Robert Mackay
A rippled wafer is formed of a convoluted wafer ribbon (80). It has an average of >=12 turns/cm 2>, where a turn is a change in direction of the wafer ribbon of >=45[deg].
A rippled wafer (90) formed of a convoluted wafer ribbon (80), the rippled wafer (90) having an average of at least 12 turns/cm2, wherein a turn is a change in direction of the wafer ribbon (80) of at least 45°, and a confectionery product comprising such a wafer. Also a…
A rippled wafer ( 90 ) formed of a convoluted wafer ribbon ( 80 ), the rippled wafer ( 90 ) having an average of at least 12 turns/cm 2 , wherein a turn is a change in direction of the wafer ribbon ( 80 ) of at least 45°, and a confectionery product comprising such a wafer. Also…
A rippled wafer is formed of a convoluted wafer ribbon (80). It has an average of >=12 turns/cm 2>, where a turn is a change in direction of the wafer ribbon of >=45[deg].
A rippled wafer is formed of a convoluted wafer ribbon (80). It has an average of >=12 turns/cm 2>, where a turn is a change in direction of the wafer ribbon of >=45[deg].
A rippled wafer is formed of a convoluted wafer ribbon (80). It has an average of >=12 turns/cm 2>, where a turn is a change in direction of the wafer ribbon of >=45[deg].
A rippled wafer is formed of a convoluted wafer ribbon (80). It has an average of >=12 turns/cm 2>, where a turn is a change in direction of the wafer ribbon of >=45[deg].
A rippled wafer is formed of a convoluted wafer ribbon (80). It has an average of >=12 turns/cm 2>, where a turn is a change in direction of the wafer ribbon of >=45[deg].
A rippled wafer is formed of a convoluted wafer ribbon, the rippled wafer having an average of at least 12 turns/cmé, wherein a turn is a change in direction of the wafer ribbon of at least 45{. The wafer is baked on a heated drum 20, removed by blade 50 and convoluted in…