Patents
Inventor / Author Profile

Record Loren E

53Total Forward Citations
5Indexed Patents
4Patent H-Index
US 5,394,420 A#2495387 Most Cited · 28 citations0.9/yr · PR 6.21ExpiredUS · Utility
Multiform crystal and apparatus for fabrication
Inventors: Senn Robert H, Record Loren EAssignee: Trw IncFiled 1994-01-27 · Granted 1995-02-28

A multiform crystal 10 suitable for laser applications is described. The multiform crystal 10 comprises at least two single crystal segments 12 fused together with a joint 14 therebetween, the joint being substantially optically transparent to light propagating through the…

US 5,548,606 A#7284533 Most Cited · 13 citations0.4/yr · PR 3.88ExpiredUS · Utility
Multiform crystal and apparatus for fabrication
Inventors: Senn Robert H, Record Loren EAssignee: Trw IncFiled 1994-10-31 · Granted 1996-08-20

A multiform crystal 10 suitable for laser applications is described. The multiform crystal 10 comprises at least two single crystal segments 12 fused together with a joint 14 therebetween, the joint being substantially optically transparent to light propagating through the…

US 6,405,918 B1#18712528 Most Cited · 6 citations0.2/yr · PR 1.32ExpiredUS · Utility
Mechanical retention system for braze and solder joints
Inventors: Claridge Rex C, Adams Christopher M, Luevano Annetta J, Record Loren EAssignee: Trw IncFiled 2000-10-30 · Granted 2002-06-18

Brazing or soldering of pieces of low wettable materials ( 1, 3 ), such as single crystal silicon, is accomplished by sandwiching the brazing material ( 5 ) between the pieces and sealing the edges of the brazing material with a tape ( 11 ) wrapped about the periphery of the…

DE 19,549,513 B4#53388029 Most Cited · 1 citations0.1/yr · PR 0.82ExpiredDE · Utility
Multi-form crystal fabrication process
Inventors: Senn Robert H, Record Loren EAssignee: Northrop Grumman Corp N D GesFiled 1995-01-18 · Granted 2004-04-15

A process for joining single crystal segments to form a multiform crystal involves the steps of polishing two single crystal segments to form at least one optically flat face on each of the crystal segments. The optically flat face has a roughness of less than 1/2 the wavelength…