To produce a high-temperature superconductor of the composition Bi 2 (Sr,Ca) 3 Cu 2 O 8+x having a strontium to calcium ratio of 5:1 to 2:1 and a value of x between 0 and 2, the oxides and/or carbonates of bismuth, strontium, calcium and copper are vigorously mixed in a…
Preisler Eberhard
Method for joining parts of ceramic high-temperature superconductor material of the composition Bi.sub.(2+a-b) (Sr 1-c ) Ca c ) .sub.(3-a) Pb b Cu.sub.(2+d) O x , where a is 0 to 0.3, b is 0 to 0.5, c is 0.1 to 0.9 and d is 0 to 2 and x has a value depending on the state of…
A high-temperature superconductor of the composition Bi2(Sr,Ca)3Cu2O8+x having a strontium:calcium ratio of from 5:1 to 2:1 and a value for x of between 0 and 2 is prepared by vigorously mixing the oxides and/or carbonates of bismuth, strontium, calcium and copper in a…
A high-temperature superconductor of the composition Bi2(Sr,Ca)3Cu2O8+x having a strontium:calcium ratio of from 5:1 to 2:1 and a value for x of between 0 and 2 is prepared by vigorously mixing the oxides and/or carbonates of bismuth, strontium, calcium and copper in a…
Die Erfindung bezieht sich auf einen resistiven Strombegrenzer (1), mit wenigstens einem den Nennstrom tragenden Leiter (2) aus einem Hochtemperatur-Supraleiter-Material, dessen wirksame elektrische Länge um mindestens das Dreifache größer ist als seine lineare Ausdehnung.…
The invention relates to a resistive current limiter having at least one conductor of a superconductive high-temperature material, carrying the rated current. The electrically active length of said conductor is at least three times greater than its linear extent.
For the production of tube-shaped mouldings of high-temperature superconductor material based on oxides of bismuth, calcium, strontium and copper, a homogeneous melt of the oxide mixture is allowed to run in a predetermined stoichiometry at temperatures from 900 to 1100 DEG C…
For the production of tube-shaped mouldings of high-temperature superconductor material based on oxides of bismuth, calcium, strontium and copper, a homogeneous melt of the oxide mixture is allowed to run in a predetermined stoichiometry at temperatures from 900 to 1100 DEG C…
The present invention relates to a method for the preparation of electrolytic manganese dioxide in which flocculent nuclei of a manganese oxide hydrate is dispersed in the electrolyte.
Process for preparing a high-T c superconductor as a precursor material for the oxide-powder-in-tube method (OPIT). The present invention relates to a process for preparing a high-T c superconductor as a precursor material for the oxide-powder-in-tube method, which involves…
In a process for producing a high-temperature superconductor and shaped products thereof, consisting of oxides or bismuth, strontium, calcium, copper and, if appropriate, lead and also sulphates of strontium and/or barium, oxides of bismuth, strontium, calcium, copper and, if…
The invention relates to solid bodies made of high-temperature superconducting material to which contact is made by solid, compact metallic conductors. To produce said solid bodies, high-temperature superconducting material is either melted completely or a melt is obtained from…
The invention relates to a resistive current limiter having at least one conductor of a superconductive high-temperature material, carrying the rated current. The electrically active length of said conductor is at least three times greater than its linear extent.
The disclosure relates to a process for removing molybdenum from aqueous salt solutions by adsorbing it on manganese dioxide. To this end, the salt solution is contacted with a bed of manganese dioxide (MnO 2 ) precipitated electrolytically and transformed into granular material.
A resistive current limiter takes the form of a hollow cylinder and is composed of high-temperature superconducting material. In this connection, the high-temperature superconducting material may be a polynary oxide. To produce said resistive current limiter, a homogeneous melt…
Die Erfindung betrifft ein Verfahren zur Entfernung von Molybdän aus wäßrigen Salzlösungen durch Adsorption an Mangandioxid, welches dadurch gekennzeichnet ist, daß man die Salzlösung mit einer Schüttung aus Mangandioxid (MnO2) in Kontakt bringt, das auf elektrolytischem Wege…
The invention relates to a resistive current limiter having at least one conductor of a superconductive high-temperature material, carrying the rated current. The electrically active length of said conductor is at least three times greater than its linear extent.
Die Erfindung betrifft einen aus den Oxiden des Bismuts, Strontiums, Calciums und Kupfers und gegebenenfalls des Bleis der Zusammensetzung Bi2-a+b+c Pba (Sr, Ca)3-b-c Cu2+d Ox mit a = 0 bis 0,7 ; b + c = 0 bis 0,5 ; d = - 0,1 bis 0,1; x = 7 bis 1o und einem Verhältnis von Sr :…
The present invention relates to a process for preparing a high-T c superconductor as a precursor material for the oxide-powder-in-tube method, which involves mixing the oxides of the elements Bi, Sr, Ca and Cu and completely melting them at temperatures of ≧1000° C., then…
Ein resistiver Strombegrenzer hat die Form eines Hohlzylinders und besteht aus Hochtemperatur- Supraleiter-Material. Dabei kann das Hochtemperatur-Supraleiter-Material ein polynäres Oxid sein. Zur Herstellung dieses resistiven Strombegrenzers bereitet man eine homogene Schmelze…
The present invention relates to a process for the production of a high-Tc superconductor as precursor material for the oxide-powder-in-tube method, in which the oxides of the elements Bi, Sr, Ca and Cu are mixed and completely melted at temperatures of >/= 1000@C, in which…
The disclosure relates to activated metal anodes consisting essentially of zirconium, niobium, tantalum or titanium and having its surface area activated by means of metallic manganese; the manganese content at the anode surface area of more than 16 weight % decreases towards…
A resistive current limiter takes the form of a hollow cylinder and is composed of high-temperature superconducting material. In this connection, the high-temperature superconducting material may be a polynary oxide. To produce said resistive current limiter, a homogeneous melt…