Patents
Inventor / Author Profile

Parker Euan

141Total Forward Citations
17Indexed Patents
5Patent H-Index
Frequent Co-Inventors: Grele Bruno
US 4,656,203 A#1043897 Most Cited · 47 citations1.2/yr · PR 7.64ExpiredUS · Utility
Friction materials and their manufacture
Inventors: Parker EuanAssignee: Turner & Newall PlcFiled 1985-03-04 · Granted 1987-04-07

Low density friction products composed of non-asbestos reinforcing fibers embedded in a matrix of binder material, optionally including friction and wear modifiers, are described in which the actual density of the product is less than 72% of the theoretical density. Clutch…

US 4,775,705 A#1220005 Most Cited · 43 citations1.1/yr · PR 8.08ExpiredUS · Utility
Friction materials and their manufacture
Inventors: Parker Euan, Grele BrunoAssignee: T & N PlcFiled 1986-12-19 · Granted 1988-10-04

Non-asbestos brake pads made of reinforcing, temperature resistant, web-forming fibers such as aromatic polyamide pulp, optionally including other fibers and friction and wear modifiers is described. The brake pads have an actual density not greater than 88% and not less than a…

US 5,190,991 A#3036306 Most Cited · 25 citations0.8/yr · PR 3.85ExpiredUS · Utility
Brake linings
Inventors: Parker Euan, Grele BrunoAssignee: Nuturn CorpFiled 1990-11-01 · Granted 1993-03-02

A brake lining is made from a preform which has been formed by a compression step parallel to that surface of the brake lining preform which is to be the braking surface of the lining in use and has subsequently been compressed in a direction substantially normal to said surface…

EP 0,180,381 A2#8977416 Most Cited · 11 citations0.3/yr · PR 3.01PendingEP · Application
Friction materials and their manufacture
Inventors: Parker EuanAssignee: Nuturn CorpFiled 1985-10-17

Low density friction products composed of non-asbestos reinforcing fibers embedded in a matrix of binder material, optionally including friction and wear modifiers, are described in which the actual density of the product is less than 72% of the theoretical density. Clutch…

EP 0,271,965 A2#10254154 Most Cited · 10 citations0.3/yr · PR 2.33PendingEP · Application
Friction materials and their manufacture
Inventors: Parker Euan, Grele BrunoAssignee: Nuturn CorpFiled 1987-12-17

A non-asbestos brake pad is made of reinforcing fibres embedded in a binder material and the reinforcing fibres include a temperature resistant web-forming fibre in an amount of from 22 percent to 40 percent by volume of total solids in the pad. The pad also has an actual…

GB 2,165,851 A#29059359 Most Cited · 3 citations0.1/yr · PR 1.37ExpiredGB · Utility
Friction materials and their manufacture
Inventors: Parker EuanAssignee: Nuturn CorpFiled 1985-10-16

Low density friction products composed of non-asbestos reinforcing fibers embedded in a matrix of binder material, optionally including friction and wear modifiers, are described in which the actual density of the product is less than 72% of the theoretical density. Clutch…

CA 1,282,566 C#90637284 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Friction materials and their manufacture
Inventors: Parker Euan, Grele BrunoAssignee: Nuturn CorpFiled 1987-12-18 · Granted 1991-04-09

ABSTRACT A non-asbestos brake pad is made of reinforcing fibres embedded in a binder material and the reinforcing fibres include a temperature resistant web-forming fibre in an amount of from 22 percent to 40 percent by volume of total solids in the pad. The pad also has an…

DE 3,582,857 D1#109221355 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Reibungsmaterialien und ihre herstellung.
Inventors: Parker EuanAssignee: Nuturn CorpFiled 1985-10-17 · Granted 1991-06-20

Low density friction products composed of non-asbestos reinforcing fibers embedded in a matrix of binder material, optionally including friction and wear modifiers, are described in which the actual density of the product is less than 72% of the theoretical density. Clutch…

EP 0,180,381 A3#106354845 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Friction materials and their manufacture
Inventors: Parker, EuanAssignee: Nuturn CorporationFiled 1985-10-17

Low density friction products composed of non-asbestos reinforcing fibers embedded in a matrix of binder material, optionally including friction and wear modifiers, are described in which the actual density of the product is less than 72% of the theoretical density. Clutch…

MX 166,539 B#112338910 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredMX · Utility
Relleno de freno y metodo para su fabricacion
Inventors: Parker Euan, Grele BrunoAssignee: Nuturn CorpFiled 1987-12-21

La presente invención se refiere a relleno de freno que no contiene asbeto fabricado a partir de una composición que comprende fibras reforzantes puestas en una matriz de material ligante, caracterizado porque la fibra reforzante comprende una fibra formadora de tejido…