A continuous casting mold having the wall thickness of each of parts corresponding to a point where molten steel begins to solidify during continuous casting is arranged to be locally thinner than other parts of the mold. High frequency oscillation is applied to the locally…
Oota Mituhiro
At the point where the molten steel begins to solidify during continuous casting, the wall of the continuous casting mould is thinner than in the remaining parts of the mould. The thinner sections (22) of the mould (6) are made to vibrate at a high frequency with a sufficient…
Die Stranggußform weist an der Stelle, wo sich der geschmolzene Stahl beim Stranggießen zu verfestigen beginnt, eine geringere Wandungsdicke auf als an den übrigen Teilen der Form. Die verdünnten Abschnitte (22) der Form (6) werden in hochfrequente Schwingungen mit ausreichender…
The mould walls possess thin zones (a) in the region where solidification of the molten metal commences; and oscillations are applied to zones (a). Zones (a) are pref. 5-30 mm thick, and 50-150 mm long in a vertical direction. The oscillation appts. is pref. fixed directly, or…