Thermoplastic polydiorganosiloxane/polycarbonate block copolymers based on dihydroxydiphenylcycloalkanes corresponding to the following general formula (I): ##STR1## wherein R 1 and R 2 independently represent hydrogen, halogen, preferably chlorine or bromine, C 1 -C 8 alkyl, C…
Morbitzer Leo
The present invention relates to thermoplastic moulding compositions, which have improved impact strength at low temperature, comprising thermoplastic polyesters, in particular polyalkylene terephthalates, and grafted, partially or highly cross-linked diene rubbers and/or…
Moulding compositions based on ABS-graft polymers, containing: A. 5 to 70 parts, by weight of a graft polymer obtained by grafting 20 to 60 parts by weight of a mixture of styrene and acrylonitrile in a ratio, by weight, of 95 : 5 to 60 : 40 onto 80 to 40 parts, by weight, of…
A shaped article, in particular a support for image information layers prepared from a biaxially stretched film prepared from a polymer blend of 50 to 97 wt.% of a linear polyester and 3 to 50 wt.% of a polymer containing styrene, wherein the percentages relate to the sum of…
This invention relates to thermoplastic molding compositions having improved impact strength at low temperatures comprising polyamides and grafted, at least partially crosslinked diene rubbers and/or acrylate rubbers having a bimodal rubber particle size distribution.
The use of a liquid polymethyl phenyl siloxane or a liquid polydimethyl siloxane, in combination with calcium stearate, pentaerythritol tetrastearate, bis-stearylamide of ethylene diamine or mixtures thereof for improving the physical properties of ABS-polymers.
A homogeneous thermoplastic mixture comprising (A) from 85 to 99.5% by weight of a propylene-ethylene copolymer containing from 0.5 to 15% by weight of copolymerized ethylene units and having a melt index of from 1.0 to 30 g/min at 230° C. and under a load of 5 kg; and (B) from…
Mixtures of polycarbonates with copolymers and/or graft polymers based on styrene/acrylonitrile, where the acrylonitrile content in the styrene-acrylonitrile copolymer is from 6 to 15% by weight.
A homogeneous, thermoplastic mixture comprising (A) from 85 to 99.5% by weight of isotactic polypropylene; and (B) from 15 to 0.5% by weight of a liquid, saturated diorganopolysiloxane having a viscosity of from 30,000 to 80,000 cSt at 20° C. The elastic properties of moulded…
A block copolymer is produced from I. 1 to 60% by weight of at least one telechelic diene polymer containing terminal carbonate ester, --OH--, --NH 2 --, carboxylic acid or carboxylic acid ester groups and having a molecular weight M n of from about 400 to 1300, and II. 99 to…
The present invention relates to thermoplastic moulding compositions consisting of polycarbonates, graft polymers and copolymers, which are characterized in that they contain special graft polymers and/or special copolymers, with the result that these moulding compositions…
The new polyester carbonate-polysiloxane block copolymers having recurrent structural units of the following formulae <IMAGE> (1) <IMAGE> (2) <IMAGE> (3) and <IMAGE> (4) have improved resistance to petrol compared with known polyester…
Novel vulcanizable mixtures comprising silicone-core, acrylate-shell rubber particles dispersed within a fluorocarbon rubber.
Mixtures of (1) 99 to 1% of one or more segment copolymers of alternating linear or branched segments A and B wherein A are polymer blocks of aromatic vinyl compounds with Tg>20° C. (hard segment) and B are polymer blocks containing polymerized conjugated dienes with Tg>0°…
The invention relates to the use of mixtures consisting of 5 to 95% by weight of an aromatic polycarbonate of which the linear chains contain from 0.1 mol-% to 50 mol-% bifunctional structural units corresponding to formula (1) ##STR1## and 95 to 5% by weight of a thermoplastic…
Blockcopolymere aus Polyamidblöcken und telechelen Dienpolymerisatblöcken mit MG von 400 - 5000.
The thermoplastic compositions comprise polyarylene sulphides (PAS), preferably polyphenylene sulphides (PPS), and particulate, crosslinked silicone rubbers.
Molding compositions comprising a "terminally unsaturated"polyurethane, a copolymerizable vinyl or vinylidene compound and a rubbery-elastic polymer having a glass transition temperature of between -90° and +10° C. can be used for the preparation of molded articles…
Thermoplastic moulding materials, with improved toughness at low temperatures, of polyamide and cross-linked graft rubbers from the diene rubber and acrylate rubber series, obtained by heating blends of the two components below the melting point of the polyamide.
1. Thermoplastic moulding compositions comprising I. 30-94% by weight of at least one polyamide, II. 70-3% by weight of a graft product prepared from a) 50-95% by weight of a cross-linked polymer of butadiene and/or subst. butadiene, which can optionally be composed to an extent…
The novel polyester carbonate-polysiloxane block copolymers containing recurring structural units <IMAGE> have improved gasoline (petrol) resistance compared with known polyester carbonate-polysiloxane block copolymers. They are used to produce mouldings, in particular for…
The invention relates to a crosslinkable mixture of a) from 98 to 35 parts by weight of a free-radical-vulcanisable fluororubber (fluorinated rubber) and b) from 2 to 65 parts byw eight of a silicone/acrylate core/shell rubber having a silicone content b1) of 50 to 95 parts by…
Block copolyesters based on polyalkylene terephthalates which contain polydiene blocks show an extremely low deformation even when they are processed into thin articles. They still have a crystallinity which is decreased by less than the ratio corresponding to the polydiene…
Transparent mixtures of aromatic polycarbonates and poly-C1-C8-alkyl (meth)acrylates are prepared by melting the polymers employed in the presence of supercritical gases or gas mixtures, intensively mixing the molten polymers until the viscosity of the melt has dropped by at…
Die Erfindung betrifft homogene, thermoplastische Mischungen aus A) 85 - 99,5 Gew.-% Propylen-Ethylen-Copolymerisat mit 0,5 - 15 Gew.-% copolymerisierten Ethyleneinheiten und mit einem Schmelz-index von 1,0 bis 30 g/10 min. bei 230°C und einer Belastung von 5 kg und B) 0.5 - 15…