Patents
Inventor / Author Profile

Rasquin Andre

24Total Forward Citations
7Indexed Patents
2Patent H-Index
US 4,609,529 A#5592502 Most Cited · 16 citations0.4/yr · PR 4.39ExpiredUS · Utility
Zinc-based alloys with improved ductility
Inventors: Skenazi Andre, Coutsouradis Dimitri, Rasquin AndreAssignee: Centre Rech MetallurgiqueFiled 1984-02-08 · Granted 1986-09-02

The ductility and/or tensile strength of certain zinc-based alloys (25 to 40 wt. % aluminum, 0.5 to 5 wt. % copper, and up to 0.1 wt. % magnesium) are improved when various elements are added. A first series of improved alloys is comprised of boron (between 5 ppm and 0.1 wt. %),…

WO 9,313,230 A1#34195600 Most Cited · 2 citations0.1/yr · PR 3.80PendingWO · Application
Zinc alloys with enhanced ductility

The ductility and/or breaking strength of zinc alloys containing 25% to 40% aluminium, 0.5% to 5% copper and up to 0.1% magnesium can be improved by the addition of various elements. A first series of improved alloys contains between 5 ppm and 0.1% boron, possibly together with…

BE 1,005,415 A6#53930364 Most Cited · 1 citations0.0/yr · PR 0.82ExpiredBE · Utility
Method for separating iron and heavy metals contained in a chloride solution
Inventors: Brouhon Jean-marc, Rasquin AndreAssignee: Centre Rech MetallurgiqueFiled 1991-10-14 · Granted 1993-07-20

The chloride content of the solution is set to a value between 1 g/l and150 g/l, and its pH is adjusted to a value less than 4 and its temperatureto a value between 20 degrees C and 90 degrees C. The solution is suspendedwith a reagent composed of at least one substance selected…

EP 0,119,180 A2#56491428 Most Cited · 1 citations0.0/yr · PR 0.80PendingEP · Application
Zinc base alloy with ductility properties

1. Zinc alloy containing from 25% to 40% of aluminium, from 0.5% to 5% of copper and up to 0.1% of magnesium, characterized in that it has a boron content of between 0.0005% (5 ppm) and 0.1%, and additionally a titanium content of between 0.0025% (25 ppm) and 0.5% and/or a…