Mannich polyols having a viscosity of from 300 to 3,500 cps (0.3 to 3.5 Pa*s) at 25 DEG C are prepared by admixing a phenol, an alkanolamines, and formaldehyde mixed in molar ratios of from 1:1:1 to 1:2.2:2.2 resulting in an initiator which can be alkoxylated using a mixture of…
Inventor / Author Profile
Moore S E
15Total Forward Citations
5Indexed Patents
2Patent H-Index
Mannich polyols having nominal functionalities of 3-5.4 and viscosities of 300-3500 centipoises (0.3-3.5 Pa.s) at 25 ℃ are prepared by combining phenol, alkanolamine, formaldehyde in a molar ratio of 1: 1 to 1: 2.2 to form an intermediate and alkoxylating with a mixture of…
Methods and apparatuses for detecting characteristics of a microelectronic substrate. A method in accordance with an embodiment of the invention includes positioning the microelectronic substrate proximate to and spaced apart from the first and second spaced apart electrodes,…