A steel strip having a coating of a metal alloy on at least one surface of the strip is disclosed. The metal alloy contains aluminium, zinc, silicon, and magnesium as the major elements. The metal alloy also contains strontium and/or calcium and unavoidable impurities and…
Renshaw Wayne
A method of controlling “rough coating” and “pinhole - uncoated” surface defects on a steel strip coated with a aluminium-zinc-silicon alloy. The alloy has 50-60 %wt Al, 37-46 %wt Zn and 1.2-2.3 %wt Si. The method includes heat treating the steel strip in a heat treatment…
An Al-Zn-Si-Mg alloy coated strip that has Mg 2 Si particles in the coating microstructure is disclosed. The distribution of Mg 2 Si particles is such that the surface of the coating has only a small proportion of Mg 2 Si particles or is at least substantially free of any Mg 2…
A method of controlling “rough coating” and “pinhole-uncoated” surface defects on a steel strip coated with a aluminum-zinc-silicon alloy. The alloy has 50-60 % wt Al, 37-46 % wt Zn and 1.2-2.3 % wt Si. The method includes heat treating the steel strip in a heat treatment…
A steel strip having a coating of a metal alloy on at least one surface of the strip is disclosed. The metal alloy contains aluminium, zinc, silicon, and magnesium as the major elements. The metal alloy also contains strontium and/or calcium and unavoidable impurities and…
A method of forming a coating of an Al-Zn-Si-Mg alloy on a steel strip to form an Al-Zn-Mg-Si coated steel strip is disclosed. The method includes the steps of dipping steel strip into a bath of molten Al-Zn-Si-Mg alloy and forming a coating of the alloy on exposed surfaces of…
A hot dip method of forming an Al-Zn-Si-Mg alloy coating on a strip is disclosed. The method includes controlling the conditions in the molten bath to minimise the top dross layer in the molten bath. In particular, the method includes controlling top dross formation by including…
An Al-Zn-Si-Mg alloy coated strip that has Mg 2 Si particles in the coating microstructure is disclosed. The distribution of Mg 2 Si particles is such that a surface region of the coating has only a small proportion of Mg 2 Si particles or is at least substantially free of any…
Red rust staining of Al/Zn coated steel strip in “acid rain” or “polluted” environments can be minimised by forming the coating as an Al—Zn—Si—Mg alloy coating with an OT:SDAS ratio greater than a value of 0.5:1, where OT is the overlay thickness on a surface of the strip and…
A method of forming a coating of an Al-Zn-Si-Mg alloy on a steel strip to form an Al-Zn-Mg-Si coated steel strip is disclosed. The method includes the steps of dipping steel strip into a bath of molten Al-Zn-Si-Mg alloy and forming a coating of the alloy on exposed surfaces of…
A method of forming a coating of an Al-Zn-Si-Mg alloy on a steel strip to form an Al-Zn-Mg-Si coated steel strip is disclosed. The method comprises the following steps: dipping a steel strip into a bath of molten Al-Zn-Si-Mg alloy to form a coating of the Al-Zn-Si-Mg alloy on…
A method of controlling ''rough coating'' and ''pinhole - uncoated'' surface defects on a steel strip coated with a aluminium-zinc-silicon alloy. The alloy has 50-60 %wt Al, 37-46 %wt Zn and 1.2-2.3 %wt Si. The method includes heat treating the…
An Al—Zn—Si—Mg alloy coated strip that has Mg 2 Si particles in the coating microstructure is disclosed. The distribution of Mg 2 Si particles is such that a surface region of the coating has only a small proportion of Mg 2 Si particles or is at least substantially free of any…
A hot dip method of forming an Al-Zn-Si-Mg alloy coating on a strip is disclosed. The method includes controlling the conditions in the molten bath to minimise the top dross layer in the molten bath. In particular, the method includes controlling top dross formation by including…
Red rust staining of Al/Zn coated steel strip in "acid rain" or "polluted" environments can be minimised by forming the coating as an Al-Zn-Si-Mg alloy coating with an OT:SDAS ratio greater than a value of 0.5:1, where OT is the overlay thickness on a surface of…
PROBLEM TO BE SOLVED: To reduce red rust stain of an Al/Zn film steel strip in "acid rain" and "contamination" environment, and corrosion at a cross section edge in marine environment.SOLUTION: The invention relates to an Al-Zn-Si-Mg alloy film on a steel strip…
Disclosed is a steel strip having a coating of a metal alloy on at least one surface of the strip, wherein the metal alloy contains aluminium, zinc, silicon, and magnesium as the major elements and also contains strontium and/or calcium and unavoidable impurities and optionally…
An Al—Zn—Si—Mg alloy coated strip that has Mg 2 Si particles in the coating microstructure is disclosed. The distribution of Mg 2 Si particles is such that the surface of the coating has only a small proportion of Mg 2 Si particles or is at least substantially free of any Mg 2…
A method of controlling “rough coating” and “pinhole-uncoated” surface defects on a steel strip coated with a aluminum-zinc-silicon alloy. The alloy has 50-60% wt Al, 37-46% wt Zn and 1.2-2.3% wt Si. The method includes heat treating the steel strip in a heat treatment furnace…
A hot dip method of forming an Al—Zn—Si—Mg alloy coating on a strip is disclosed. The method includes controlling the conditions in the molten bath to minimise the top dross layer in the molten bath. In particular, the method includes controlling top dross formation by including…
A method of forming an Al—Zn—Si—Mg alloy coating on a steel strip includes dipping steel strip into a bath of molten Al—Zn—Si—Mg alloy and forming a coating of the alloy on exposed surfaces of the steel strip. The method also includes controlling conditions in the molten coating…
A method of forming a coating of an Al—Zn—Si—Mg alloy on a steel strip to form an Al—Zn—Mg—Si coated steel strip is disclosed. The method includes the steps of dipping steel strip into a bath of molten Al—Zn—Si—Mg alloy and forming a coating of the alloy on exposed surfaces of…
Red rust staining of Al / Zn coated steel strip in "acid rain" or "polluted" environments can be minimised by forming the coating as an Al-Zn-Si-Mg alloy coating with an OT : SDAS ratio greater than a value of 0.5:1, where OT is the overlay thickness on a surface…
A method of forming a coating of an Al-Zn-Si-Mg alloy on a steel strip to form an Al-Zn-Mg-Si coated steel strip is disclosed. The method includes the steps of dipping steel strip into a bath of molten Al-Zn-Si-Mg alloy and forming a coating of the alloy on exposed surfaces of…
A method of forming a coating of an Al-Zn-Si-Mg alloy on a steel strip to form an Al-Zn-Mg-Si coated steel 5 strip is disclosed. The method includes the steps of dipping steel strip into a bath of molten Al-Zn-Si-Mg alloy and forming a coating of the alloy on exposed surfaces of…