Patents
CN 1,618,123 A#12537652 Most Cited · 8 citations0.4/yr · PR 2.99ExpiredCN · Utility
Lanthanide series layered superlattice materials for integrated circuit applications

An integrated circuit (40) includes a layered superlattice material (57) including one or more of the elements cerium, praseodymium, neodymium, promethium, samarium, europium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, and lutetium. These elements may…

CN 101,680,091 A#17163787 Most Cited · 6 citations0.4/yr · PR 1.83ActiveCN · Utility
Synthesizing of reactive flow deposition and inorganic foils

The present invention describes the subatmospheric chemical vapour deposition of the substrate that uses orientation response thing air-flow and move with respect to described air-flow.Therefore, use described CVD configuration can reach higher relatively sedimentation rate,…

CN 101,443,888 A#39031707 Most Cited · 2 citations0.1/yr · PR 1.04ActiveCN · Utility
Thin silicon or germanium sheets and photovoltaics formed from thin sheets

Thin semiconductor foils can be formed using light reactive deposition. These foils can have an average thickness of less than 100 microns. In some embodiments, the semiconductor foils can have a large surface area, such as greater than about 900 square centimeters. The foil can…

CN 1,237,618 C#142110027 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
Ferroelectric memory with perroelectric thin film and method of fabrication
Inventors: Araujo Narayan Solayappan VikrAssignee: Symetrix CorpFiled 2000-01-07 · Granted 2006-01-18

A coating of liquid precursor containing a metal is applied to a first electrode (122), baked on a hot plate in oxygen ambient at a temperature not exceeding 300 DEG C for five minutes, then RTP annealed at 675 DEG C for 30 seconds. The coating is then annealed in oxygen or…

HK 1,039,684 A1#90184775 Most Cited · 0 citations0.0/yr · PR 0.56PendingHK · Application
Low temperature process for fabricating layered superlattice materials and making electronic devices including same

A coating of liquid precursor containing a metal is applied to a first electrode, baked on a hot plate in oxygen ambient at a temperature not exceeding 300° C. for five minutes, then RTP annealed at 675° C. for 30 seconds. The coating is then annealed in oxygen or nitrogen…