CN 105,745,345 A#17534159 Most Cited · 6 citations0.6/yr · PR 1.68ActiveCN · Utility
Titanium-free alloy
Inventors: Rosenberg Julia, Klower JuttaAssignee: VDM Metals GmbHFiled 2015-02-10

Titanium-free alloys with high pitting and crevice corrosion resistance and high yield limit in the cold work hardened state with (in weight%) at most 0.02% C, at most 0.01% S, at most 0.03% N, 20.0-23.0% Cr, 39.0-44.0% Ni, 0.4- < 1.0% Mn, 0.1- < 0.5% Si, >4.0- <…

US 10,174,397 B2#25673035 Most Cited · 4 citations0.6/yr · PR 1.28ActiveUS · Utility
Titanium-free alloy
Inventors: Rosenberg Julia, Kloewer JuttaAssignee: Vdm Metals Int GmbhFiled 2015-02-10 · Granted 2019-01-08

Titanium-free alloy which has great resistance to pitting and crevice corrosion and a high yield point in the strain-hardened state and includes (in wt %) a maximum of 0.02% C, a maximum of 0.01% S, a maximum of 0.03% N, 20.0-23.0% Cr, 39.0-44.0% Ni, 0.4-<1.0% Mn,…

US 2017002437 A1#25673034 Most Cited · 4 citations0.4/yr · PR 1.28PendingUS · Application
Titanium-free alloy
Inventors: Rosenberg Julia, Kloewer JuttaAssignee: Vdm Metals Int GmbhFiled 2015-02-10

Titanium-free alloy which has great resistance to pitting and crevice corrosion and a high yield point in the strain-hardened state and includes (in wt %) a maximum of 0.02% C, a maximum of 0.01% S, a maximum of 0.03% N, 20.0-23.0% Cr, 39.0-44.0% Ni, 0.4-<1.0% Mn,…

DE 102014002402 A1#34752836 Most Cited · 2 citations0.2/yr · PR 1.54PendingDE · Application
Titanfreie Legierung
Inventors: KlÖwer Jutta, Rosenberg JuliaAssignee: VDM Metals GmbHFiled 2014-02-13

Titanfreie Legierung mit hoher Lochfraß- und Spaltkorrosionsbeständigkeit sowie hoher Streckgrenze im kaltverfestigten Zustand, mit (in Gew.-%) C max. 0,02% S max. 0,01% N max. 0,03% Cr 20,0–23,0% Ni 39,0–44,0% Mn 0,4–< 1,0% Si 0,1–< 0,5% Mo > 4,0–< 7,0% N b max.…

WO 2015/120832 A1#36979855 Most Cited · 2 citations0.2/yr · PR 1.13PendingWO · Application
Titanium-free alloy
Inventors: Rosenberg Julia, KlÖwer JuttaAssignee: VDM Metals GmbHFiled 2015-02-10

Titanium-free alloy which has great resistance to pitting and crevice corrosion and a high yield point in the strain-hardened state and comprises (in wt%) a maximum of 0.02% C, a maximum of 0.01% S, a maximum of 0.03% N, 20.0-23.0% Cr, 39.0-44.0% Ni, 0.4 - < 1.0 % Mn, 0.1 -…

EP 3,105,358 A1#47425156 Most Cited · 1 citations0.1/yr · PR 0.96PendingEP · Application
Titanium-free alloy
Inventors: Rosenberg Julia, KlÖwer JuttaAssignee: Vdm Metals Int GmbhFiled 2015-02-10

Titanium-free alloy which has great resistance to pitting and crevice corrosion and a high yield point in the strain-hardened state and comprises (in wt%) a maximum of 0.02% C, a maximum of 0.01% S, a maximum of 0.03% N, 20.0-23.0% Cr, 39.0-44.0% Ni, 0.4 - < 1.0 % Mn, 0.1 -…

CN 114,000,032 A#130097244 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Titanium-free alloy
Inventors: Klower Jutta, Rosenberg JuliaAssignee: Vdm Metals Int GmbhFiled 2015-02-10

Titanium-free alloys with high pitting and crevice corrosion resistance and high yield limit in the cold work hardened state with (in weight%) at most 0.02% C, at most 0.01% S, at most 0.03% N, 20.0-23.0% Cr, 39.0-44.0% Ni, 0.4- < 1.0% Mn, 0.1- < 0.5% Si, >4.0- <…

DE 102014002693 A1#128662616 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Titanfreie Legierung
Inventors: KlÖwer Jutta, Rosenberg JuliaAssignee: VDM Metals GmbHFiled 2014-02-28

Titanfreie Legierung mit hoher Lochfraß- und Spaltkorrosionsbeständigkeit sowie hoher Streckgrenze im kaltverfestigten Zustand, mit (in Gew.-%)C max. 0,02% S max. 0,01% N max. 0,03% Cr 20,0–23,0% Ni 39,0–44,0% Mn 0,4–< 1,0% Si 0,1–< 0,5% Mo > 4,0–< 7,0% Nb max. 0,15%…

KR 20160135168 A#101992981 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
Titanium-free alloy
Inventors: Rosenberg Julia, Klower JuttaAssignee: Vdm Metals Int GmbhFiled 2015-02-10

점식 및 균열 부식에 대한 큰 저항성, 및 응력-경화 상태에서의 높은 항복점을 갖는 티타늄-무함유 합금은, 최대 0.02 wt%의 C; 최대 0.01 wt%의 S; 최대 0.03 wt%의 N; 20.0 wt% 내지 23.0 wt%의 Cr; 39.0 wt% 내지 44.0 wt%의 Ni; 0.4 wt% 내지 1.0 wt% 미만의 Mn; 0.1 wt% 내지 0.5 wt% 미만의 Si; 4.0 wt% 초과 내지 7.0 wt% 미만의 Mo; 최대 0.15 wt%의 Nb; 1.5 wt% 초과 내지 2.5…

US 11,441,217 B2#139318508 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method for producing semi-finished products from a nickel-based alloy
Inventors: Kloewer Jutta, Aghajani Ali, Kraemer Geb Rosenberg JuliaAssignee: Vdm Metals Int GmbhFiled 2018-12-07 · Granted 2022-09-13

A method produces semi-finished products from a nickel-based alloy having the composition (in wt. %): Ni>50-<55%, Cr>17-<21%, Nb>4.8-<5.2%, Mo>2.8-<3.3%, Ti>0.8-<1.15%, Al>0.4-<0.6%, C maximum 0.045%, Co maximum 1.0%, Mn maximum 0.35%, Si…

US 2020325567 A1#154724431 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method for producing semi-finished products from a nickel-based alloy

A method produces semi-finished products from a nickel-based alloy having the composition (in wt. %): Ni>50 -<55%, Cr>17-<21%, Nb>4.8-<5.2%, Mo>2.8-<3.3%, Ti>0.8-<1.15%, Al>0.4-<0.6%, C maximum 0.045%, Co maximum 1.0%, Mn maximum 0.35%, Si…

WO 2019/114875 A1#129720634 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for producing semi-finished products from a nickel-based alloy

The invention relates to a method for producing semi-finished products from a nickel-based alloy having the following composition (in wt.%): Ni > 50 - < 55%, Cr > 17 - < 21%, Nb > 4.8 - < 5.2%, Mo > 2.8 - < 3.3%, Ti > 0.8 - < 1.15%, Al > 0.4 -…