A shaped, high-strength dental ceramic prothesis is made by pressing a molding composition comprising about 1-50 wt % glass particles and about 50-99 wt % ceramic particles to form a ceramic frame, veneering the frame and firing the coated frame.
Malash Atef
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
A process for manufacturing a non-metallic dental prosthesis including a ceramic frame and an esthetic ceramic veneer including the steps of: preparing the ceramic frame by press molding a composition comprising from 1 to 50 parts by weight glass particles and from 50 to 99…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
En formet, dental keramprotese med høy styrke frem- stilles ved å presse en støpeblandlng som omfatter fra l til 50 vekt-* glasspartlkler og fra 99 til 50 vekt-* uorganiske oksydpartikler ved et trykk fra 10 til 40 MPa og en temperatur fra ca. 1000 til 1200*C. Dentalproteser som…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
DENTAL PROSTHESIS ABSTRACT OF THE INVENTION A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…
A shaped, high-strength dental ceramic prosthesis is made by pressing a molding composition including from about 1 to 50 percent by weight glass particles and from about 99 to about 50 percent by weight inorganic oxide particles at a pressure of from about 10 to about 40 MPa and…