A razor blade comprising a substrate (50) with a wedge-shaped edge defined by facets that have a width of at least about 0.1 millimeter and an included angle of less than 20 degrees and characterized by a layer of amorphous diamond (60) on said wedge-shaped edge, said layer of…
Parent Robert C
A sharpened wedge-shaped edge (52) has an acute angle less than 17 degrees up to the distance 40 micrometers from the cutting edge (520) of the sharpened edge (52) and the cutting edge radius thereof is less than 500 Angstrom units, whereby a layer (60) of diamond or…
A razor blade includes a substrate (50) with a wedge-shaped edge at a distance of forty micrometers from the sharpened tip (52), and a layer of diamond or diamond-like material (60) defined by facets (66, 68) that have an included angle of less than seventeen degrees that has a…
In the present invention, there is disclosed a razor blade comprising a substrate (50) with a wedge-shaped edge (18) defined by facets (54, 56) that have a width of at least about 0.1 millimeter and an included angle of less than 20 degrees and a layer (60) of amorphous diamond…
The present invention relates to a razor blade (16, 20, 44) having a shaving edge defined by a first facet (54) and a second facet (56) that diverge at an edge angle and defining a stainless steel tip (52) at the contact of the first and the second facets (54, 56). Deposited on…
A razor blade comprising a substrate (50) with a wedge-shaped edge defined by facets that have a width of at least about 0.1 millimeter and an included angle of less than 20 degrees and characterized by a layer of amorphous diamond (60) on said wedge-shaped edge, said layer of…
A method of forming an anode comprising zinc for an alkaline cell (810) . The method involves mixing zinc particles with binders including preferably polyvinylalcohol, surfactant and water to form a wet paste. The wet paste is molded into the near shape of the cell's anode…
Una cuchilla de afeitar que tiene un filo de corte limitado por una primera superficie inclinada (54) y una segunda superficie inclinada (56), cuyo filo de corte tiene una arista (52) en la unión de dichas superficies inclinadas primera y segunda (54, 58), las cuales abarcan un…
A method of forming an anode comprising zinc for an alkaline cell (810) . The method involves mixing zinc particles with binders including preferably polyvinylalcohol, surfactant and water to form a wet paste. The wet paste is molded into the near shape of the cell's anode…
A method of forming an anode comprising zinc for an alkaline cell (810) . The method involves mixing zinc particles with binders including preferably polyvinylalcohol, surfactant and water to form a wet paste. The wet paste is molded into the near shape of the cell's anode…