The invention discloses a chemical fixation-biomass improvement coupled repairing method of cadmium zinc combined polluted acidic soil, comprising the following steps of: crushing the cadmium zinc combined pollutant acidic soil and sieving through a sieve with the aperture being…
Min Xiaobo
The invention discloses a method for extracting iron through reduction smelting of lead slag. The method comprises the following steps: adding a slagging agent and a reducing agent into the lead slag, performing reduction smelting in an inert atmosphere, reducing lead and zinc…
The invention discloses a kind of high-effective microorganism cenobium integration denitrification device based on mineralising filler.Include the reactor body of filling mineralising filler, from top to bottom respectively water inlet, spongy water distribution layer, aerobic…
The invention discloses a kind of stabilized methods of arsenic acid scum, include the following steps:(1) iron system stabilizer, mixing are added in arsenic-containing waste residue;(2) mixture addition reaction solution, stirs and slurry is made;(3) after stirring slurry…
The invention discloses a device and a method for green separation and purification of sulfur in desulfurization waste liquid, wherein the device comprises a solid-liquid separator, an air-flotation sulfur melting kettle, a fine separator and an analytical separator; a sulfur…
The invention provides a preparation method of a self-supporting cobalt phosphide nanowire electrode, which comprises the following steps: s1, carrying out solid-liquid reaction on the cobalt material and oxalic acid to obtain cobalt oxalate growing on the surface of the cobalt…
The invention provides a method for treating solid waste in the low-temperature smelting synergistic industry of antimony, which comprises the following steps: uniformly mixing a sulfur-antimony-rich raw material with industrial solid waste, a regulator and a catalyst to form a…
The invention provides a preparation method and application of a refining modifier for a regenerated aluminum alloy iron-rich phase, wherein the refining modifier comprises 60% -75% of fluxing agent, 15% -30% of boron-containing reagent and 9% -11% of Co powder, the fluxing…