A container is made by attaching an inner member to a rotational mold, extending across the interior of the mold and terminating near the interior surface, and forming a container in the mold by rotational molding.
Rees Robert L
A method of molding polymeric materials, such as olefin polymers, in a mold which has a release coating of 50-90 parts by weight polyphenylene sulfide, up to 10 parts by weight polytetrafluorethylene and a filler in an amount of 10-50 parts by weight. The release coating can be…
A hollow multilayered article is rotationally molded by introducing into the mold particles of a hompolymer or copolymer of ethylene containing a crosslinking agent and heating the mold during rotation thereof to melt this first polymeric layer. Solid particles of a different…
As an article of manufacture, a football blocking dummy useful in teaching the fundamentals of blocking and tackling is provided which has in the upper portion of the article integrally positioned therein a grasping means which protects the hands, wrists, and fingers of the…
A hand-held calculating device for calculating Federal Income Taxes or the like includes substantially flat, elongate front and rear cover members and an insert card. Suitable structure is provided for joining the cover members with the card slidably insertable therebetween. The…
Polymers of ethylene having a melt index of at least 10 are simultaneously rotationally molded and crosslinked by an acetylenic diperoxy compound to produce molded articles having high impact strength and stress cracking resistance.
Compsn. comprises a copolymer of ethylene with propylene or a 5-8C olefin, or a shear-cracked ethylene homo- or co-polymer of fused mass idex greater than 5 (pref. 10-200), and 0.1-10 wt. pts. (per 100 pts. polymer) of (i) RO.O.C.(CH3)2C=CC(CH3)2O.OR, (ii)…
1345400 Crosslinking ethylene polymers PHILLIPS PETROLEUM CO 1 Sept 1971 [2 Sept 1970] 40809/71 Addition to 1295354 Heading C3P Moulding compositions comprise (1) an ethylene polymer of melt index at least 5, density 0À920 to 0À970 gm./cc. and molecular weight distribution not…