The present invention relates to an improved process for compounding a polyolefin composition comprising providing feed components including one or more high molecular weight olefin polymer components and one or more low molecular weight polyolefin components. The high and low…
Sander Robert E
An ethylene homopolymer having a density of from about 0.956 to about 0.970 g/cm 3 and a high load melt index (190° C. and 21.6 kg) of from about 7 to about 21 g/10 min. A continuous polymerization process for the production of the ethylene homopolymer, in the presence of a…
The present invention relates to an improved process for compounding a polyolefin composition comprising providing feed components including one or more high molecular weight olefin polymer components and one or more low molecular weight polyolefin components. The high and low…
An ethylene homopolymer having a density of from about 0.956 to about 0.970 g/cm3 and a high load melt index (190 °C and 21.6 kg) of from about 7 to about 21 g/10 min. A continuous polymerization process for the production of the ethylene homopolymer, in the presence of a…
The present invention relates to an improved process for compounding a polyolefin composition comprising providing feed components including one or more high molecular weight olefin polymer components and one or more low molecular weight polyolefin components. The high and low…