An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
Ploense David
A roofing system incorporates a fire resistant asphalt composition comprising a thermoplastic elastomer modified bitumen, a filler, a brominated diphenyl ether, antimony oxide, and zinc borate. The asphalt composition is utilized with and impregnated into at least one layer of…
A roofing system incorporates a fire resistant asphalt composition comprising a thermoplastic elastomer modified bitumen, a filler, a brominated diphenyl ether, antimony oxide, and zinc borate. The asphalt composition is utilized with and impregnated into at least one layer of…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
A roofing system incorporates a fire resistant asphalt composition comprising a thermoplastic elastomer modified bitumen, a filler, a brominated diphenyl ether, antimony oxide, and zinc borate. The asphalt composition is utilized with and impregnated into at least one layer of…
A roofing system incorporates a fire resistant asphalt composition comprising a thermoplastic elastomer modified bitumen, a filler, a brominated diphenyl ether, antimony oxide, and zinc borate. The apshalt composition is utilized with and impregnated into at least one layer of…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
An emulsified drilling fluid additive includes an emulsion of asphalt, at least one emulsifier, cellulose ether, and water. The asphalt has a softening point of 160 to 212° F., a penetration depth of 0 to 45 mm, and a viscosity of 200 to 800 cP at 350° F. The drilling fluid…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
A roofing system incorporates a fire resistant asphalt composition comprising a thermoplastic elastomer modified bitumen, a filler, a brominated diphenyl ether, antimony oxide, and zinc borate. The apshalt composition is utilized with and impregnated into at least one layer of…
An emulsified drilling fluid additive includes an emulsion of asphalt, at least one emulsifier, cellulose ether, and water. The asphalt has a softening point of 160 to 212 °F, a penetration depth of 0 to 45 mm, and a viscosity of 200 to 800 cP at 350 °F. The drilling fluid…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
An emulsified drilling fluid additive includes an emulsion of asphalt, at least one emulsifier, cellulose ether, and water. The asphalt has a softening point of 160 to 212° F., a penetration depth of 0 to 45 mm, and a viscosity of 200 to 800 cP at 350° F. The drilling fluid…
An exemplary shingle includes at least one coated shingle sheet defining a headlap portion and a tab portion each having opposed upper and lower surfaces. A first line of adhesive is adhered to one of the upper surface of the headlap portion and the lower surface of the tab…
A shingle coating asphalt composition is provided that is produced from a paving grade asphalt. The asphalt composition comprises a paving-grade asphalt that has been modified with one or more polymer additives; and a secondary additive comprising one or more of a viscosity…