The invention relates to a method of manufacturing a formed aluminium alloy body-in- white ("BIW") part of a motor vehicle, the BIW part having a yield strength of more than 500 MPa after being subjected to a paint-bake cycle, the method comprising: (a) providing a…
Schepers Bruno
An aluminium alloy rolled sheet product for forming into automotive body panels, and having a yield strength of more than 160 MPa after being subjected to a paint-bake cycle, and having a gauge in a range of 0.5 to 4 mm, and preferably 0.7 to 3.5 mm, and having a composition of,…
The invention relates to a wrought aluminium-magnesium alloy product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; Cr<0.25; Fe<0.35; Si<0.2; Zr<0.25; Ti<0.3; others≦0.05, each up to a total of max.…
A method of manufacturing a formed aluminium alloy body-in-white (“BIW”) part of a motor vehicle, the BIW part having a yield strength of more than 500 MPa after being subjected to a paint-bake cycle. The method includes (a) providing a rolled aluminium sheet product of an…
Aluminium-magnesium alloy in the form of a rolled product or an extrusion, having the composition in weight percent:—Mg 4.5-5.6 Mn 0.05-0.4 Zn 0.40-0.8 Cu 0.06-0.35 Cr 0.25 max. Fe 0.35 max. Si 0.25 max. Zr 0.12 max. Ti 0.3 max. others (each) max. 0.05, (total) max. 0.15 balance…
The invention relates to an aluminium alloy rolled sheet product for forming into automotive body panels, and having a yield strength of more than 160 MPa after being subjected to a paint-bake cycle, and having a gauge in a range of 0.5 to 4 mm, and preferably 0.7 to 3.5 mm, and…
Die Erfindung betrifft ein Aluminium-Magnesium-Knetlegierungsprodukt mit folgender Zusammensetzung (in Gew.-%): 3,1 < Mg < 4,5; 0,4 < Mn < 0,85; 0,4 < Zn < 0,8; 0,06 < Cu < 0,35; Cr < 0,25; Fe < 0,35; Si < 0,2; Zr < 0,25; Ti < 0,3; andere…
The invention relates to an aluminium alloy rolled sheet product for forming into automotive body panels, and having a yield strength of more than 160 MPa after being subjected to a paint-bake cycle, and having a gauge in a range of 0.5 to 4 mm, and preferably 0.7 to 3.5 mm, and…
Die Erfindung betrifft ein gewalztes Aluminiumlegierungsblechprodukt zur Umformung in Automobilkarosserie-Formteile, und mit einer Dehngrenze von mehr als 160 MPa, nachdem es einem Einbrennzyklus unterzogen worden ist, und mit einer Stärke im Bereich von 0,5 bis 4 mm, und…
A method of making a wrought aluminium-magnesium alloy rolled product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; 0.06<Cr<0.2; Fe<0.35; Si<0.2; Zr<0.05; Ti<0.3; impurities≦0.05 each up to a…
A method of manufacturing a formed aluminum alloy body-in-white (“BIW”) part of a motor vehicle, the BIW part having a yield strength of more than 500 MPa after being subjected to a paint-bake cycle. The method includes (a) providing a rolled aluminum sheet product of an…
Ein gewalztes Aluminiumlegierungserzeugnis, das auf mindestens einer Seite von einer ein komplexes Titanfluorid enthaltenden Passivierungsschicht beschichtet ist, um die Zunahme des Kontaktwiderstandes des Erzeugnisses, wenn dieses korrosionsbewirkenden Zuständen ausgesetzt…
A method of making a wrought aluminium-magnesium alloy rolled product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; 0.06<Cr<0.2; Fe<0.35; Si<0.2; Zr<0.05; Ti<0.3; impurities≰0.05 each up to a…
The invention relates to a method of manufacturing a formed aluminium alloy body-in- white ("BIW") part of a motor vehicle, the BIW part having a yield strength of more than 500 MPa after being subjected to a paint-bake cycle, the method comprising: (a) providing a…
Method for making an aluminium-magnesium alloy in the form of a rolled product, having the composition in weight percent of: Mg 4.8-5.6, Mn 0.05-0.4, Zn 0.40-0.6, Cu 0.06-0.35, Cr 0.25 max., Fe 0.35 max., Si 0.25 max., Zr 0.12 max., Ti 0.3 max., others (each) max. 0.05, (total)…
A method of manufacturing a formed aluminium alloy body-in-white ('BIW') part of a motor vehicle, the BIW part having a yield strength of more than 500 MPa after being subjected to a paint-bake cycle. The method includes providing a rolled aluminium sheet product of an…
The invention relates to an aluminium alloy rolled sheet product for forming into automotive body panels, and having a yield strength of more than 160 MPa after being subjected to a paint-bake cycle, and having a gauge in a range of 0.5 to 4 mm, and preferably 0.7 to 3.5 mm, and…
Aluminium-magnesium alloy in the form of a rolled product or an extrusion, having the composition in weight percent:- Mg 4.5-5.6 Mn 0.05-0.4 Zn 0.40-0.8 Cu 0.06-0.35 Cr 0.25 max. Fe 0.35 max. Si 0.25 max. Zr 0.12 max. Ti 0.3 max. others (each) max. 0.05, (total) max. 0.15…
Aluminium-magnesium alloy in the form of a rolled product or an extrusion, having the composition in weight percent:- Mg 4.5-5.6 Mn 0.05-0.4 Zn 0.40-0.8 Cu 0.06-0.35 Cr 0.25 max. Fe 0.35 max. Si 0.25 max. Zr 0.12 max. Ti 0.3 max. others (each) max. 0.05, (total) max. 0.15…
An aluminum alloy rolled sheet product for forming into automotive body panels, and having a yield strength of more than 160 MPa after being subjected to a paint-bake cycle, and having a gauge in a range of 0.5 to 4 mm, and preferably 0.7 to 3.5 mm, and having a composition of,…
Method for making an aluminium-magnesium alloy in the form of a rolled product, having the composition in weight percent of: Mg 4.8-5.6, Mn 0.05-0.4, Zn 0.40-0.6, Cu 0.06-0.35, Cr 0.25 max., Fe 0.35 max., Si 0.25 max., Zr 0.12 max., Ti 0.3 max., others (each) max. 0.05, (total)…
A method of making a wrought aluminium-magnesium alloy rolled product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; 0.06<Cr<0.2; Fe<0.35; Si<0.2; Zr<0.05; Ti<0.3; impurities≰0.05 each up to a…
Die Erfindung betrifft ein gewalztes Aluminiumblechprodukt mit einer Stärke im Bereich von 0,5 bis 3,5 mm und einer im Wesentlichen rekristallisierten Mikrostruktur und einer chemischen Zusammensetzung von, in Gew.-%, Mg 4,5% bis 6,5%, Zn 1,1% bis 1,9%, entweder Mn 0,04% bis…
Aluminium-Magnesiumlegierung in Form eines Walzprodukts oder eines Strangpreßprofils mit folgender Zusammensetzung in Gew.-%: DOLLAR A Mg 4,5-5,6 DOLLAR A Mn 0,05-0,4 DOLLAR A Zn 0,40-0,8 DOLLAR A Cu 0,06-0,35 DOLLAR A Cr 0,25 max. DOLLAR A Fe 0,35 max. DOLLAR A Si 0,25 max.…