Patents
US 4,259,118 A#756893 Most Cited · 56 citations1.2/yr · PR 7.75ExpiredUS · Utility
Thermally high pre-stressable glass with high hot stressing factors
Inventors: Sack WernerAssignee: Jenaer Glaswerk Schott & GenFiled 1980-05-05 · Granted 1981-03-31

Glass compositions have been found which, with a low linear thermal expansion coefficient of 33.9-53.2×10 -7 /°C. at 20-300° C. will pre-stress to a much higher extent under similar prestressing conditions than known glasses of the same thermal expansion, and which consequently…

US 4,315,054 A#1110314 Most Cited · 46 citations1.1/yr · PR 2.54ExpiredUS · Utility
Crack-resistant, heat-absorbing fusion glasses enabling low processing temperatures for the hermetic encapsulation of electronic components
Inventors: Sack Werner, Lindig OttoAssignee: Schott GlaswerkeFiled 1980-07-30 · Granted 1982-02-09

A fusion glass of the series SiO2-Al2O3-Na2O-PbO-Fe3O4 consists essentially of 43.0-46.2% by weight of SiO2; 1.0-2.0% by weight of Al2O3; 6.2-16.0% by weight of Na2O; 33.0-46.1% by weight of PbO; 2.0-4.5% by weight of Fe3O4; and a maximum of 0.2% by weight of Sb2O3, all…

US 3,617,317 A#2952164 Most Cited · 25 citations0.5/yr · PR 7.44ExpiredUS · Utility
Glass batches for the production of transparent glass ceramics containing solid solutions of {62 -eucryptite
Inventors: Sack Werner, Scheidler HerwigAssignee: Jenaer Glaswerk Schott & GenFiled 1968-06-26 · Granted 1971-11-02

Glass having the following composition: SiO2 67.7-69.6 Al2O3 18.7-19.2 Li2O 2.8-2.9 Na2O 0.7 CaO 0.8-2.2 MgO 0.0-2.5 ZnO 0.0-5.2 TiO2 1.5 ZrO2 1.8 Sb2O3 1.0 the sum of CaO+MgO+ZnO being 3.3-5.8 percent by weight and the weight ratio of MgO+ZnO/CaO being between 1.4 and 6.6.…

US 4,298,388 A#4426741 Most Cited · 19 citations0.4/yr · PR 5.00ExpiredUS · Utility
Alkali-free sealing glasses for molybdenum
Inventors: Sack WernerAssignee: Jenaer Glaswerk Schott & GenFiled 1980-10-08 · Granted 1981-11-03

SiO 2 -Al 2 O 3 -alkaline earth oxides glass compositions suitable for glass/molybdenum sealings with high thermal load capability, having coefficients of thermal expansion in the temperature range of 20°-300° C. of 4.6-5.1×10 -6 /° C., glass transformation temperatures (Tg) of…

US 3,672,919 A#4724149 Most Cited · 18 citations0.3/yr · PR 7.25ExpiredUS · Utility
Sealing glass having high absorption of infrared radiation
Inventors: Sack WernerAssignee: Jenaer Glaswerk Schott & GenFiled 1969-09-19 · Granted 1972-06-27

GLASS WHICH IS HEAT ABSORBING AND ELECTRICALLY HIGHLY INSULATING AND SUITABLE FOR SEALING OF ELEMENTS OF NICKELCHROMIUM-IRON AND NICKEL-MANGANESE-IRON ALLOYS CONTAINING IRON (II) OXIDE IN AN AMOUNT PROVIDING HIGH INFRARED ABSORPTION AT 1-2 UN. AND LESS THAN 20% BY WEIGHT OF PBO.

US 4,001,741 A#6573235 Most Cited · 14 citations0.3/yr · PR 5.94ExpiredUS · Utility
Low working temperature reed glasses
Inventors: Lindig Otto, Sack WernerAssignee: Jenaer Glaswerk Schott & GenFiled 1976-01-28 · Granted 1977-01-04

A glass having a softening temperature (E W ) between 596° and 634° C. and a working temperature (V A ) between 792° and 863° C., said glass being produced from a melt having a composition expressed in percentages by weight as follows: ______________________________________ SiO…

EP 0,132,751 A1#7827945 Most Cited · 13 citations0.3/yr · PR 1.80PendingEP · Application
Tungsten-sealing glasses with high thermal load capability
Inventors: Sack Werner Dr Dipl-chemAssignee: Schott Glaswerke, Zeiss StiftungFiled 1984-07-17

1. Glass composition for a glass-/tungsten seal capable of withstanding high thermal stress, having coefficients of heat expansion between about 4,02 and 4,17 - 10**-6 /degrees C in the temperature range between 20 and 300 degrees C, characterized in that the transformation…

US 4,515,897 A#8517672 Most Cited · 12 citations0.3/yr · PR 2.11ExpiredUS · Utility
Crystallizing glass solders and stripping films with such glass solder imprinted thereon
Inventors: Sack Werner, Kiefer WernerAssignee: Schott GlaswerkeFiled 1984-01-23 · Granted 1985-05-07

Partially crystallizing glass solders, and stripping films using them as agents to be transferred, which are sintered at temperatures below 900° C. from glass powder with granulation of less than <150 μm, thereafter exhibiting thermal expansion coefficients of -23.5 to…

US 4,007,048 A#9745654 Most Cited · 10 citations0.2/yr · PR 7.94ExpiredUS · Utility
Dark red transparent refractory glass
Inventors: Sack Werner, Scheidler HerwigAssignee: Jenaer Glaswerk Schott & GenFiled 1975-06-17 · Granted 1977-02-08

Glass ceramic and the process for producing a dark red glass ceramic comprising the production of basic glass by melting at about 1620° C a mixture of approximate percentages of sand 53.30%, hydrated alumina 27.15%, zirconium silicate 1.90%, titanium oxide 2.02%, lithium…

DE 2,429,563 B1#12357544 Most Cited · 8 citations0.2/yr · PR 6.21ExpiredDE · Utility
Durchsichtige, in der Aufsicht schwarze, in der Durchsicht dunkelrote Glaskeramik des Systems SiO tief 2-AI tief 2 O tief 3-Li tief 2 O mit hohem Wärmespannungsfaktor R größer als 1000, insbesondere zur Herstellung von beheizbaren Platten, sowie Verfahren zur Herstellung der Glaskeramik Jenaer Glaswerk Schott & Gen., 6500 Mainz

EP 2,474,659 A1#14481314 Most Cited · 7 citations0.5/yr · PR 2.35PendingEP · Application
Drum with curved structure for a washing machine

The drum (3) has a cylinder-shaped casing (19) limited by a front wall (20) and comprising a curvature structure, where the structure has curved segments (22). Channels are formed between the segments, and holes (25) for passing washing liquid are arranged in the channels, where…

US 4,599,319 A#23510851 Most Cited · 4 citations0.1/yr · PR 1.65ExpiredUS · Utility
PbO-free glasses for cathode ray tubes having a high protective effect against X-rays while simultaneously having good resistance to acid and stability to radiation
Inventors: Sack WernerAssignee: Schott GlasswerkeFiled 1984-07-06 · Granted 1986-07-08

New, PbO-free glasses for cathode ray tubes are composed of (in % by weight) 50-52 SiO2; 0-3 Al2O3; 1-1.7 Li2O; 6.5-10.7 Na2O; 0-4.5 K2O; 0.4-1.4 F; 0-0.5 TiO2; 0.2-1.2 CeO2; 0-5 ZnO; 0-7.0 BaO; 15-22 SrO; and 6.3-10.3 ZrO2, and are characterized by a high protective effect…

DE 2,756,555 B2#29542197 Most Cited · 3 citations0.1/yr · PR 1.30ExpiredDE · Utility
Thermisch™·5!»»"1«1™ Gläser mit hoher Temperaturwechselfestigkeit und Wärmedehnungskoeffizienten im Temperaturbereich von 20 bis 300 Grad C von 33,9 bis 53,2 mal 107 Grad C auf der Basis SiO2 - B2 O3 -Al2O3-Na2O

DE 2,419,724 A1#35553562 Most Cited · 2 citations0.0/yr · PR 1.30PendingDE · Application
Borosilicate glass opacified with barium phosphate - having good resistance against thermal shocks

Borosilicate glass opacified with barium phosphate, having good resistance against thermal shocks, consists of (in wt.%): siO2 71-76.2, B2O3 11-15.5, Al2O3 2.5-4.5, Li2O 0-1.5, Na2O 0.5-5, K2O 0-2.5 (Li2O + Na2O + K2O = 2-6.2), BaO 1.3-8.5, P2O5 1.5-2.2, and NaCl as refining…

DE 2,433,752 A1#34703981 Most Cited · 2 citations0.0/yr · PR 1.57PendingDE · Application
Glass for colour television screens - contg. no fluorine and arsenic oxide and contg. cerium oxide and opt. antimony oxide
Inventors: Sack Werner Dipl Chem DrAssignee: Jenaer Glaswerk Schott & GenFiled 1974-07-13

Glass compsn. for television screens are free from F and As2O3. High resistance to radiation is obtd. by clarifying with CeO2 alone or with CeO2 + Sb2O3 with simultaneous introduction of a small TiO2 addn. High X-ray protection is achieved by simultaneous introduction of PbO +…

DE 3,116,317 A1#37299495 Most Cited · 2 citations0.1/yr · PR 1.11PendingDE · Application
Emergency signal lamp or similar indicator luminaire
Inventors: Sack WernerAssignee: Sack WernerFiled 1981-04-24

The invention relates to an emergency signal luminaire or similar indicator luminaire, at least one electric lamp being accommodated in a lamp housing and at least one surface of the housing being constructed as a transilluminated signal face containing a message, and the…

DE 3,302,774 A1#34714995 Most Cited · 2 citations0.1/yr · PR 1.56PendingDE · Application
Crystallising glass solders having low coefficients of thermal expansion

Partially crystallising glass solders which are sintered at temperatures below 900 DEG C from glass powders having particle sizes of < 150 mu m and then have coefficients of thermal expansion of from -23.5 to 34.3 . 10<7> . K<-1>, whose crystallisation temperature…

EP 0,023,312 A1#41322467 Most Cited · 2 citations0.0/yr · PR 0.98PendingEP · Application
Crack-free, heat absorbing sealing glasses with low working temperatures for hermetically encapsulating electronic components
Inventors: Sack Werner, Lindig OttoAssignee: Schott GlaswerkeFiled 1980-07-16

Es werden neidrig erweichende wärmeabsorbierende Verschmelzgläser zur hermetischen Kapselung elektrotechnischer Bauteile, insbesondere sowohl magnetisch als auch nicht magnetisch betätigter Leiterkontakte vorgeschlagen, welche folgende Zusammensetzungen aufweisen: SiO2 43,0 -…

GB 1,057,907 A#35778771 Most Cited · 2 citations0.0/yr · PR 1.25ExpiredGB · Utility
Improvements in or relating to glass
Inventors: Sack WernerAssignee: Zeiss StiftungFiled 1964-02-21

A lead-free silicate glass is composed, in per cent by weight, of: SiO2, 57.4-71.1; Na2O, 3-4; K2O, 13.5-16.4; BaO, 5.5-12.5; F, 1.4-2.0; B2O3, 0-10.7; Al2O3, 0-3; Li2O, 0-1; CaO, 0-2; TiO2, 0-3. It may also include 0.1-0.4% As2O3 and/or Sb2O3. The glass may be fused to an alloy…