Patents
EP 0,363,784 A1#35678005 Most Cited · 2 citations0.1/yr · PR 1.27PendingEP · Application
Flux for hot galvanising
Inventors: Meyer Hermann Dr, Goesele Wilhelm Dr, Parthey Harry DrAssignee: Basf AgFiled 1989-10-03

A flux for hot galvanising consists of 70 to 90 % by weight of zinc chloride, 4.5 to 20 % by weight of potassium chloride, 0.4 to 5 % by weight of butynediol, 0 to 5 % by weight of ammonium chloride and 0.1 to 1.5 % by weight of a nonionic surfactant of the general formula…

EP 0,363,784 B1#35730950 Most Cited · 2 citations0.1/yr · PR 1.26ExpiredEP · Utility
Flux for hot galvanising
Inventors: Meyer, Hermann, Dr., Goesele, Wilhelm, Dr., Parthey, Harry, Dr.Assignee: BASF AktiengesellschaftFiled 1989-10-03 · Granted 1992-07-29

A flux for hot galvanising consists of 70 to 90 % by weight of zinc chloride, 4.5 to 20 % by weight of potassium chloride, 0.4 to 5 % by weight of butynediol, 0 to 5 % by weight of ammonium chloride and 0.1 to 1.5 % by weight of a nonionic surfactant of the general formula…

DE 3,744,387 A1#53519652 Most Cited · 1 citations0.0/yr · PR 0.82PendingDE · Application
Process for preparing boron trifluoride

To prepare boron trifluoride, calcium fluoride is reacted with oleum and boron compounds. The reaction is carried out in two stages, with a) in a first stage, reacting calcium fluoride with oleum and b) in a second stage, reacting the reaction mixture from the first stage with a…

DE 3,834,733 A1#112680020 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Flussmittel fuer die feuerverzinkung
Inventors: Meyer Hermann Dr, Goesele Wilhelm Dr, Parthey Harry DrAssignee: Basf AgFiled 1988-10-12

A flux for hot galvanising consists of 70 to 90 % by weight of zinc chloride, 4.5 to 20 % by weight of potassium chloride, 0.4 to 5 % by weight of butynediol, 0 to 5 % by weight of ammonium chloride and 0.1 to 1.5 % by weight of a nonionic surfactant of the general formula…

DE 58,901,945 D1#73484167 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Flussmittel fuer die feuerverzinkung.
Inventors: Meyer Hermann Dr, Goesele Wilhelm Dr, Parthey Harry DrAssignee: Basf AgFiled 1989-10-03 · Granted 1992-09-03

A flux for hot galvanising consists of 70 to 90 % by weight of zinc chloride, 4.5 to 20 % by weight of potassium chloride, 0.4 to 5 % by weight of butynediol, 0 to 5 % by weight of ammonium chloride and 0.1 to 1.5 % by weight of a nonionic surfactant of the general formula…

EP 0,249,228 A2#123680407 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Process for the preparation of anhydrous aluminium chloride

Wasserfreies Aluminiumchlorid wird durch Umsetzung von γ-Tonerde mit Kohlenmonoxid und Chlor und/oder Phosgen in einer Wirbelschicht bei Temperaturen von 400 bis 700°C hergestellt. Als γ-Tonerde wird eine solche eingesetzt, die mit CuK?-Strahlung ein Röntgendiffraktogramm…

EP 0,359,020 A1#95822117 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Process for the recovery of wastes containing sodium sulfate
Inventors: Meyer Hermann Dr, Roemer Rainer Dr, Pforr Gerhard DrAssignee: Basf AgFiled 1989-08-29

Die Anmeldung betrifft ein Verfahren zur Aufarbeitung von natriumsulfathaltigen Rückständen durch Reduktion des Sulfates, bei dem man das Sulfat oder Mischungen oder Lösungen des Sulfates auf Temperaturen über 1000°C, insbesondere über 1 200°C unter reduzierenden Bedingungen…