The invention relates to a method for regenerating a zeolitic catalyst, comprising the following steps: (I) at least one partially deactivated catalyst is heated to a temperature ranging from 250 to 600 DEG C in an atmosphere containing less than 2 vol. % oxygen; (II) the…