Patents
US 6,519,973 B1#651106 Most Cited · 61 citations2.6/yr · PR 4.55ExpiredUS · Utility
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

A process and furnace for melting glass is set forth wherein the majority of the combustion energy over the melting zone of the furnace is provided by oxy-fuel combustion while a majority of the combustion energy over the fining zone of the furnace is provided by air-fuel…

US 2007227299 A1#680951 Most Cited · 59 citations3.1/yr · PR 10.63PendingUS · Application
Wear Resistant Low Friction Coating Composition, Coated Components, and Method for Coating Thereof
Inventors: Marchiando Robert, Leist JonAssignee: Momentive Performance Mat IncFiled 2006-12-21

A composition for coating sliding or rolling or fretting or impacting members is formed by preparing a composite powder of TiB2 and BN, with a TiB 2 to BN ratio ranging from 1:7 to 20:1, and a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt,…

US 8,034,153 B2#1632408 Most Cited · 37 citations2.5/yr · PR 2.82ActiveUS · Utility
Wear resistant low friction coating composition, coated components, and method for coating thereof
Inventors: Marchiando Robert, Leist JonAssignee: Momentive Performances Materials IncFiled 2006-12-21 · Granted 2011-10-11

A composition for coating sliding or rolling or fretting or impacting members is formed by preparing a composite powder of TiB2 and BN, with a TiB 2 to BN ratio ranging from 1:7 to 20:1, and a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt,…

CN 101,037,566 A#3394316 Most Cited · 23 citations1.2/yr · PR 4.64ActiveCN · Utility
Wear resistant low friction coating composition, coated components, and method for coating thereof
Inventors: Leist Jon, Marchiando RobertAssignee: Momentive Performance Mat IncFiled 2006-12-22

A composition formed to be used for coating, sliding, or rolling, or eroding, or impacting components, includes composite powder for preparing TiB2 and BN, wherein a ratio of the TiB2 and BN is 1:7 to 20:1, and a metal matrix selected from nickel, chromium, iron, cobalt,…

EP 1,136,451 A2#3920662 Most Cited · 21 citations0.8/yr · PR 3.70PendingEP · Application
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

Glass forming ingredients are melted in a furnace (140; 200) having a melting zone (184; 236) and a fining zone (170; 270) and in which the majority of the combustion energy (172-184; 238-248) over the melting zone (184; 236) is provided by oxy-fuel combustion while a majority…

US 6,217,681 B1#4792364 Most Cited · 18 citations0.7/yr · PR 4.35ExpiredUS · Utility
Method for oxygen-enhanced combustion using a vent stream

Oxygen-enhanced combustion in a manufacturing plant using a nitrogen plant to obtain a nitrogen product stream for use in the plant is effected by utilizing the oxygen-rich vent, waste, or exhaust stream as the primary source of oxidant for combustion of fuel in burners used to…

EP 1,801,248 A2#6151307 Most Cited · 15 citations0.8/yr · PR 3.51PendingEP · Application
Wear resistant low friction coating composition, coated components, and method for coating thereof
Inventors: Leist Jon, Marchiando RobertAssignee: Momentive Performance Mat IncFiled 2006-12-22

A composition for coating sliding or rolling or fretting or impacting members is formed by preparing a composite powder of TiB 2 and BN, with a TiB 2 to BN ratio ranging from 1:7 to 20:1, and a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt,…

US 2008038083 A1#7799760 Most Cited · 13 citations0.7/yr · PR 1.92PendingUS · Application
Fasteners Coated with Boron Nitride and Means for Securing Fasteners

An anti-seizing composition that facilitates securing fasteners in an assembly, e.g., a nail that is driven by a hammer or a threaded nail or screw that is screwed into a coupling, a nut, or a building block, etc. In one embodiment, the composition comprises a sufficient amount…

US 2008015122 A1#10704413 Most Cited · 10 citations0.6/yr · PR 1.79PendingUS · Application
Lubricant Composition and Cable Pulling Method

The present invention is directed to enhanced compositions that facilitate the pulling of cables through conduits. In one embodiment, the composition comprises a sufficient amount of boron nitride, which, upon application onto the cable surface, allows the cable to be pulled…

JP 2001316121 A#11284361 Most Cited · 9 citations0.4/yr · PR 2.55ExpiredJP · Utility
Glass melting system having oxygen-fuel combustion over melting zone and air-fuel combustion over clarifying zone, and furnace therefor

PROBLEM TO BE SOLVED: To provide a system for melting glass achieving improved quality and productivity of glass, and to provide a furnace for the system. SOLUTION: This system supplies combustion energy over the melting zone of the furnace mostly by oxygen-fuel combustion, more…

KR 20010090506 A#31431313 Most Cited · 3 citations0.1/yr · PR 1.15ExpiredKR · Utility
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

PURPOSE: Provided are a glass melting process and a furnace therefor with oxygen-fuel combustion over melting zone and air-fuel combustion over refining zone, capable of achieving improved quality and productivity of glass. CONSTITUTION: In the process, glass forming ingredients…

US 7,900,892 B2#34042769 Most Cited · 3 citations0.2/yr · PR 0.96ActiveUS · Utility
Lubricant composition and cable pulling method
Inventors: Student Joerg, Sun Rickson, Shaffer Gregory W, Lelonis Donald, Hans PaulAssignee: Momentive Performance Mat IncFiled 2006-11-01 · Granted 2011-03-08

The present invention is directed to enhanced compositions that facilitate the pulling of cables through conduits. In one embodiment, the composition comprises a sufficient amount of boron nitride, which, upon application onto the cable surface, allows the cable to be pulled…

KR 20070066991 A#36406518 Most Cited · 2 citations0.1/yr · PR 1.17ActiveKR · Utility
Wear resistant low friction coating composition, coated components, and method for coating thereof
Inventors: Marchiando Robert, Leist JonAssignee: Momentive Performance Mat IncFiled 2006-12-22

A coating composition is provided to comprise a composite material having a balanced combination of a low friction characteristic from a material such as BN and a wear resistance from a material such as TiB2. The coating composition for use on a contact surface comprises 5-60wt%…

EP 1,801,248 A3#52687698 Most Cited · 1 citations0.1/yr · PR 0.82ActiveEP · Utility
Wear resistant low friction coating composition, coated components, and method for coating thereof
Inventors: Leist Jon, Marchiando RobertAssignee: Momentive Performance Mat IncFiled 2006-12-22

A composition for coating sliding or rolling or fretting or impacting members is formed by preparing a composite powder of TiB 2 and BN, with a TiB 2 to BN ratio ranging from 1:7 to 20:1, and a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt,…

TW 200,831,811 A#60093237 Most Cited · 1 citations0.1/yr · PR 0.76ActiveTW · Utility
Fasteners coated with boron nitride and means for securing fasteners

An anti-seizing composition that facilitates securing fasteners in an assembly, e.g., a nail that is driven by a hammer or a threaded nail or screw that is screwed into a coupling, a nut, or a building block, etc. In one embodiment, the composition comprises a sufficient amount…

BR 0,101,132 A#106760584 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredBR · Utility
Processo de fusão do vidro com fornalha e combustão oxigênio-combustìvel sobre a zona de fusão e combustão ar-combustìvel sobre a zona de refino

Glass forming ingredients are melted in a furnace (140; 200) having a melting zone (184; 236) and a fining zone (170; 270) and in which the majority of the combustion energy (172-184; 238-248) over the melting zone (184; 236) is provided by oxy-fuel combustion while a majority…

CA 2,340,866 A1#85561920 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

A process and furnace for melting glass is set forth wherein the majority of the combustion energy over the melting zone of the furnace is provided by oxy-fuel combustion while a majority of the combustion energy over the fining zone of the furnace is provided by air-fuel…

CA 2,340,866 C#116517853 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

A process and furnace for melting glass is set forth wherein the majority of the combustion energy over the melting zone of the furnace is provided by oxy-fuel combustion while a majority of the combustion energy over the fining zone of the furnace is provided by air-fuel…

CZ 20,011,060 A3#81082998 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCZ · Utility
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

Glass forming ingredients are melted in a furnace (140; 200) having a melting zone (184; 236) and a fining zone (170; 270) and in which the majority of the combustion energy (172-184; 238-248) over the melting zone (184; 236) is provided by oxy-fuel combustion while a majority…

CZ 301,478 B6#78566538 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCZ · Utility
Process for melting glass forming ingredients in a furnace and furnace for melting glass forming ingredients

In the present invention, there is disclosed a process for melting glass forming ingredients in a furnace, wherein the process is characterized in that a majority of the combustion energy over the melting zone is provided by oxy-fuel combustion while a majority of the combustion…

DE 60,101,011 D1#129824047 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Glasschmelzverfahren und Ofen dafür mit Sauerstoff-Brennstoffverbrennung in der Schmelzzone und Luft-Brennstoffverbrennung in der Lauterzone

Glass forming ingredients are melted in a furnace (140; 200) having a melting zone (184; 236) and a fining zone (170; 270) and in which the majority of the combustion energy (172-184; 238-248) over the melting zone (184; 236) is provided by oxy-fuel combustion while a majority…

DE 602006017498 D1#72166057 Most Cited · 0 citations0.0/yr · PR 0.56ActiveDE · Utility
Verschleißfeste reibungsarme Beschichtungszusammensetzung und Verfahren zur Beschichtung
Inventors: Leist Jon, Marchiando RobertAssignee: Momentive Performance Mat IncFiled 2006-12-22

A composition for coating sliding or rolling or fretting or impacting members is formed by preparing a composite powder of TiB 2 and BN, with a TiB 2 to BN ratio ranging from 1:7 to 20:1, and a metallic matrix selected from the group consisting of nickel, chromium, iron, cobalt,…

EP 1,136,451 A3#132158205 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Glass melting process and furnace therefor with oxy-fuel combustion over melting zone and air-fuel combustion over fining zone

Glass forming ingredients are melted in a furnace (140; 200) having a melting zone (184; 236) and a fining zone (170; 270) and in which the majority of the combustion energy (172-184; 238-248) over the melting zone (184; 236) is provided by oxy-fuel combustion while a majority…

EP 1,881,089 A1#128268234 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Fasteners coated with boron nitride and means for securing fasteners

An anti-seizing composition that facilitates securing fasteners in an assembly, e.g., a nail that is driven by a hammer or a threaded nail or screw that is screwed into a coupling, a nut, or a building block, etc. In one embodiment, the composition comprises a sufficient amount…

ES 2,204,809 T3#142287177 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Horno y procedimiento de fusion de vidrio con combustion sobre la zona de fusion y combustion de aire sobre la zona de afino.

Glass forming ingredients are melted in a furnace (140; 200) having a melting zone (184; 236) and a fining zone (170; 270) and in which the majority of the combustion energy (172-184; 238-248) over the melting zone (184; 236) is provided by oxy-fuel combustion while a majority…