1) being compacted by being subjected to a local compressive stress, thus reducing their…
It is a kind of by the basis material of tungsten or molybdenum or the crucible (1) with wall (3) based on the manufacture of the material of tungsten or molybdenum, it is characterized in that barrier layer (2) are at least partly configured in the outside (6) and/or wall (3)…
Method for producing a glass melt component (1) consisting of refractory metals, wherein a surface region (2) of the glass melt component (1) is at least partially densified by applying a local compressive stress, as a result of which its porosity is reduced compared to a volume…
The invention relates to a component made of refractory metal, characterized in that the surface of the component is at least partially coated with TiB 2 A layer. The invention also relates to the manufacture of the component and to TiB 2 Use as a release agent in high…
The invention relates to a crucible (1) having a wall (3) which is made of a base material of tungsten or molybdenum or of a tungsten-based or molybdenum-based material, characterized in that a barrier layer (2) from a metallic material with a higher affinity to carbon and/or…
The invention relates to the production of a glass-melting component (1) consisting of a refractory metal, at least some sections of a surface edge zone (2) of the glass-melting component (1) being compacted by being subjected to a local compressive stress, thus reducing their…
The present invention relates to a component consisting of a refractory metal, characterized in that the surface of the component is at least partially coated with a layer of TiB 2 . The invention also relates to the production of the component and the use of TiB 2 as a…
The invention relates to a part made of a refractory metal, characterized in that the surface of the part is at least partly coated with a layer of Y2O3, to the production of the coated part, and to the use of Y2O3 as a release agent in high-temperature applications.
본 발명은 텅스텐 또는 몰리브덴의 기본 재료로, 또는 텅스텐-계 또는 몰리브덴-계 재료로, 제조된 벽(3)을 갖는 도가니(1)로서, 벽(3)의 외측 면(6) 상에 그리고/또는 벽(3) 내에, 적어도 부분적으로, 기본 재료보다 탄소 및/또는 산소에 대한 더 큰 친화도를 갖는 금속 재료로 제조된 장벽층(2)이 형성되어 있는 것을 특징으로 하는, 도가니(1)에 관한 것이다.
본 발명은 내화 금속으로 구성된 유리 용융 부품(1)을 제조하기 위한 방법으로서, 유리 용융 부품(1)의 표면 영역(2)은 국부적 압축 응력의 인가에 의해 적어도 섹션들에서 치밀화되며 그 결과 표면 영역(2) 아래에 위치하며 잔류 다공성을 갖는 체적 섹션(3)과 비교하여 감소된 다공성을 갖는 제조 방법에 관한 것이다.
FIELD: glass melting.SUBSTANCE: invention relates to a method for producing a glass melting component, as well as the glass melting component. A method for producing a glass melting component that consists of a refractory metal in which the surface area of the glass melting…
A crucible includes a wall made of a base material of tungsten or molybdenum or of a material based on tungsten or molybdenum. A barrier layer is disposed at least in sections on an outer side of the wall and/or in the wall. The barrier layer is made of a metallic material…
A process for producing a glass melting component composed of refractory metal. A surface zone of the glass melting component is densified at least in sections by application of local compressive stress. As a result the surface zone has its porosity reduced compared to a volume…
A component formed of a refractory metal has a surface that is at least partially coated with a layer of titanium diboride. There is also described a method of manufacturing the component and the application of TiB2 as a release agent in high-temperature applications.
A component formed of a refractory metal has a surface that is at least partially coated with a layer of yttria. There is also described a method of manufacturing a coated component, and the application of Y 2 O 3 as a release agent in high temperature applications.
The invention relates to a crucible (1) having a wall (3) which is made of a base material of tungsten or molybdenum or of a tungsten-based or molybdenum-based material, characterized in that a barrier layer (2) from a metallic material with a higher affinity to carbon and/or…
The present invention relates to a component consisting of a refractory metal, characterized in that the surface of the component is at least partially coated with a layer of TiB2. The invention also relates to the production of the component and the use of TiB2 as a releasing…
The invention relates to a part made of a refractory metal, characterized in that the surface of the part is at least partly coated with a layer of Y 2 O 3 , to the production of the coated part, and to the use of Y 2 O 3 as a release agent in high-temperature applications.