Powder additive for powder metallurgy. The surface of the body of powder additive for use in powder metallurgy is coated with an organic binder, thereby obtaining powder additive to cause adhesion of the powder additive to the surface of iron-based powder by the organic binder,…
Satoshi Uenosono
In a Cr-Cu alloy that is formed by powder metallurgy and contains a Cu matrix and flattened Cr phases, the Cr content in the Cr-Cu alloy is more than 30% to 80% or less by mass, and the average aspect ratio of the flattened Cr phases is more than 1.0 and less than 100. The Cr-Cu…
A pure iron powder which contains as impurities, in terms of mass%, up to 0.005% C, 0.01-0.03%, excluding 0.01%, Si, 0.03-0.07% Mn, up to 0.01% P, up to 0.01% S, up to 0.10% O, and up to 0.001% N. The iron powder particles each is composed of up to four crystal grains on the…
An alloy steel powder for powder metallurgy includes an iron-based powder containing about 0.5 mass percent or less of Mn as a prealloyed element and 0.2 to about 1.5 mass percent of Mo as a prealloyed element; and a Mo-containing alloy powder bonded on the surface of the…
In the case where Mn: 0.5 mass% or less and Mo: 0.2 to 1.5 mass% of Mo is diffused and adhered to the surface of the iron-based powder to form an alloy steel powder, and Ni powder: 0.2-5 mass% and/or Cu powder: 0.2 to 3 mass% of a powder mixture for powder metallurgy. The mixed…
The invention aims to provide an alloy part for heat dissipation which has low thermal expansion coefficient like the prior composite material, high thermal conductivity like pure copper and excellent machinability and a manufacturing method thereof. In particular, since various…
A method for manufacturing sponge iron includes heating iron oxide together with a solid reducing agent to reduce the iron oxide into sponge iron, wherein the iron oxide includes a mixture of powdered hematite and powdered iron ore or a mixture of powdered hematite and powdered…
An alloy steel powder for powder metallurgy includes an iron-based powder containing about 0.5 mass percent or less of Mn as a prealloyed element and 0.2 to about 1.5 mass percent of Mo as a prealloyed element; and a Mo-containing alloy powder bonded on the surface of the…
In a method for producing sponge iron by heating iron oxide and a solid reducing agent together and reducing the iron oxide into sponge iron, a mixed powder of fine hematite powder and iron ore powder or a mixed powder of fine hematite powder and mill scale powder is used as the…
The invention provides an iron-based mixed powder for powder metallurgy enabling the iron-based mixed powder to improve the machinability, without being accompanied by degrading the mechanical property of a sintered body. In order to obtain the purpose of the invention, the…