Patents
US 2014050938 A1#7084379 Most Cited · 14 citations1.2/yr · PR 1.99PendingUS · Application
Electrospark deposition process for oxidation resistant coating of cooling hole
Inventors: Lin Dechao, Ucok Ibrahim, Onal KivilcimAssignee: Lin Dechao, Ucok IbrahimFiled 2012-08-14

A method of providing an oxidation resistant coating is disclosed. The method includes providing a substrate having a first surface and cooling holes. A portable coating device includes electro-spark deposition (ESD) equipment and an ESD torch connected with the ESD equipment.…

US 2015132605 A1#6963826 Most Cited · 14 citations1.3/yr · PR 2.42PendingUS · Application
Composite composition for turbine blade tips, related articles, and methods

A composite composition that includes an MCrAlX alloy and a nano-oxide ceramic is disclosed. In the formula, M includes nickel, cobalt, iron, or a combination thereof, and X includes yttrium, hafnium, or a combination thereof, from about 0.001 percent to about 2 percent by…

CN 103,160,711 A#9390461 Most Cited · 11 citations0.8/yr · PR 2.14ActiveCN · Utility
Nickel-cobalt-based alloy and bond coat and bond coated articles incorporating the same

In an exemplary embodiment, a high temperature oxidation and hot corrosion resistant MCrAlX alloy is disclosed, wherein, by weight of the alloy, M comprises nickel in an amount of at least about 30 percent and X comprises from about 0.005 percent to about 0.19 percent yttrium.…

US 9,511,436 B2#10623873 Most Cited · 10 citations1.0/yr · PR 1.89ActiveUS · Utility
Composite composition for turbine blade tips, related articles, and methods

A composite composition that includes an MCrAlX alloy and a nano-oxide ceramic is disclosed. In the formula, M includes nickel, cobalt, iron, or a combination thereof, and X includes yttrium, hafnium, or a combination thereof, from about 0.001 percent to about 2 percent by…

US 2013157078 A1#12193895 Most Cited · 9 citations0.7/yr · PR 1.57PendingUS · Application
Nickel-Cobalt-Based Alloy And Bond Coat And Bond Coated Articles Incorporating The Same

In an exemplary embodiment, a high temperature oxidation and hot corrosion resistant MCrAlX alloy is disclosed, wherein, by weight of the alloy, M comprises nickel in an amount of at least about 30 percent and X comprises from about 0.005 percent to about 0.19 percent yttrium.…

EP 2,781,560 A1#15752322 Most Cited · 7 citations0.6/yr · PR 1.55PendingEP · Application
A bond coat system and a coated component
Inventors: Pabla Surinder Singh, Onal KivilcimAssignee: Gen ElectricFiled 2014-03-12

A bond coat system (210) and coated component are disclosed. The bond coat system (210) includes a first coating layer (212) adjacent a substrate (200) and a second coating layer (214) adjacent the first coating layer (212). The first coating layer (212) includes a γ/β…

US 2016031033 A1#33254297 Most Cited · 3 citations0.3/yr · PR 1.05PendingUS · Application
Electrospark deposition process for oxidation resistant coating of cooling hole
Inventors: Lin Dechao, Ucok Ibrahim, Onal KivilcimAssignee: Gen ElectricFiled 2015-08-03

A method of providing an oxidation resistant coating is disclosed. The method includes providing a substrate having a first surface and cooling holes. A portable coating device includes electro-spark deposition (ESD) equipment and an ESD torch connected with the ESD equipment.…

JP 2013127117 A#42536966 Most Cited · 2 citations0.1/yr · PR 0.95ActiveJP · Utility
Nickel-cobalt-based alloy and bond coat and bond coated articles incorporating the same

PROBLEM TO BE SOLVED: To provide bond coat materials that improve the spallation resistance of protective coating systems in which they are employed (particularly those which employ TBCs).SOLUTION: There is provided a high temperature oxidation and hot corrosion resistant MCrAlX…

JP 2014198902 A#43152910 Most Cited · 2 citations0.2/yr · PR 0.94ActiveJP · Utility
Bond coat system and coated component
Inventors: Pabla Surinder Singh, Onal KivilcimAssignee: Gen ElectricFiled 2014-03-14

PROBLEM TO BE SOLVED: To provide a bond coat material capable of improving peel resistance in a protective film system in which the bond coat material is used, especially in a system using TBC, concerning the bond coat material.SOLUTION: A bond coat system and a coated component…

US 2017247784 A1#37041546 Most Cited · 2 citations0.2/yr · PR 1.13PendingUS · Application
Coated articles and coating methods
Inventors: Onal KivilcimAssignee: Gen ElectricFiled 2016-02-29

A coated article is disclosed including a substrate, a bond coating, and a thermally insulating top coating. The substrate includes a substrate surface and a substrate material at the substrate surface. The bond coating is disposed on and contacts the substrate surface, and…

EP 2,607,510 A1#61679108 Most Cited · 1 citations0.1/yr · PR 0.74PendingEP · Application
Nickel-cobalt-based alloy and bond coat and bond coated articles incorporating the same

In an exemplary embodiment, a high temperature oxidation and hot corrosion resistant MCrAlX alloy is disclosed, wherein, by weight of the alloy, M comprises nickel in an amount of at least about 30 percent and X comprises from about 0.005 percent to about 0.19 percent yttrium.…

US 9,789,557 B2#58725165 Most Cited · 1 citations0.1/yr · PR 0.78ActiveUS · Utility
Electrospark deposition process for oxidation resistant coating of cooling hole
Inventors: Lin Dechao, Ucok Ibrahim, Onal KivilcimAssignee: Gen ElectricFiled 2015-08-03 · Granted 2017-10-17

A method of providing an oxidation resistant coating is disclosed. The method includes providing a substrate having a first surface and cooling holes. A portable coating device includes electro-spark deposition (ESD) equipment and an ESD torch connected with the ESD equipment.…

CN 104,479,428 A#142899553 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Composition and component
Inventors: Onal KivilcimAssignee: Gen ElectricFiled 2014-06-11

A composition useful as a bond coat is provided. The composition includes about 3% to about 7% chromium, about 10% to about 30% nickel, about 12% to about 18% aluminum, about 0.0005% to about 0.15% yttrium, about 0.0% to about 16% strengtheners, balance cobalt, and incidental…

EP 2,813,591 A1#117476038 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Co alloy composition and component
Inventors: Onal KivilcimAssignee: Gen ElectricFiled 2014-06-06

A composition useful as a bond coat 210 is provided. The composition includes about 3% to about 7% chromium, about 10% to about 30% nickel, about 12% to about 18% aluminum, about 0.0005% to about 0.15% yttrium, about 0.0% to about 16% strengtheners, balance cobalt, and…

EP 2,817,427 A1#65050860 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Alloys for bond coatings and articles incorporating the same

In an exemplary embodiment, a high temperature oxidation and hot corrosion resistant MCrAlX alloy is disclosed, wherein M comprises cobalt and X comprises, by weight of the alloy, from about 0.001 percent to less than 0.19 percent yttrium. In these alloys, X may also optionally…

JP 2015014047 A#62116252 Most Cited · 0 citations0.0/yr · PR 0.56ActiveJP · Utility
Composition and component
Inventors: Onal KivilcimAssignee: Gen ElectricFiled 2014-06-06

PROBLEM TO BE SOLVED: To provide a composition useful as a bond coat with a reduced amount of chromium.SOLUTION: The composition includes about 3 to about 7 wt.% chromium, about 10 to about 30 wt.% nickel, about 12 to about 18 wt.% aluminum, about 0.0005 to about 0.15 wt.%…

US 2013115072 A1#112925472 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Alloys for bond coatings and articles incorporating the same

In an exemplary embodiment, a high temperature oxidation and hot corrosion resistant MCrAlX alloy is disclosed, wherein M comprises cobalt and X comprises, by weight of the alloy, from about 0.001 percent to less than 0.19 percent yttrium. In these alloys, X may also optionally…

US 2014363698 A1#97886042 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Composition and component
Inventors: Onal KivilcimAssignee: Gen ElectricFiled 2013-06-11

A composition useful as a bond coat is provided. The composition includes about 3% to about 7% chromium, about 10% to about 30% nickel, about 12% to about 18% aluminum, about 0.0005% to about 0.15% yttrium, about 0.0% to about 16% strengtheners, balance cobalt, and incidental…

US 2018009051 A1#85878190 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Electrospark deposition process for oxidation resistant coating of cooling hole
Inventors: Lin Dechao, Ucok Ibrahim, Onal KivilcimAssignee: Gen ElectricFiled 2017-09-07

A method of providing an oxidation resistant coating is disclosed. The method includes providing a substrate having a first surface and cooling holes. A portable coating device includes electro-spark deposition (ESD) equipment and an ESD torch connected with the ESD equipment.…

US 9,957,598 B2#66186449 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Coated articles and coating methods
Inventors: Onal KivilcimAssignee: Gen ElectricFiled 2016-02-29 · Granted 2018-05-01

A coated article is disclosed including a substrate, a bond coating, and a thermally insulating top coating. The substrate includes a substrate surface and a substrate material at the substrate surface. The bond coating is disposed on and contacts the substrate surface, and…

WO 2013/071086 A1#82018050 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Alloys for bond coatings and articles incorporating the same

In an exemplary embodiment, a high temperature oxidation and hot corrosion resistant MCrAlX alloy is disclosed, wherein M comprises cobalt and X comprises, by weight of the alloy, from about 0.001 percent to less than 0.19 percent yttrium. In these alloys, X may also optionally…